journal article·2017-03-24Open access

Interaction between Deformation and Crack Initiation under Vickers Indentation in Na2O–TiO2–SiO2 Glasses

Garth Scannell, Denis Laille, Fabrice Célarié, Liping Huang, Tanguy Rouxel

Abstract

An observed minimum in the critical crack initiation load at Poisson's ratio (ν) of 0.21-0.22 in Na2O-TiO2-SiO2 glasses was investigated. Vickers indentation was used to examine hardness and average cracking length, fracture toughness was measured through the single-edge pre-cracked beam method (SEPB), and volumes of densification and shear flow around indents were measured using atomic force microscopy (AFM). Relations between the critical crack initiation load and hardness, average crack length, fracture toughness, and the volume fractions of densification and shear flow were studied. No correlations were observed between hardness, average crack length, or fracture toughness with the critical crack initiation load. A link between the minimum in crack initiation load and a change in deformation mechanisms (densification vs. shear flow) was observed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Semiconductor materials and devices · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Indentation deformation mechanism of isostatically compressed mixed alkali aluminosilicate glasses10.1016/j.jnoncrysol.2015.06.028 ↗
2. A Ti K-edge EXAFS study of the medium range environment around Ti in oxide glasses10.1016/S0022-3093(98)00846-1 ↗
3. Coordination chemistry of Ti(IV) in silicate glasses and melts: II. Glasses at ambient temperature and pressure10.1016/0016-7037(96)00145-7 ↗
4. Deformation and cracking behavior of glasses indented with diamond tips of various sharpness10.1016/j.jnoncrysol.2012.01.052 ↗
5. Micromechanics of crack nucleation during indentations
6. Shear deformation under pyramidal indentations in soda-lime glasses10.1007/BF00752121 ↗
7. A Ti L-edge X-ray absorption of Ti-silicate glasses10.1007/s002690100208 ↗
8. Load dependence of densification in glass during Vickers indentation test10.2109/jcersj2.119.110 ↗
9. Effect of densification on crack initiation under Vickers indentation test10.1016/j.jnoncrysol.2010.07.015 ↗
10. Hardness, toughness, and brittleness: an indentation analysis10.1111/j.1151-2916.1979.tb19075.x ↗
11. Intrinsic plasticity or brittleness of metallic glasses10.1080/09500830500080474 ↗
12. High-pressure effects on oxide glasses: I, densification in a rigid state10.1111/j.1151-2916.1963.tb13776.x ↗
13. Glass science in the United States: current status and future directions10.1111/ijag.12058 ↗
14. Gwyddion: an open-source software for SPM data analysis10.2478/s11534-011-0096-2 ↗
15. Evaluation of fracture toughness for ceramic materials by a single-edge-precracked-beam method10.1111/j.1151-2916.1988.tb05049.x ↗
16. High-temperature Raman spectroscopy of Na2TiSi2O7 glass and melt: coordination of Ti4+ and nature of the configurational changes in the liquid10.1127/ejm/10/1/0049 ↗
17. Driving force for indentation cracking in glass: composition, pressure and temperature dependence10.1098/rsta.2014.0140 ↗
18. Towards glasses with better indentation cracking resistance10.1016/j.crme.2013.10.008 ↗
19. Structure and properties of Na2O-TiO2-SiO2 glasses: role of Na and Ti on modifying the silica network10.1016/j.jnoncrysol.2016.06.028 ↗
20. Elastic properties and indentation cracking behavior of Na2O-TiO2-SiO2 glasses10.1016/j.jnoncrysol.2015.09.011 ↗
21. A new low-brittleness glass in the soda-lime-silica glass family10.1111/j.1151-2916.1998.tb02649.x ↗
22. Brittleness of glass10.1016/S0022-3093(99)00348-8 ↗
23. Composition dependence of indentation deformation and indentation cracking in glass10.1016/j.actamat.2013.06.034 ↗
24. Wide-range stress intensity factor expressions for ASTM E 399 standard fracture toughness specimens10.1007/BF00032844 ↗
25. “Determination of the toughness of glass: single edge precracked beam procedure,”
26. Towards ultrastong glasses10.1002/adma.201102795 ↗
27. Indentation-induced densification of soda-lime silicate glass10.3139/146.101478 ↗
28. Effects of the indenter shape on the indentation-induced densification of soda-lime glass10.1557/jmr.2010.0287 ↗