Review on the impact of marine environment on the reliability of electronic packaging materials
Source abstract
Abstract
Marine environments pose significant challenges to the reliability of electronic packaging materials. This review summarizes the main degradation mechanisms and reliability impacts of electronic packaging materials under marine conditions, including salt spray corrosion, high humidity, thermal cycling, and mechanical shock. Salt spray corrosion initiates localized galvanic corrosion through chloride ion (Cl−) diffusion, creating corrosion pits and stress concentration, thereby accelerating electrochemical-mechanical coupled failures. High humidity promotes moisture ingress into polymer packaging materials, resulting in hygroscopic plasticization, weakened interfacial adhesion, and delamination failure. Thermal cycling, due to mismatched coefficients of thermal expansion (CTE), induces growth of interfacial intermetallic compound (IMC) layers at solder joints and creep-fatigue interactions, further promoting interfacial crack propagation. Mechanical shock generates transient, high-strain-rate loading, rapidly initiating and propagating cracks within brittle packaging structures, ultimately leading to structural failure. Additionally, this paper discusses the current status and limitations of Physics of Failure (PoF)-based reliability models such as the Coffin-Manson and Arrhenius models for evaluating electronic packaging reliability in marine environments. Finally, it suggests that future studies should further develop multiphysics coupling models to more accurately predict long-term material performance under extreme marine conditions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Material Properties and Processing · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (77)
Show source-provided references
1. Influence of paint on steel corrosion for marine applications10.4236/jsemat.2014.44022 ↗
2. Effect of nickel-based laser coatings on phase composition and corrosion behaviour of titanium alloy for offshore application10.1016/j.matpr.2020.04.671 ↗
3. Low-field time-dependent dielectric integrity10.1109/tr.1980.5220804 ↗
4. Electromigration failure modes in aluminum metallization for semiconductor devices10.1109/proc.1969.7340 ↗
5. On the relationship between moisture uptake and mechanical property changes in a carbon fibre/epoxy composite10.1177/00219983221091465 ↗
6. Reliability and failure analysis in designing a typical operation amplifier10.1109/IPFA.2010.5531973 ↗
7. Influence of rapid thermal cycling on the microstructures of single SnAgCu and SnPb solder joints10.1109/ICEPT.2013.6756596 ↗
8. Corrosion of electronic materials and devices10.1126/science.234.4774.340 ↗
9. Method of determining reliability screens for time dependent dielectric breakdown10.1109/IRPS.1979.362863 ↗
10. Effect of simulation methodology on solder joint crack growth correlation and fatigue life prediction10.1115/1.1413764 ↗
11. Crevice corrosion study of materials for propulsion applications in the marine environment10.14773/CST.2015.14.6.288 ↗
12. Physically based models of electromigration: from Black’s equation to modern TCAD models10.1016/j.microrel.2010.01.007 ↗
13. Study on graphene modified organic anti-corrosion coatings: a comprehensive review10.1016/j.jallcom.2019.07.256 ↗
14. Package structural integrity analysis considering moisture
15. Peridynamic analysis of marine composites under shock loads by considering thermomechanical coupling effects10.3390/jmse6020038 ↗
16. Corrosion behavior of 316L stainless steel coatings on ZE41 magnesium alloy in chloride environments10.1016/j.surfcoat.2019.124994 ↗
17. Shock and impact reliability of electronic assemblies with perimeter vs full array layouts: a numerical comparative study10.1515/jmbm-2022-0058 ↗
18. Salt spray corrosion of mechanical junctions of magnesium castings10.1007/978-3-319-48223-1_92 ↗
19. Dynamic fracture mechanics10.1007/978-3-642-19240-1_7 ↗
20. Corrosion study on BGA assemblies10.1109/PanPacific.2016.7428402 ↗
21. Estimation and test for the parameters of the arrhenius model10.1002/qre.4680030404 ↗
22. In-situ characterization of moisture absorption and hygroscopic swelling of an epoxy molding compound for electronic packaging10.1007/s10973-021-10941-w ↗
23. Corrosion behavior of 700L automotive beam steel in marine atmospheric environment10.3390/ma17204964 ↗
24. Failure mechanism of EB-PVD thermal barrier coatings under the synergistic effect of thermal shock and CMAS corrosion10.3390/coatings12091290 ↗
25. Corrosion behavior of materials Al5083 alloy, 316L stainless steel and A681 carbon steel in seawater10.35219/mms.2021.2.07 ↗
26. High strain rate compression behavior for Sn–37Pb eutectic alloy, lead-free Sn–1Ag–0.5Cu and Sn–3Ag–0.5Cu alloys10.1016/j.microrel.2009.01.002 ↗
27. Influence of marine climate on corrosion of common materials for electronic equipment10.1109/Radar53847.2021.10028025 ↗
28. Corrosion control of airborne electronic equipment in environment of marine climate10.1007/978-981-32-9437-0_58 ↗
29. Study of interface reliability in QFN device under hygro-thermal environment10.1109/ICEPT.2008.4607146 ↗
30. Failure characteristics and mechanisms of Sn-based solder interconnections under vibrational conditions10.1109/ICEPT63120.2024.10668776 ↗
31. Effect of aging on mechanical properties of high temperature Pb-rich solder joints10.1016/j.microrel.2018.03.009 ↗
32. Ridge regression based development of norris-landzberg acceleration factors and goldmann constants for leadfree electronics
33. Atmospheric corrosion behavior of low-alloy steels in a tropical marine environment10.1007/s42243-019-00316-9 ↗
34. Research on composite fretting behaviour of Au-plated copper wire spring contacts used in electrical connectors10.1109/HOLM.2019.8924029 ↗
35. Impact of 5% NaCl salt spray pretreatment on the long-term reliability of wafer-level packages with Sn-Pb and Sn-Ag-Cu solder interconnects10.1007/s11664-011-1705-y ↗
36. Salt spray corrosion and electrochemical corrosion property of anodic oxide films on ADC12 aluminum alloy10.1142/S0217984921505710 ↗
37. Sequential analysis of drop impact and thermal cycling of electronic packaging structures
38. Formation and evolution of intermetallic layer structures at SAC305/Ag/Cu and SAC0705-Bi-Ni/Ag/Cu solder joint interfaces after reflow and aging10.1007/s10854-014-2257-8 ↗
39. Understanding the impact response of lead-free solder at high strain rates10.1016/j.ijmecsci.2020.105416 ↗
40. Singular stress fields at corners in flip-chip packages10.1016/j.engfracmech.2012.02.010 ↗
41. A numerical method on thermal-humidity behavior of electronic packaging
42. Neville · 1995
43. A study of moisture and thermally induced die stresses in plastic ball grid array packages10.1109/ITHERM.2017.7992622 ↗
44. Failure mechanisms of thermomechanically loaded SnAgCu/plastic core solder ball composite joints in low-temperature Co-fired ceramic/printed wiring board assemblies10.1007/s11664-006-0066-4 ↗
45. Effect of thermal cycling and vibration on cracking in Sn-3.0Ag-0.5Cu solder bump10.1016/j.matpr.2021.10.222 ↗
46. Corrosion behavior of riveted joints with electrophoretic treatment in neutral salt spray environment10.1002/maco.202314097 ↗
47. Component reliability modeling through the use of bayesian networks and applied physics-based models10.1109/RAM.2018.8462986 ↗
48. Effect of acinetobacter sp. on corrosion behavior of 10MnNiCrCu steel in simulated marine environment10.20964/2021.06.55 ↗
49. Lifetime prediction of Cu-Al wire bonded contacts for different mould compounds10.1109/ECTC.2014.6897318 ↗
50. Towards a quantitative mechanistic understanding of the thermal cycling of SnAgCu solder joints10.1109/ECTC.2014.6897314 ↗
51. A new method for equivalent acceleration of JEDEC moisture sensitivity levels10.1109/ECTC.2008.4550084 ↗
52. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–RE alloys: RE=Ce, La, Nd, Y, Gd10.1016/j.corsci.2013.06.032 ↗
53. Polyalphaolefin oil/MgO-20 nanofluids coating shows corrosion resistance, high moisture resistance, and water resistance for electrical and electronic equipment10.3390/coatings13091576 ↗
54. Investigation of thermal-mechanical and moisture driven delamination in lead-free QFN packages during SMT reflow soldering process10.1109/ICEPT.2006.359847 ↗
55. Thermal cycling aging effect on the reliability and morphological evolution of SnAgCu solder joints10.1109/TEPM.2007.907575 ↗
56. Delamination of plasticized devices in dynamic service environments10.3390/mi15030376 ↗
57. Whole field vapor pressure modeling of QFN during reflow with coupled hygro-mechanical and thermo-mechanical stresses10.1109/ECTC.2002.1008314 ↗
58. A comprehensive solution for modeling moisture induced delamination in electronic packaging during solder reflow10.1016/j.microrel.2020.113791 ↗
59. Influence of humidity on the power cycling lifetime of SiC MOSFETs10.1109/TCPMT.2022.3223957 ↗
60. Simulation study of the high-G drop impact testing of microelectronic packaging products10.1109/ITherm51669.2021.9503272 ↗
61. Damage behavior of SnAgCu/Cu solder joints subjected to thermomechanical cycling10.1016/j.jallcom.2013.05.026 ↗
62. Comparative assessment of mechanical properties of HPS between electrochemical corrosion and spray corrosion10.1016/j.conbuildmat.2019.117735 ↗
63. Thermal-mechanical fatigue reliability of pbsnag solder layer of die attachment for power electronic devices10.1109/ICEPT.2009.5270615 ↗
64. Study on salt spray corrosion of Ni–graphite abradable coating with 80Ni20Al and 96NiCr–4Al as bonding layers10.1016/j.surfcoat.2011.03.007 ↗
65. Residual fatigue life prediction of ball bearings based on Paris law and RMS10.3901/CJME.2012.02.320 ↗
66. Growth kinetics of intermetallic compound in solder joints during thermal cycling: a review10.1109/EPTC53413.2021.9663867 ↗
67. Surface analysis of silver-plated circuit boards in a salt-spray environment10.1016/j.jallcom.2016.07.207 ↗
68. Research on ceramic package for high temperature electronic devices
69. Electrochemical corrosion failure mechanism of M152 steel under a salt-spray environment10.1007/s12613-015-1183-y ↗
70. Field studies of corrosion behaviour of printed circuit board and hot air solder levelling during the marine environment of industrial pollution10.1016/S1452-3981(23)17387-1 ↗
71. Electrochemical and salt spray corrosion behavior of copper alloy contact wires in chloride solution10.4028/www.scientific.net/MSF.789.622 ↗
72. Moisture absorption and void growing effects on failure of electronic packaging10.1109/ICEPT.2008.4607128 ↗
73. Moisture desorption and hygro-vapor-thermal induced interfacial delamination in underfilled FCBGA package during reflow process
74. The dynamic response of brittle materials under impact loading10.1515/ijnsns-2016-0019 ↗
75. Research on reliability of SnAg1.8/Cu solder joints in extreme environment
76. Failure analysis of printed circuit board solder joint under thermal shock10.3390/coatings13030572 ↗
77. Long term corrosion characteristics of metallic materials in marine environments10.1179/147842208X338938 ↗