journal article·2024-02-22Open access

Corrosion fatigue performance of modified 17-4PH in simulated geothermal environment

Zhipeng Li, Ming Sun, Hongguang Zhang, Weiwei Xu, Lianlian Wu

Abstract

Corrosion fatigue behavior of a new candidate material for geothermal turbine blade, modified 17-4PH, was investigated in detail. The environmental acceleration of crack growth rate was discussed in terms of∆K. Fracture surface and side surface were observed by SEM. The crack path on side surface was also analyzed by EBSD. Then, the corrosion mechanism was discussed. Striation width on the fracture surface was compared to the crack growth per cycle. Since pitting occurred during the corrosion fatigue test, anodic polarization test was exercised to measure the pitting potential, and the cause for the pitting was also discussed. The hardness was also characterized by micro-hardness test and auger electron mapping.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Fatigue fracture in polygrystalline molybdenum10.1016/0001-6160(70)90074-x ↗
2. Secondary cracking during surface crack growth under tensile fatigue loading10.1016/0013-7944(88)90220-2 ↗
3. 1985
4. Corrosion behaviour of different steel types in artificial geothermal fluids10.1016/j.geothermics.2019.05.018 ↗
5. Pitting corrosion of metals- A review of the critical factors10.1149/1.1838615 ↗
6. Fujii · 1976 · 213
7. Aging reactions in a 17-4PH stainless steel10.1016/s0254-0584(01)00460-6 ↗
8. 2008
9. Roles of hydrogen sulfided in the behavior of engineering alloys: a review of literature and experience
10. Evaluation of suitability of high-alloyed materials for geothermal applications in the north German basin10.5006/1.3676631 ↗
11. The influence of metallurgical structures on the mechanism of fatigue crack propagation10.1520/STP47230S ↗
12. Milella · 91
13. Milella · 788
14. Milella · 100
15. Use of crack-line loaded specimens for measuring plane-strain fracture toughness
16. Investigation of the mechanism for brittle-striation formation in low carbon steel fatigued in hydrogen gas (fractographic observation on fracture processes visualized by controlling load sequence and testing environment): (fractographic observation on fracture processes visualized by controlling load sequence and testing environment)10.1299/jmmp.5.370 ↗
17. The latest geothermal steam turbines
18. Corrosion resistance of materials for geothermal steam turbines10.1299/jsmeicope.2003.3._3-297_ ↗
19. Stress corrosion cracking susceptibility of 17-4PH turbine steel in aqueous environments10.1179/000705995798114159 ↗
20. Geothermal power plant cycles and main components
21. Relationship of microstructure transformation and hardening behavior of type 17-4PH stainless steel10.1016/s1005-8850(06)60050-9 ↗
22. The a.c. corrosion of stainless steel—II. The breakdown of passivity of ss304 in neutral aqueous solutions10.1016/0010-938x(85)90019-8 ↗
23. The a.c. corrosion of stainless steel—II. The polarization of ss304 and ss316 in acid sulfate solutions10.1016/0010-938x(85)90020-4 ↗
24. A comparison of stress corrosion cracking susceptibility of steam turbine blade materials for geothermal plants10.5006/2058 ↗