Achieving high-quality silver sintered joint for highly-reliable schottky barrier diodes via pressureless method
Source abstract
Abstract
The fabrication of silver joints was done using the pressureless sintering technology to suit the demand of high-reliability schottky barrier diodes (SBD). Porosity of 10.6% and shear strength of 39.6 MPa were reached under the optimized parameters of 290°C sintering temperature and 40 min residence time. The sintered joint demonstrated good mechanical/thermal/electrical performance in the ultimate reliability assessment testing, including the temperature cycling test, second sintering test, steady-state lifetime test, and intermittent lifetime test. This study demonstrated the viability of pressureless sintering of silver joints with good high-temperature reliability, which has significant application potential for aeronautical high-reliability power electronics.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Electrical Contact Performance and Analysis · GaN-based semiconductor devices and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
2. A review on die attach materials for SiC-based high-temperature power devices10.1007/s11663-010-9365-5 ↗
3. Microstructural studies and bonding strength of pressureless sintered nano-silver joints on silver, direct bond copper (DBC) and copper substrates aged at 300 °C10.1016/j.jallcom.2016.06.132 ↗
4. Enhancement of creep resistance and thermal behavior of eutectic Sn-Cu lead-free solder alloy by Ag and In-additions10.1016/j.matdes.2012.04.007 ↗
5. Pressureless sintering of nanosilver paste at low temperature to join large area (≥100 mm2) power chips for electronic packaging10.1016/j.matlet.2014.04.127 ↗
6. Low temperature joining of copper by Ag nanopaste: correlation of mechanical properties and process parameters10.1007/s40194-016-0381-1 ↗
7. Photocurrent spectroscopic study of temperature-dependent photoresponse and valence-band splitting in MnAl2S4 layers10.1007/s11664-014-3248-5 ↗
8. Correction to: fracture of Sn-3.5%Ag solder alloy under creep10.1007/s11664-000-0119-z ↗
9. Correction to: fracture of Sn-3.5%Ag solder alloy under creep10.1007/s11664-018-6588-8 ↗
10. Investigations of interfacial reactions of Sn-Zn based and Sn-Ag-Cu lead-free solder alloys as replacement for Sn-Pb solder10.1016/j.jallcom.2005.03.053 ↗
11. Comparison study of surge current capability of body diode of SiC MOSFET and SiC Schottky diode
12. Robust Ag nanoplate ink for flexible electronics packaging10.1039/c5nr00312a ↗
13. Silver nanosintering: a lead-free alternative to soldering10.1007/s00339-008-4807-5 ↗
14. Simplification of low-temperature sintering nanosilver for power electronics packaging10.1007/s11664-013-2561-8 ↗
15. Design and analysis of P-GaN/N-GaO based junction barrier Schottky diodes10.1109/TED.2021.3119261 ↗
16. Microstructural stability of Ag sinter joining in thermal cycling10.1007/s10854-012-0929-9 ↗
17. Reactive wetting, evolution of interfacial and bulk IMCs and their effect on mechanical properties of eutectic Sn-Cu solder alloy10.1016/j.cis.2011.05.005 ↗
18. Effects of nano-structured particles on microstructure and microhardness of Sn-Ag solder alloy10.1007/s10854-009-9981-5 ↗
19. Effects of Nano-TiO2 additions on thermal analysis, microstructure and tensile properties of Sn3.5Ag0.25Cu solder10.1016/j.matdes.2009.08.008 ↗
20. Brief review of nanosilver sintering: manufacturing and reliability10.1007/s11664-021-09078-1 ↗
21. Fabrication of interconnects using pressureless low temperature sintered Ag nanoparticles10.1016/j.matlet.2012.06.089 ↗
22. Rapid pressureless low-temperature sintering of Ag nanoparticles for high-power density electronic packaging10.1016/j.scriptamat.2013.08.031 ↗
23. Device based on polymer Schottky junctions and their applications: a review10.1109/ACCESS.2020.3030644 ↗
24. The pressureless sintering of micron silver paste for electrical connections10.1016/j.jallcom.2019.04.270 ↗
25. GaN-on-Si vertical Schottky and p-n diodes10.1109/LED.2014.2314637 ↗