Dimensional Deviation Management for Selective Laser Melted Ti6Al4V Alloy Blade
Source abstract
Abstract
Selective laser melting (SLM) is prone to generate large thermal stresses, which could induce a heavy geometric change in the parts. In this study, Ti6Al4V blade was prepared by Selective laser melting (SLM). Microstructure, dimensional deviation and residual stress were investigated. Microstructure is acicular α' martensite in prior columnar β grain. The smaller the grain size, the larger the dimensional deviation. The directions of dimensional deviation at the leading and trailing edges of blade are opposite to those in the middle. The distribution of dimensional deviation exhibits a parabolic law at the trailing edge of blade. The thermal stress is big at the edges of the blade body. The large tensile stress along the edges of the blade body caused the edges to deform toward the suction side of the blade. The residual stress distribution of the pressure surface by the XRD measured has a good agreement with thermal stress distribution by calculated.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Stress and deformation evaluations of scanning strategy effect in selective laser melting.10.1016/j.addma.2016.05.007 ↗
2. Titanium alloy production technology, market prospects and industry development.10.1016/j.matdes.2010.09.011 ↗
3. Thermal and mechanical finite element modeling of laser forming from metal and ceramic powders.10.1016/j.actamat.2003.08.028 ↗
4. Laser additive manufacturing of metals10.1007/978-3-642-41341-4_6 ↗
5. A software for diffraction stress factor calculations for textured materials.10.1017/s0885715612000267 ↗
6. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting.10.1016/j.ijfatigue.2016.05.001 ↗
7. Additive manufacturing of metals.10.1016/j.actamat.2016.07.019 ↗
8. Finite element simulation of the temperature and stress fields in single layers built without-support in selective laser melting.10.1016/j.matdes.2013.05.070 ↗
9. Evaluation of residual stresses and strains using the Eigenstrain Reconstruction Method.10.1016/j.ijsolstr.2010.03.002 ↗
10. Assessing and comparing influencing factors of residual stresses in selective laser melting using a novel analysis method.10.1177/0954405412437085 ↗
11. Efficient predictive model of part distortion and residual stress in selective laser melting.10.1016/j.addma.2017.08.014 ↗
12. Understanding the residual stress distribution through the thickness of atmosphere plasma sprayed (APS) thermal barrier coatings (TBCs) by high energy synchrotron XRD; digital image correlation (DIC) and image based modelling.10.1016/j.dib.2017.06.016 ↗
13. Modeling temperature and residual stress fields in selective laser melting.10.1016/j.ijmecsci.2017.12.001 ↗
14. 13 - Aerospace applications of laser additive manufacturing10.1016/b978-0-08-100433-3.00013-0 ↗
15. Spatial variation of melt pool geometry, peak temperature and solidification parameters during laser assisted additive manufacturing process.10.1179/1743284714y.0000000701 ↗
16. Residual stresses in selective laser sintering and selective laser melting.10.1098/rspa.2018.0295 ↗
17. An improved prediction of residual stresses and distortion in additive manufacturing.10.1016/j.commatsci.2016.10.003 ↗
18. Finite element analysis of temperature distribution in single metallic powder layer during metal laser sintering.10.1016/j.ijmachtools.2006.09.025 ↗
19. Methods of measuring residual stresses in components.10.1016/j.matdes.2011.08.022 ↗
20. Selective laser melting (SLM) and topology optimization for lighter aerospace componentes.10.1016/j.prostr.2016.02.039 ↗
21. Application of thermohydrogen processing to Ti6Al4V alloy blade isothermal forging.10.1016/j.msea.2012.10.056 ↗
22. Analysis of the growth morphology of TiB and the microstructure refinement of the coatings fabricated on Ti-6Al-4V by laser boronizing.10.1021/cg0608099 ↗
23. Additive manufacturing of titanium alloy for aircraft components.10.1155/2019/2903920 ↗
24. Process maps for predicting residual stress and melt pool size in the laser-based fabrication of thin-walled structures.10.1115/1.2335852 ↗
25. AlSi12 in-situ alloy formation and residual stress reduction using anchorless selective laser melting.10.1016/j.addma.2015.06.003 ↗
26. Copper-modified Ti6Al4V alloy fabricated by selective laser melting with pro-angiogenic and anti-inflammatory properties for potential guided bone regeneration applications.10.1016/j.msec.2018.04.046 ↗
27. Selective laser melting of Ti6Al4V alloy for biomedical applications: temperature monitoring and microstructural evolution.10.1016/j.jallcom.2013.08.183 ↗
28. Material response to thermal loading due to short pulse laser heating.10.1016/s0017-9310(01)00026-6 ↗
29. Selective laser melting of titanium alloys and titanium matrix composites for biomedical applications: a review.10.1002/adem.201500419 ↗
30. A review on biomedical titanium alloys: recent progress and prospect.10.1002/adem.201801215 ↗
31. Additive manufacturing of titanium alloys by electron beam melting: a review.10.5301/jabfm.5000371 ↗
32. Horizontal dimensional accuracy prediction of selective laser melting.10.1016/j.matdes.2018.08.059 ↗
33. Determination of melt pool dimensions using DOE-FEM and RSM with process window during SLM of Ti6Al4V powder.10.1016/j.optlastec.2018.01.013 ↗