LOW-TEMPERATURE HYDROGEN DESORPTION FROM LiBH4–TiF4 COMPOSITE
Source abstract
Abstract
Approximately 6.3 wt.% of hydrogen is released from a LiBH4–0.25TiF4 combination below 150°C. Hydrogen desorption from the LiBH4–0.25TiF4 combination undergoes a quite different reaction process with respect to the LiBH4–0.33TiF3 mixture due to the higher oxidation state of Ti4+ and the lower mean bond cleavage energy of Ti–F bonds in TiF4 . This finding provides a viable approach for significantly decreasing the dehydrogenation temperature of LiBH4 by optimizing the additives with high oxidation valency.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen Storage and Materials · Ammonia Synthesis and Nitrogen Reduction · Hybrid Renewable Energy Systems
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Silicon Materials, Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, P. R. China
References (22)
Show source-provided references
1. Züttel A. · J. Alloys Compd. · 356 · 515
2. 10.3390/en401018510.3390/en4010185 ↗
3. 10.1021/jp077572r10.1021/jp077572r ↗
4. Orimo S. · J. Alloys Compd. · 404 · 427
5. 10.1063/1.243224010.1063/1.2432240 ↗
6. 10.1021/jp803916k10.1021/jp803916k ↗
7. 10.1021/jp056240o10.1021/jp056240o ↗
8. 10.1021/jp040769o10.1021/jp040769o ↗
9. 10.1021/jp802430410.1021/jp8024304 ↗
10. 10.1016/j.ijhydene.2010.04.16510.1016/j.ijhydene.2010.04.165 ↗
11. 10.1016/j.ijhydene.2010.10.01010.1016/j.ijhydene.2010.10.010 ↗
12. 10.1016/S0378-7753(03)00054-510.1016/S0378-7753(03)00054-5 ↗
13. 10.1063/1.307610610.1063/1.3076106 ↗
14. 10.1039/b920270f10.1039/b920270f ↗
15. 10.1139/v71-54610.1139/v71-546 ↗
16. 10.1063/1.174711010.1063/1.1747110 ↗
17. 10.1021/jp907746z10.1021/jp907746z ↗
18. Ghaemy M. · Iran. Poly. J. · 6 · 5
19. 10.1021/jp910266m10.1021/jp910266m ↗
20. Suwarno · Int. J. Tech. · 1 · 28
21. Fieser M. · 1989 · 14
22. 10.1007/BF0287361710.1007/BF02873617 ↗