Source abstract
Abstract
100 mol% activator orthorhombic Tb2 (MoO4)3 green phosphors were prepared using a solid-state reaction method. The impact of sintering temperature on the crystalline phase structures, the compositions, the sizes and morphologies of particles, the values of energy bandgap ([Formula: see text][Formula: see text]), the photoluminescence (PL) excitation and emission spectra, the fluorescence lifetimes, PL quantum yield (PLQY), and the luminescent thermal stabilities of the prepared material were comprehensively investigated. The particle size increased from 2.54 to 5.81 [Formula: see text]m and the [Formula: see text] decreased from 3.60 to 3.41 eV with the calcine temperature increased from 800°C to 1100°C. The Tb2(MoO4)3 green phosphor prepared at 1000°C exhibited optimal PL intensity though it did not possess the highest PLQY with 380 nm excitation. Moreover, the sample prepared at 1000°C showed better thermal stabilities than that prepared at 1100°C. The research proved the sintering temperature has great effects on the properties of Tb2(MoO4)3 phosphors.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Solid-state spectroscopy and crystallography · Synthesis and characterization of novel inorganic/organometallic compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Fujian Key Laboratory of Functional Materials and Applications, School of Materials Science and Engineering, Xiamen University of Technology, Xiamen 361024, P. R. China
Department of Fundamental Courses, Xiamen Donghai Institute, Xiamen 361112, P. R. China
Funding
Fujian Provincial Natural Science Foundation of China · Open Fund of Fujian Provincial Key Laboratory of Functional Materials and Applications of China · Fujian Provincial Key Technical Innovation and Industrialization Projects of China
References (32)
Show source-provided references