Improvement in the electrode–electrolyte interface of all-solid-state battery using aerosol deposition technology
Source abstract
Abstract
All-solid-state battery (ASSB) has attracted much attention since it is a potential candidate to solve the safety issue of batteries. However, the rigid contact between the electrode and electrolyte limits the electrochemical performance of ASSB. It is therefore necessary to modify the electrode–electrolyte interface to decrease the interfacial resistance. Herein, we use the aerosol deposition (AD) method to directly deposit the electrode, Na3V2(PO4)3 (NVP), on the Na3Zr2Si2PO12 (NZSP) electrolyte at room temperature. The electrolyte pellet coated with NVP demonstrates a negligible interfacial resistance and low total resistivity of about 1831.64 [Formula: see text] cm[Formula: see text]. Furthermore, the electrochemical performance in terms of cyclic voltammetry and charge/discharge of the ASSB consisting of NVP ∣ NZSP ∣ sodium (Na) metal is also investigated.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National University of Singapore (Chongqing) Research Institute, Chongqing 401123, P. R. China
National University of Singapore, Engineering Drive 1, Singapore 117575, Singapore
Funding
National University of Singapore
References (14)
Show source-provided references
1. Gao H. · Angew. Chem. Int. Ed. Engl. · 2017 · 56 · 20
2. He L. · Funct. Mater. Lett. · 2020 · 14 · 3
3. Kuwata N. · Solid State Ion. · 2006 · 177 · 282710.1016/j.ssi.2006.07.023 ↗
4. Gao H. · Vacuum · 2015 · 112 · 110.1016/j.vacuum.2014.10.017 ↗
5. Vardelle A. · Plasma Chem. Plasma Process. · 2014 · 35 · 3
6. Jain I. P. · Surf. Sci. Rep. · 2011 · 66 · 7710.1016/j.surfrep.2010.11.001 ↗
7. Schubert M. · Funct. Mater. Lett. · 2019 · 12 · 5
8. Oh J. A. S. · ACS Appl. Mater. Interface. · 2019 · 11 · 4310.1021/acsami.8b18453 ↗
9. Oh J. A. S. · ACS Appl. Mater. · 2020 · 3 · 7
10. Sarobol P. · SAND. · 2016 · 2016 · 2870
11. Lee D. W. · Nanoscale Res. Lett. · 2016 · 11 · 16210.1186/s11671-016-1378-9 ↗
12. Schubert M. · Funct. Mater. Lett. · 2019 · 12 · 3
13. Park H. · J. Thermal Spray Technol. · 2013 · 22 · 6
14. Chen G. · Adv. Funct. Mater. · 2020 · 30 · 200128910.1002/adfm.202001289 ↗