INFLUENCE OF ANNEALING ON RECOVERY STRESS OF COLD-WORKED Ni–Ti WIRE
Source abstract
Abstract
The effect of annealing on the recovery stress of Ni – Ti wire has been studied by using a dynamic mechanical analyzer (DMA), TAQ800. The results show that the recovery stresses decrease with increasing annealing temperature in the range of 350–600°C and increase with increasing annealing temperature in the range of 600–900°C. It was found that the recovery stress is proportional to the plateau stress at room temperature, the recoverable strain under zero load and relative temperature increase above As.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · High Entropy Alloys Studies · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Metallurgy and Materials Engineering (MTM), Katholieke Universiteit Leuven, Kasteelpark Arenberg 44 bus 2450, B-3001 Leuven, Belgium
References (11)
Show source-provided references
1. 10.1016/S0921-5093(99)00293-210.1016/S0921-5093(99)00293-2 ↗
2. 10.1016/S0921-5093(00)00816-910.1016/S0921-5093(00)00816-9 ↗
3. 10.1088/0964-1726/12/5/30310.1088/0964-1726/12/5/303 ↗
4. 10.1016/j.msea.2003.11.00610.1016/j.msea.2003.11.006 ↗
5. 10.1016/j.msea.2003.11.00710.1016/j.msea.2003.11.007 ↗
6. 10.1016/S1359-6462(98)00155-910.1016/S1359-6462(98)00155-9 ↗
7. 10.1016/S1359-6454(98)00325-510.1016/S1359-6454(98)00325-5 ↗
8. 10.1016/S0921-5093(00)01982-110.1016/S0921-5093(00)01982-1 ↗
9. 10.1088/0964-1726/14/5/01610.1088/0964-1726/14/5/016 ↗
10. 10.1016/S0925-8388(96)02572-810.1016/S0925-8388(96)02572-8 ↗
11. Treppmann D. · J. de Physique IV Col. C. 8, Suppl. J. De Phys. III · 5 · C8