Fatigue performance control strategy of TC11 and TC17 linear friction welded joints via annealing treatment
Source abstract
Abstract
A post-weld annealing strategy was developed to control the high-cycle fatigue performance of dissimilar TC11/TC17 titanium alloy linear friction welded joints. By systematically varying the stress relief annealing temperature (590, 605, 630, and 650 °C), the microstructural evolution, residual stress, and mechanical properties were investigated. The results demonstrate that increasing the annealing temperature promotes the decomposition of metastable β phase and the precipitation of fine secondary α, which raises the α phase area fraction in the fracture zone; this effect saturates above 630 °C. Concurrently, the longitudinal tensile residual stress, which reaches 400 MPa in the as-welded state, is substantially relaxed and is essentially eliminated at 630 °C. These synergistic changes enable a monotonic increase in the fatigue limit from 453.3 MPa to 512.5 MPa as the temperature rises to 630 °C, after which the property stabilizes. Fracture toughness exhibits divergent trends among the weld zones: the KIC of the weld nugget zone and the TC17-side thermo-mechanically affected zone increases with annealing temperature, while that of the TC11-side zone decreases due to the globularization of lamellar α; all three zones stabilize at approximately 33 MPa m 1/2 and 40 MPa m 1/2 , respectively. Integrating the microstructural evolution, residual stress relief, and mechanical property improvements, the optimal stress relief annealing strategy is to apply a temperature of at least 630 °C, which ensures superior fatigue resistance and microstructural stability for TC11/TC17 linear friction welded joints.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Fatigue and fracture mechanics · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Key Laboratory of Strength and Structural Integrity
Aircraft Strength Research Institute of China
References (29)
Show source-provided references
1. Phase transformations during cooling in α + β titanium alloys10.1016/s0921-5093(97)00802-2 ↗
2. Study of the linear friction welding process of dissimilar Ti-6Al-4V-stainless steel joints10.1080/10426914.2016.1151048 ↗
3. Fracture behaviour of linear friction welds in titanium alloys
4. Measurement of strain in a titanium linear friction weldby neutron diffraction10.1016/s0921-4526(02)01514-4 ↗
5. Frictional heat induced morphological responses at the interface in rotary friction welding of austenitic alloys: corona-bond and heat-pattern10.1016/j.jmrt.2023.02.221 ↗
6. Machining the integral impeller and blisk of aero-engines: a review of surface finishing and strengthening technologies10.1007/s10033-017-0123-3 ↗
7. Manufacturing processes of integral blade rotors for turbomachinery, processes and new approaches10.3390/app10093063 ↗
8. On friction, heat input, and material flow initiation during friction stir welding: tool and process optimization10.3390/jmmp7010034 ↗
9. Texture development in Ti-6Al-4V linear friction welds10.1016/j.msea.2006.12.095 ↗
10. Microstructure characterization and mechanical properties of linear friction welded Ti-6Al-4V alloy10.1002/adem.200700034 ↗
11. Hot working of Ti-6Al-3Mo-2Zr-0.3Si alloy with lamellar α + β starting structure using processing map10.1016/j.matdes.2008.07.031 ↗
12. Microstructure evolution and mechanical properties of linear friction welded Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) titanium alloy joints10.1002/adem.200900185 ↗
13. Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint10.1179/1362171811y.0000000079 ↗
14. Thermal-mechanical and microstructural simulation of rotary friction welding processes by using finite element method10.3390/ma17040815 ↗
15. Microstructural features, tensile properties, and impact toughness of linear friction welded high-temperature alloy joints for blisk assembly applications10.1155/2022/2233443 ↗
16. Effect of friction time on heat distribution, material flow, and microstructure of friction welding of dissimilar steels
17. Effect of the forging pressure on the microstructure and residual stress development in Ti-6Al-4V linear friction welds10.1016/j.actamat.2009.07.055 ↗
18. Subtransus deformation mechanisms of TC11 titanium alloy with lamellar structure10.1016/s1003-6326(09)60437-4 ↗
19. FEM simulation of the linear friction welding of titanium alloys10.1016/j.commatsci.2010.03.026 ↗
20. High and low cycle fatigue behavior of linear friction welded Ti–6Al–4V10.1016/j.ijfatigue.2014.10.002 ↗
21. Elucidating the in-process interfacial friction regime and thermal responses during inertia friction welding of dissimilar superalloys10.1016/j.jmrt.2024.03.210 ↗
22. Study on the distribution of residual stresses in linear friction welds of Ti6A14V
23. Linear friction welding of Ti-6Al-4V: modelling and validation10.1016/j.actamat.2011.02.028 ↗
24. The magnitude and origin of residual stress in Ti-6Al-4V linear friction welds: an investigation by validated numerical modeling10.1007/s11663-011-9563-9 ↗
25. High frequency linear friction welding of a titanium alloy10.1016/s0043-1648(98)00145-8 ↗
26. Linear friction welding of Ti-6Al-4V: processing, microstructure, and mechanical-property inter-relationships10.1007/s11661-005-0335-5 ↗
27. Strain-controlled fatigue properties of linear friction welded dissimilar joints between Ti-6Al-4V and Ti-6.5-Al-3.5Mo-1.5Zr-0.3Si alloys10.1016/j.msea.2014.06.010 ↗
28. Research on the adaptive machining technology of blisk10.4028/www.scientific.net/amr.69-70.446 ↗
29. Low cycle fatigue properties of linear friction welded joint of TC11 and TC17 titanium alloys10.1016/j.jallcom.2016.03.113 ↗