Role of crevice size induced microenvironment variation within the gap in initiating crevice corrosion of 201 stainless steel
Source abstract
Abstract
The effects of the real-time changes in the microenvironment within the crevice caused by the change in crevice size on the induction of crevice corrosion of 201 stainless steel (201-SS) in 1 M (pH = 4.00) NaCl solution were evaluated using conventional methods and scanning electrochemical microscopy (SECM) containing potentiometric probes. Results show that a decrease in pH and an increase in the Cl− concentration within the gap are the pivotal determinants of crevice corrosion initiation. A narrower crevice creates a more aggressive corrosive environment. After immersion for 48 h, the corresponding pH values at the mouths of crevice with widths of 100, 250, 400 and 550 μm dropped to 1.64, 2.26, 2.73 and 2.88, respectively. The crevice size affects the accumulation rate of erosive ions and the initiation time of pits corrosion within the crevice, through the volume and diffusion effect. The coupling effect of the decrease in pH value and the increase in concentration of chloride ions is the main driver for the negative shift of the open circuit potential (OCP) and corrosion potential of 201-SS.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Introduction of Cu2+ to the inside of the crevice by chelation and its effect on crevice corrosion of Type 316L stainless steel10.1016/j.corsci.2022.110850 ↗
2. In-situ radial pH monitoring inside the crevice of stainless steel combined with potentiometric scanning electrochemical microscopy10.1016/j.electacta.2023.143109 ↗
3. Galvanically enhanced fretting-crevice corrosion of cemented femoral stems10.1016/j.jmbbm.2014.08.021 ↗
4. Unraveling the inhibitive performance and adsorption behavior of expired compound glycyrrhizin tablets as an eco-friendly corrosion inhibitor for copper in acidic medium10.1016/j.jtice.2024.105913 ↗
5. Transient numerical model for crevice corrosion of pipelines under disbonded coating with cathodic protection10.1016/j.matdes.2015.09.047 ↗
6. A multiphysics model for studying transient crevice corrosion of stainless steel10.1016/j.jmst.2020.06.008 ↗
7. A metallic biomaterial tribocorrosion model linking fretting mechanics, currents, and potentials: model development and experimental comparison10.1002/jbm.b.34643 ↗
8. Effects of long-term annealing on pitting corrosion behavior of Type 304 borated stainless steels10.1016/j.corcom.2024.08.001 ↗
9. Crevice corrosion repassivation of Ni-Cr-Mo alloys by cooling10.5006/3100 ↗
10. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗
11. A peridynamic model for crevice corrosion damage10.1016/j.electacta.2021.139512 ↗
12. Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids10.5006/3324 ↗
13. Improving the discharge performance of aqueous Mg-air battery using dicarboxylic acid additives10.1016/j.materresbull.2024.113160 ↗
14. Pitting corrosion of 304 stainless steel in secondary water supply system10.1016/j.corcom.2021.11.010 ↗
15. The role of acetic acid or H+ in initiating crevice corrosion of N80 carbon steel in CO2-saturated NaCl solution10.1016/j.corsci.2017.08.028 ↗
16. Crevice corrosion of N80 carbon steel in CO2-saturated environment containing acetic acid10.1016/j.corsci.2016.08.002 ↗
17. Insight into the triggering effect of (Al, Mg, Ca, Mn)-oxy-sulfide inclusions on localized corrosion of weathering steel10.1016/j.jmst.2020.06.031 ↗
18. Effect of crevice gap on crevice corrosion initiation and development of 2205 duplex stainless steel in NaCl solution10.1016/j.jmrt.2022.10.059 ↗
19. Sudden pH and Cl-concentration changes during the crevice corrosion of type 430 stainless steel10.1149/1945-7111/ac9bda ↗
20. An investigation into the stages of alloy 625 crevice corrosion in an ocean water environment: initiation, propagation and repassivation in a remote crevice assembly10.1149/2.0491911jes ↗
21. Nodular corrosion inside the crevice of Alloy 690 in deaerated high-temperature chloride solution10.1016/j.corsci.2021.109442 ↗
22. Estimation of potential distribution during crevice corrosion through analysis of I-V curves obtained by LAPS10.3390/s20102873 ↗
23. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938x(89)90039-5 ↗
24. The influence of the crevice induced IR drop on polarization measurement of localized corrosion behavior of 316L stainless steel10.1016/j.corsci.2019.04.030 ↗
25. Study on microstructure and mechanical properties of steel corrosion products in marine environment10.3389/fmats.2024.1474315 ↗
26. Crevice corrosion of solution annealed 25Cr duplex stainless steels: effect of W on critical temperatures10.1016/j.corsci.2020.109053 ↗
27. A mathematical model of crevice corrosion for buried pipeline with disbonded coatings under cathodic protection10.1016/j.jlp.2016.03.024 ↗
28. Sulphate reducing bacteria (SRB) biofilm development and its role in microbial corrosion of carbon steel10.3389/fmats.2024.1360869 ↗
29. A quantitative phase-field model for crevice corrosion10.1016/j.commatsci.2018.03.011 ↗
30. Stress corrosion cracking resistant nanostructured Al-Mg alloy with low angle grain boundaries10.1016/j.actamat.2021.117607 ↗
31. Crevice corrosion of U75V high-speed rail steel with varying crevice gap size by in-situ monitoring10.1016/j.jmrt.2021.12.116 ↗
32. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
33. Influence of chloride concentration on Stress corrosion cracking and crevice corrosion of austenitic stainless steel in saline environments10.3390/ma13245640 ↗
34. A highly sensitive, long-time stable Ag/AgCl ultra-micro sensor for in situ monitoring chloride ions inside the crevice using SECM10.1016/j.talanta.2024.126026 ↗
35. Crevice corrosion of X80 carbon steel induced by sulfate reducing bacteria in simulated seawater10.1016/j.bioelechem.2021.107933 ↗
36. A comparison study of crevice corrosion on typical stainless steels under biofouling and artificial configurations10.1038/s41529-022-00301-w ↗
37. The effect of applied stress on the crevice corrosion of 304 stainless steel in 3.5 wt% NaCl solution10.1016/j.corsci.2021.110039 ↗
38. A fabrication of iridium oxide film pH micro-sensor on Pt ultramicroelectrode and its application on in-situ pH distribution of 316L stainless steel corrosion at open circuit potential10.1016/j.snb.2017.08.219 ↗
39. Crevice corrosion behavior of 201 stainless steel in NaCl solutions with different pH values by in situ monitoring10.3390/ma17051158 ↗
40. Quasi-simultaneous electrochemical/chemical imaging of local Fe2+ and pH distributions on 316 L stainless steel surface10.1016/j.jelechem.2020.114107 ↗