Influence of Surface Finishes and a Calcium Phosphate-Based Consolidant on the Decay of Sedimentary Building Stones Due to Acid Attack
Source abstract
Abstract
Natural stone has long been used as a building material because of its physical-mechanical resistance and its aesthetic appeal. However, over the last century increasing industrial activity has created a more polluted, more acidic urban atmosphere that can cause serious damage to many buildings and historic monuments, and in particular those made with carbonate rocks, which are most prone to decay. In order to mitigate these effects, a number of phosphate-based consolidants have been developed. These are applied to the surface of the rock and are highly compatible with the carbonated substrate. Research about the role of the surface and its different possible finishes in the transmission of the agents that damage or protect the stone would therefore be very useful, both when choosing the most suitable stone for new constructions and when restoring historic buildings. The main objective of this research was to determine whether the roughness of three types of surface finish (saw-cut, honed and bush-hammered) influences the durability of four types of natural stone (two calcarenites, one travertine and one sandstone) widely used in Andalusia (Spain). The efficacy of a calcium phosphate-based consolidant as a mitigator of deterioration in polluted urban environments was also studied and to this end the physical properties of non-treated and treated samples were measured and compared. The samples were then exposed to artificial atmospheres with SO2 pollution in order to assess the damage caused to each surface finish. The results indicate that all the surface finishes were vulnerable to the decay caused by acidic atmospheres, although the saw-cut finish was less affected by acid attack, perhaps because it did not require additional industrial processing. The mineral composition and texture of the rocks were critical factors in terms of the amount and type of decay they suffered, and the travertine and sandstone were more resistant to deterioration than the calcarenites. Similarly, the pore system of each rock was decisive in the penetration of the consolidant, so ensuring that the treated samples were more resistant to acid attack without significantly altering the water vapor permeability, the color or the roughness of the surface.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Building materials and conservation · Conservation Techniques and Studies · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (97)
Show source-provided references
1. Amoroso · 2002
2. Conservation of calcareous stone monuments: screening different diammonium phosphate based formulations for countering phototrophic colonization10.1016/j.culher.2017.03.002 ↗
3. Deposition of sulfur dioxide to building stones: the influence of the ambient concentration on the deposition velocity10.1007/s00254-008-1414-x ↗
4. The influence of petrophysical properties on the salt weathering of porous building rocks10.1007/s00254-006-0475-y ↗
5. Influence of surface roughness on color changes in building stones10.1002/col.10178 ↗
6. Berns · 2000
7. Durability assessment to environmental impact of nano-structured consolidants on Carrara marble by field exposure tests10.1016/j.scitotenv.2016.10.004 ↗
8. The rate of darkening of material surfaces10.1201/b17004-30 ↗
9. Effectiveness of oxalic acid treatments for the protection of marble surfaces10.1016/j.matdes.2016.11.037 ↗
10. Weathering of limestone building material by mixed sulfate solutions. Characterization of stone microstructure, reaction products and decay forms10.1016/j.matchar.2007.12.003 ↗
11. Gypsum: a review of its role in the deterioration of building materials10.1007/s00254-006-0566-9 ↗
12. Acid deposition and the deterioration of stone: a brief review of a broad topic
13. Characterization of the properties of the Montoro sandstone, its alterations and its applicability for construction
14. Behavior of brick samples in aggressive environments10.1023/a:1005142612180 ↗
15. Rock fabric heterogeneity and its influence on the petrophysical properties of a building limestone: lede stone (Belgium) as an example10.1016/j.enggeo.2016.11.007 ↗
16. Bulk and surface properties in stone conservation10.1201/NOE0415450188.ch1 ↗
17. Consolidation of lime mortars with ethyl silicate, nanolime and barium hydroxide. Effectiveness assessment with microdrilling data10.1016/j.culher.2017.07.006 ↗
18. Calcium orthophosphates in nature, biology and medicine10.3390/ma2020399 ↗
19. Calcium orthophosphates: occurrence, properties, biomineralization, pathological calcification and biomimetic applications10.4161/biom.18790 ↗
20. Model study of the first steps in the deterioration of calcareous stone I. Initial surface sulphite formation on calcite10.1016/0169-4332(94)90103-1 ↗
21. Model study of the first steps in the deterioration of calcareous stone III. Manganese and iron mediated sulphation of natural stone10.1016/0169-4332(94)90062-0 ↗
22. Influence of the petrophysical and durability properties of carbonate rocks on the deterioration of historic constructions in Tebessa (northeastern Algeria)10.1007/s10064-018-1410-7 ↗
23. Consolidation of carbonate stones: influence of treatment procedures on the strengthening action of consolidants10.1016/j.culher.2011.07.003 ↗
24. Natural biocides for the conservation of stone cultural heritage: a review10.1016/j.culher.2019.01.005 ↗
25. Non-destructive testing for the assessment of granite decay in heritage structures compared to quarry Stone10.1016/j.ijrmms.2012.12.048 ↗
26. TEOS-based treatments for stone consolidation: acceleration of hydrolysis-condensation reactions by poulticing10.1007/s10971-014-3610-3 ↗
27. Brushing, poultice or immersion? The role of the application technique on the performance of a novel hydroxyapatite-based consolidating treatment for limestone10.1016/j.culher.2014.05.009 ↗
28. Travertinos coloreados en la Cordillera Bética (SE de la Península Ibérica). Situación geológica y características petrofísicas10.21701/bolgeomin.128.2.013 ↗
29. Effect of relative humidity and grain size on the reaction rates of marble at high concentrations of SO2
30. Hydroxyapatite coatings for marble protection: optimization of calcite covering and acid resistance10.1016/j.apsusc.2016.01.202 ↗
31. Color changes in architectural limestones from pollution and cleaning10.1002/col.20322 ↗
32. Soiling of building stones in urban environments10.1016/s0360-1323(02)00017-3 ↗
33. Hamilton · 2009 · 30810.1007/978-0-387-84893-8 ↗
34. Effect of dry deposition of NOx and SO2 gaseous pollutants on the degradation of calcareous building stones10.1016/0960-1686(92)90288-v ↗
35. Determining the weathering classification of stone cultural heritage via the analytic hierarchy process and fuzzy inference system10.1016/j.culher.2020.02.011 ↗
36. The Oceanus statue of the Fontana di Trevi (Rome): the analysis of black crust as a tool to investigate the urban air pollution and its impact on the stone degradation10.1016/j.scitotenv.2017.03.185 ↗
37. Study of the effects of salt crystallization on degradation of limestone rocks10.2451/2013PM0007 ↗
38. The mineralogical composition of sandstone and its effect on sulphur dioxide deposition10.3989/mc.2008.v58.i289-290.86 ↗
39. Efflorescence on thin sections of calcareous stones10.1016/j.culher.2003.09.002 ↗
40. A comparative study of porous limestones treated with silicon-based strengthening agents10.1016/j.porgcoat.2007.09.020 ↗
41. Changes on the surface properties of foliated marbles at different cutting orientations10.1016/j.conbuildmat.2019.06.099 ↗
42. Ammonium phosphates as consolidating agents for carbonatic stone materials used in architecture and cultural heritage: preliminary research10.1080/15583058.2010.495445 ↗
43. Gypsum formation in non-calcareous building sandstone: a case study of Scrabo sandstone10.1002/esp.232 ↗
44. Particle-modified consolidants: a study on the effect of particles on sol-gel properties and consolidation effectiveness10.1016/j.culher.2006.10.002 ↗
45. The influence of rock fabric in the durability of two sandstones used in the Andalusian Architectural Heritage (Montoro and Ronda, Spain)10.1016/j.enggeo.2015.08.009 ↗
46. Evaluation of stone durability using a combination of ultrasound, mechanical and accelerated aging tests10.1088/1742-2132/10/3/035003 ↗
47. The pore system of sedimentary rocks as a key factor in the durability of building materials10.1016/j.enggeo.2011.01.008 ↗
48. Gypsum crust as a source of calcium for the consolidation of carbonate stones using a calcium phosphate-based consolidant10.1016/j.conbuildmat.2017.03.155 ↗
49. Methods for measuring rock surface weathering and erosion: a critical review10.1016/j.earscirev.2014.04.006 ↗
50. Diammonium hydrogen phosphate (DAP) as a consolidant in carbonate stones: impact of application methods on effectiveness10.1016/j.culher.2019.09.003 ↗
51. Acid-resistant coatings on marble10.1111/jace.14355 ↗
52. Hydroxyapatite-based consolidant and the acceleration of hydrolysis of silicate-based consolidants10.1016/j.culher.2014.01.001 ↗
53. New treatment for corrosion-resistant coatings for marble and consolidation of limestone
54. Nucleation, growth and evolution of calcium phosphate films on calcite10.1016/j.jcis.2014.08.018 ↗
55. Drilling resistance: overview and outlook10.1127/1860-1804/2007/0158-0665 ↗
56. Limestone biodeterioration: a review on the Portuguese cultural heritage scenario10.1016/j.culher.2018.07.008 ↗
57. Photocatalytic activity of TiO2-SiO2 nanocomposites applied to buildings: influence of particle size and loading10.1016/j.apcatb.2013.01.021 ↗
58. Atmospheric aerosol and soiling of external surfaces in an urban environment10.1016/s1352-2310(97)00507-4 ↗
59. New insight on the interaction of diammonium hydrogenphosphate conservation treatment with carbonatic substrates: a multi-analytical approach10.1016/j.microc.2016.02.008 ↗
60. Price · 2011 · 164
61. Přikryl · 2007 · 330
62. Salt weathering: influence of evaporation rate, supersaturation and crystallization pattern10.1002/(sici)1096-9837(199903)24:3<191::aid-esp942>3.0.co;2-g ↗
63. Petrographic of limestone cultural heritage as the basis of a methodology to rock replacement and masonry assessment: cartagena de Indias case of study10.1016/j.cscm.2019.e00281 ↗
64. Damages caused to European monuments by air pollution: assessment and preventive measures10.1201/b17004-15 ↗
65. Effectiveness of hydroxyapatite as a consolidating treatment for lithotypes with varying carbonate content and porosity
66. Consolidation if calcareous and siliceous sandstones by hydroxiapatite: comparision with a TEOS based consolidant10.1016/j.culher.2012.11.029 ↗
67. Comparative study between ammonium phosphate and ethyl silicate towards conservation of prehistoric paintings in the magura cave (Bulgaria)10.3390/coatings10030250 ↗
68. Conversion of calcium sulfate dihydrate into calcium phosphates as a route for conservation of gypsum stuccoes and sulfated marble10.1016/j.conbuildmat.2018.03.075 ↗
69. Phosphate-based treatments for conservation of stone10.21809/rilemtechlett.2017.34 ↗
70. Hydroxyapatite and other calcium phosphates for the conservation of cultural heritage: a review10.3390/ma11040557 ↗
71. The use of hydroxyapatite as a new inorganic consolidant for damaged carbonate stones10.1016/j.culher.2011.02.005 ↗
72. Granitic building stone decay in an urban environment: a case of authigenic kaolinite formation by heterogeneous sulphur dioxide attack10.1016/B978-044450517-0/50124-0 ↗
73. The efficiency of nanolime and dibasic ammonium phosphate in the consolidation of beige limestone from the Pasargadae World Heritage Site10.1007/s12520-019-00863-y ↗
74. New nanomaterials for applications in conservation and restoration of stony materials: a review10.3989/mc.2017.07616 ↗
75. X-ray radiography and tomography for monitoring the penetration depth of consolidants in Opuka - the building stone of Prague monuments10.1016/j.culher.2012.01.010 ↗
76. Transforming gypsum into calcium phosphate: a better way to preserve lime paint layers on natural stone?
77. Relationships among mechanical, physical and petrographic properties of Siwalik sandstones, Central Nepal Sub-Himalayas10.1016/j.enggeo.2006.10.005 ↗
78. Simulation of the dissolution of weathered versus unweathered limestone in carbonic acid solutions of varying strength10.1002/esp.1441 ↗
79. Black crusts on travertine: factors controlling development and stability10.1007/s00254-008-1297-x ↗
80. Surface change and decay of sandstone samples exposed to a polluted urban atmosphere over a six-year period: belfast, Northern Ireland10.1016/s0360-1323(03)00077-5 ↗
81. 2003
82. 2010
83. 2011
84. 2002
85. 2013
86. 2013
87. Initial stages of carbonate weathering: climate chamber studies under realistic pollution conditions10.1007/s00254-008-1440-8 ↗
88. An experimental study on the influence of surface finishing on the weathering of a building low-porous limestone in coastal environments10.1016/j.enggeo.2012.12.013 ↗
89. Rough and polished travertine building stone decay evaluated by a marine aerosol aging test10.1016/j.conbuildmat.2010.01.011 ↗
90. Digital image processing of weathered stone caused by efflorescences: a tool for mapping and evaluation of stone decay10.1016/j.conbuildmat.2010.10.003 ↗
91. Evaluation of the petrophysical properties of sedimentary building stones in order to establish quality criteria10.1016/j.conbuildmat.2012.12.026 ↗
92. Surface changes on crystalline stones due to salt crystallisation10.1007/s12665-012-2003-6 ↗
93. Influence of surface finish and composition on the deterioration of building stones exposed to acid atmospheres10.1016/j.conbuildmat.2015.12.125 ↗
94. Vergès-Belmin · 2008
95. Völz · 200110.1002/3527600485 ↗
96. Historical overview
97. Effect of the addition of hydroxyl-terminated polydimethylsiloxane to TEOS-based stone consolidants10.1016/j.culher.2009.07.002 ↗