Abstract

The performance of four 1.5 mm thick high-density polyethylene (HDPE) geomembranes (GMBs) (denoted MxA-15, MxC-15, MyE-15, and MyEW-15) immersed in a brine solution with 200,000 ppm total dissolved solids and a pH = 8.7 is presented for 4 years. Accelerated ageing experiments were conducted at 40, 65, 75, and 85°C for 4 years. It is shown that neither the Std-OIT nor HP-OIT had reached a residual value before physical degradation was observed, suggesting that the traditional three-stage concept for degradation did not apply when based on the values obtained (as is usual) through the entire GMB thickness. The time to nominal failure, based on a reduction of 50% of the initial value, was less than 4 years for all GMBs at temperatures ≥ 65°C. However, using the time at which the stress crack resistance (SCR), obtained from the single point notched constant tensile load (SP-NCTL) test, decreased to 50% of the minimum requirements of GRI-GM13, the times to nominal failure are greater than 20 years for at T ≤ 65°C for MyE-15.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Landfill Environmental Impact Studies · Geotechnical Engineering and Soil Stabilization · Geotechnical Engineering and Underground Structures

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Geotechnical and Geoenvironmental Engineering, GeoEngineering Centre at Queen's – RMC, Queen's University, Kingston, Ontario, Canada K7L 3N6,(corresponding author)

GeoEngineering Centre at Queen's – RMC, Queen's University, Kingston, Ontario, Canada K7L 3N6,

References (29)

Show source-provided references
1. Abdelaal F. B. · 2011
2. Abdelaal F. B. · 2012
3. Abdelaal F. B. · 2013 · 127
4. 10.1016/j.geotexmem.2014.06.00110.1016/j.geotexmem.2014.06.001 ↗
5. 10.1680/gein.15.0000610.1680/gein.15.00006 ↗
6. ASTM D5397 Standard Test Method for Evaluation of Stress Crack Resistance of Polyolefin Geomembranes Using Notched Constant Tensile Load Test. ASTM International, West Conshohocken, PA, USA.
7. 10.1016/j.geotexmem.2014.01.00410.1016/j.geotexmem.2014.01.004 ↗
8. 10.1680/gein.2004.11.2.6010.1680/gein.2004.11.2.60 ↗
9. Hsuan, Y. & Koerner, R. (1995). Long-term Durability of HDPE Geomembrane. Part 1: Depletion of Antioxidant, GRI Report 16. Geosynthetics Research Institute, Philadelphia, PA, USA.
10. 10.1061/(ASCE)1090-0241(1998)124:6(532)10.1061/(ASCE)1090-0241(1998)124:6(532) ↗
11. 10.1016/j.solener.2010.06.00510.1016/j.solener.2010.06.005 ↗
12. Müller W. · 2007
13. 10.1016/S0141-3910(02)00269-010.1016/S0141-3910(02)00269-0 ↗
14. 10.1680/gpte.32347.000110.1680/gpte.32347.0001 ↗
15. 10.1680/gein.2009.16.3.18310.1680/gein.2009.16.3.183 ↗
16. 10.1680/gein.13.0000310.1680/gein.13.00003 ↗
17. 10.1061/(ASCE)GT.1943-5606.000109010.1061/(ASCE)GT.1943-5606.0001090 ↗
18. 10.1016/j.geotexmem.2014.08.00110.1016/j.geotexmem.2014.08.001 ↗
19. 10.1016/j.wasman.2009.05.01010.1016/j.wasman.2009.05.010 ↗
20. 10.1680/gein.2008.15.2.13610.1680/gein.2008.15.2.136 ↗
21. 10.1061/(ASCE)GT.1943-5606.000020710.1061/(ASCE)GT.1943-5606.0000207 ↗
22. 10.1061/(ASCE)GT.1943-5606.000030210.1061/(ASCE)GT.1943-5606.0000302 ↗
23. 10.1016/j.geotexmem.2009.10.01210.1016/j.geotexmem.2009.10.012 ↗
24. Rowe R. K. · 2004
25. 10.1061/(ASCE)1090-0241(2008)134:1(68)10.1061/(ASCE)1090-0241(2008)134:1(68) ↗
26. 10.1061/(ASCE)1090-0241(2008)134:7(906)10.1061/(ASCE)1090-0241(2008)134:7(906) ↗
27. 10.1016/j.geotexmem.2008.09.00710.1016/j.geotexmem.2008.09.007 ↗
28. 10.1139/t02-07410.1139/t02-074 ↗
29. Tan D. · 2012