Evaluation of Sinking-In and Cracking Behavior of Soda-Lime Glass under Varying Angle of Trigonal Pyramid Indenter
Source abstract
Abstract
It is well known that glass undergoes elastic and inelastic deformation under a sharp diamond indenter. Although brittle or less-brittle behavior of glass must be connected with such mechanical responses of glass under the indenter, there has been limited research on in-situ deformation behavior of glass during the loading and unloading indentation cycle. This is because most indentation tests were conducted using a commercial hardness tester for which this information is not available. In this study, the in-situ sinking-in region of glass during indentation test is determined using a custom-designed indentation microscope with trigonal pyramid indenters having different tip angles. It is found that both the shape of contact region and the amount of sinking-in are affected by indenter geometries, and that the projected contact region of the glass sample under Berkovich indenter is not a regular triangle, but a concave triangle with bowed-in edges. This is due to the larger amount of sinking-in under the face than under the ridge of indenter. It is also found that these deformation behaviors of glass are inseparably linked with contact damage or cracking in glass.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Metal and Thin Film Mechanics · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Indentation deformation/fracture of normal and anomalous glasses10.1016/0022-3093(79)90154-6 ↗
2. The area of contact between a small sphere and a flat surface10.1080/01418618108236169 ↗
3. The response of solids to elastic/plastic indentation I. Stresses and residual stresses10.1063/1.329930 ↗
4. Kinetics of indentation cracking in glass10.1111/j.1151-2916.1993.tb03726.x ↗
5. Direct observation of indentation cracking in glass and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
6. Contact area determination in indentation testing of elastomers10.1557/JMR.2009.0093 ↗
7. Elastic-plastic behaviour in materials loaded with a spherical indenter10.1023/A:1018552222072 ↗
8. Fischer-Cripps · 200710.1007/978-0-387-68188-7 ↗
9. Green · 199810.1017/CBO9780511623103 ↗
10. Deformation and cracking behavior of glasses indented with diamond tips of various sharpness10.1016/j.jnoncrysol.2012.01.052 ↗
11. Johnson · 1987
12. Constitutive modeling of the densification process in silica glass under hydrostatic compression10.1016/j.actamat.2013.07.067 ↗
13. Micropillar testing of amorphous silica10.1111/j.2041-1294.2011.00075.x ↗
14. Constitutive law for the densification of fused silica, with applications in polishing and microgrinding10.1111/j.1151-2916.1996.tb08748.x ↗
15. Lawn · 199310.1017/CBO9780511623127 ↗
16. Kinetics of shear-activated indentation crack initiation in soda-lime glass10.1007/BF00547596 ↗
17. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
18. Indentation of elastic solids with a rigid Vickers pyramidal indenter10.1016/j.mechmat.2006.04.006 ↗
19. Residual stress effects in sharp-contact cracking: I. Indentation fracture mechanics10.1007/BF00551043 ↗
20. Optical indentation microscopy – a new family of instrumented indentation testing10.1080/14786430600788947 ↗
21. In-situ observation of cube-corner indentation of soda-lime glass and fused silica10.1111/j.1551-2916.2004.01494.x ↗
22. Elastic indentation response of float glass surfaces10.1111/j.1551-2916.2009.03377.x ↗
23. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
25. Driving force for indentation cracking in glass: composition, pressure and temperature dependence10.1098/rsta.2014.0140 ↗
26. Elastic recovery in the unloading process of pyramidal microindentation10.1557/JMR.2003.0224 ↗
27. Instrumented indentation microscope: a powerful tool for the mechanical characterization in microscales10.1557/jmr.2006.0276 ↗
28. Instrumented pyramidal and spherical indentation of polycrystalline graphite10.1557/jmr.2004.19.1.228 ↗
29. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
30. Composition dependence of indentation deformation and indentation cracking in glass10.1016/j.actamat.2013.06.034 ↗
31. Cone crack nucleation at sharp contacts10.1111/j.1151-2916.1992.tb05522.x ↗
32. Depth-sensing indentation at macroscopic dimensions10.1557/JMR.2002.0388 ↗
33. Composition- and structure-dependence of brittleness in glass
34. Elastic stress fields causes by indenting brittle materials10.1080/01418618208236917 ↗
35. Direct observation of indentation deformation and cracking of silicate glasses10.1557/jmr.2015.214 ↗
36. Effects of indenter geometry on indentation-induced densification of soda-lime glass10.1557/JMR.2010.0287 ↗