Microstructure-property-corrosion degradation during 475 °C aging of additively manufactured UNS S32205 duplex stainless steel: experimental and statistical assessment

Santosh Kumar, V. Shamanth, Seelam Srikanth, Rayappa Shrinivas Mahale, Manjunath G. Avalappa, S. P. Jagadish, Chennabasappa Hampali

Abstract

Duplex stainless steels fabricated by Laser Bed Powder Fusion (LPBF) exhibit refined and metastable microstructures that can be particularly sensitive to intermediate-temperature exposure. In this study, the effect of 475 °C thermal aging on the microstructural stability, mechanical performance, fracture behavior, and corrosion response of LPBF-fabricated UNS S32205 duplex stainless steel is systematically investigated. LPBF specimens were solution annealed and subsequently aged at 475 °C for durations ranging from 100 to 1,000 h, followed by detailed microstructural, mechanical, electrochemical, and fractographic characterization. Microstructural analysis indicates progressive ferrite decomposition during aging, leading to embrittlement and deterioration of mechanical and corrosion performance. These transformations result in significant strengthening at intermediate aging times, followed by strength saturation and a severe reduction in tensile ductility at prolonged exposure. One-way ANOVA confirms that aging induces statistically significant changes ( p < 0.001) in young’s modulus, yield strength, ultimate tensile strength, and elongation relative to the solution-annealed condition, while effect size analysis demonstrates that aging duration overwhelmingly governs mechanical variability. Canonical discriminant analysis provides a clear multivariate separation of aging conditions and establishes a direct correlation between the combined evolution of mechanical properties and fracture mode transition from ductile dimple rupture to quasi-cleavage and brittle fracture. Electrochemical testing in 3.5 wt% NaCl reveals a progressive deterioration in corrosion resistance with aging, consistent with chromium partitioning and passive film destabilization associated with ferrite spinodal decomposition. The results demonstrate that LPBF-fabricated UNS S32205 exhibits classical 475 °C embrittlement behavior, with enhanced sensitivity arising from its additively manufactured microstructure. This work provides a statistically validated, process-aware framework linking thermal aging to microstructure-property-corrosion degradation, offering critical guidance for the qualification and reliable deployment of LPBF duplex stainless-steel components in thermally exposed service conditions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Hydrogen embrittlement and corrosion behaviors in metals · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechanical Engineering, REVA University

School of Civil Engineering, REVA University

Department of Automation and Robotics, JSPM’s Rajarshi Shahu College of Engineering

Department of Mechanical Engineering, K. L. S. Gogte Institute of Technology

Department of Mechanical Engineering, Rao Bahaddur Y Mahabaleswarappa Engineering College

Mechanical Engineering department, HKBK College of Engineering

References (55)

Show source-provided references
1. Microstructure and mechanical characterization of AISI 4340 steel additively manufactured by Laser Powder Bed Fusion10.3390/met15040412 ↗
2. Standard reference test method for making potentiodynamic anodic polarization measurements
3. Standard test method for conducting potentiodynamic polarization resistance measurements10.1520/G0059-23 ↗
4. Standard test methods for tension testing of metallic materials10.1520/E0008_E0008M-25 ↗
5. Wire laser metal deposition of 22% Cr duplex stainless steel: as-deposited and heat-treated microstructure and mechanical properties10.1007/s10853-022-06878-6 ↗
6. Tailoring of the microstructure of laser powder bed fused Inconel 718 using solution annealing and aging treatments10.3390/met11060921 ↗
7. Tailoring of the microstructure of laser powder bed fused Inconel 718 using solution annealing aging treatments10.3390/met1106921 ↗
8. In situ characterisation of surface roughness and its amplification during multilayer single-track laser powder bed fusion additive manufacturing10.1016/j.addma.2023.103809 ↗
9. Physical simulation of additively manufactured super duplex stainless steels – microstructure and properties10.1016/j.addma.2020.101269 ↗
10. Element-resolved electrochemical analysis of the passivity of additively manufactured stainless steel 316L10.1016/j.corsci.2021.109576 ↗
11. Temperature‐Dependent Dynamic Strain aging in selective Laser melted 316L10.1002/adem.202001501 ↗
12. Influence of ageing time on microstructure, hardness and corrosion of UNS Zeron 100 super duplex stainless steel10.1088/1757-899x/1189/1/012016 ↗
13. Thermal aging behaviors of duplex stainless steels used in nuclear power plant: a review10.1016/j.jnucmat.2020.152693 ↗
14. Machine learning prediction and multivariate pattern recognition for optimizing the mechanical behavior of heat-treated LPBF-fabricated UNS S32205 duplex stainless steel10.1016/j.jmapro.2025.11.080 ↗
15. Microstructural, mechanical, and tribological evolution under different heat treatment conditions of inconel 625 alloy fabricated by selective laser melting10.1002/adem.202100966 ↗
16. Susceptibility to pitting and environmentally assisted cracking of 17-4PH martensitic stainless steel produced by laser beam melting10.3390/ma15207121 ↗
17. Effect of annealing temperature on the corrosion behavior of duplex stainless steel studied by in situ techniques10.1016/j.corsci.2011.07.019 ↗
18. Effects of nitrogen and tensile direction on stress corrosion cracking susceptibility of Ni-Free FECRMNC-Based duplex stainless steels10.3390/ma10030294 ↗
19. Precipitation of T1 and θ′ phase in Al-4Cu-1Li-0.25Mn during Age hardening: microstructural investigation and phase-field simulation10.3390/ma10020117 ↗
20. Spinodal decomposition in functionally graded super duplex stainless steel and weld metal10.1007/s11661-018-4600-9 ↗
21. Microstructure evolution and the influence on residual stress in metal additive manufacturing with analytics10.3390/cryst15050435 ↗
22. Utilization of brittle σ phase for strengthening and strain hardening in ductile VCrFeNi high-entropy alloy10.1016/j.msea.2018.11.136 ↗
23. Comparative analysis of minimum chip thickness, surface quality and BURR formation in Micro-Milling of wrought and selective laser melted TI6410.3390/mi14061160 ↗
24. Tensile properties and fracture analysis of Duplex (2205) and super duplex (2507) stainless steels, produced via laser powder bed fusion additive manufacturing10.3390/met14070838 ↗
25. An overview on additive manufacturing of duplex stainless steels: microstructure, mechanical properties, corrosion resistance, postheat treatment, and future perspectives10.1002/srin.202400463 ↗
26. Microstructure analysis of novel LPBF-processed duplex stainless steels correlated to their mechanical and corrosion properties10.1016/j.msea.2020.140432 ↗
27. Co-dependent microstructural evolution pathways in metastable δ-ferrite in cast austenitic stainless steels during thermal aging10.1016/j.jnucmat.2018.08.038 ↗
28. Kinetics of sigma phase precipitation in Niobium-Stabilized austenitic stainless steel and effect on the mechanical properties10.4028/www.scientific.net/msf.783-786.848 ↗
29. Influence of intermetallic precipitation on metallurgical, mechanical and pitting behavior of AISI 2205 duplex stainless steel welded joints10.1088/2053-1591/ab664c ↗
30. Effect of heat treatment on the microstructure duplex stainless steel 220510.1016/j.matpr.020.06.196 ↗
31. Effect of heat treatment on the microstructure of duplex stainless steel 220510.1016/j.matpr.2020.06.196 ↗
32. The anisotropic grain size effect on the mechanical response of polycrystals: the role of columnar grain morphology in additively manufactured metals10.1016/j.jmst.2023.10.010 ↗
33. Effect of reversion heat treatment on the mechanical properties of thermally embrittled UNS S32760 Duplex stainless steel10.4028/www.scientific.net/msf.830-831.127 ↗
34. Exploring the impact of cooling rate on microstructural features, mechanical properties, and corrosion resistance of a novel NB-Stabilized Super duplex stainless steel in shielded metal arc welding10.3390/cryst13081192 ↗
35. 748 K (475 °C) Embrittlement of duplex stainless steel: effect on microstructure and fracture behavior10.1007/s11661-016-3944-2 ↗
36. Investigation of stress corrosion cracking of austenitic, duplex and super duplex stainless steels under drop evaporation Test using synthetic seawater10.1590/1980-5373-mr-2018-0211 ↗
37. Nanostructure evolution and mechanical property changes during aging of a super duplex stainless steel at 30010.1016/j.msea.201.09.009 ↗
38. Nanostructure evolution and mechanical property changes during aging of a super duplex stainless steel at 300 °C10.1016/j.msea.2015.09.009 ↗
39. The effect of the selective laser melting mode on second phases precipitation in 316L steel during subsequent heat treatment10.1088/1757-899x/1029/1/012053 ↗
40. Additively manufactured maraging steel: influence of heat treatment on corrosion and mechanical properties10.3390/ma18091999 ↗
41. Stress corrosion cracking of 316L stainless steel additively manufactured with sinter-based material extrusion10.3390/ma16114006 ↗
42. Understanding Laves phase precipitation induced embrittlement of modified 9Cr–1Mo steel10.1007/s42452-018-0101-0 ↗
43. Dissolution of alpha-prime precipitates in thermally embrittled S2205-duplex steels during reversion-heat treatment10.1016/j.rinp.2015.10.004 ↗
44. The effect of microstructural changes on mechanical and electrochemical corrosion properties of duplex stainless steel aged for short periods10.3390/ma13235511 ↗
45. Effect of spinodal decomposition on the mechanical behavior of Fe–Cr alloys10.1016/j.msea.2010.01.020 ↗
46. Evolution of Fe-Rich phases in thermally processed aluminum 6061 powders for AM applications10.3390/ma15175853 ↗
47. Pitting corrosion of type 316L stainless steel elaborated by the selective laser melting Method: influence of Microstructure10.1007/s11665-021-05621-7 ↗
48. Effect of heat treatment on the modification of microstructure of selective laser melted (LPBF) IN718 and its consequences on mechanical behavior10.1557/jmr.2020.129 ↗
49. Influence of ferrite-austenite distribution in 2205 duplex stainless steel on high-temperature solution nitriding behaviour10.1016/j.surfcoat.2022.129134 ↗
50. Isothermal aging embrittlement in an Fe-22Cr-25Ni alloy10.1016/j.msea.2018.09.023 ↗
51. The low-temperature aging embrittlement in a 2205 duplex stainless steel10.1016/j.msea.2003.12.051 ↗
52. Effect of aging at different temperatures on microstructure evolution of 347H Heat-Resistant Steel-Welded joints10.3390/met15050518 ↗
53. Effect of heat treatment above the miscibility gap on nanostructure formation due to spinodal decomposition in Fe-52.85 at.%Cr10.1016/j.actamat.2017.12.008 ↗
54. Microstructure evolution and Σ-Phase precipitation kinetics of 2507 duplex stainless steel aging at 850 °C10.4028/www.scientific.net/amr.711.87 ↗
55. Resistance of thermally aged DSS 2304 against localized corrosion attack10.3390/met8121022 ↗