journal article·2024-10-01

Antioxidant-stabilizer depletion of 4 HDPE geomembranes with high HP-OIT in MSW leachate

M. Clinton, R. K. Rowe

Geosynthetics International· Volume 31· Issue 5
Publisher page

Abstract

The antioxidant-stabilizer depletion of four 1.5-mm HDPE geomembranes from the same manufacturer each with a different resin and additive package is examined in air and a synthetic municipal solid waste leachate at a range of temperatures (40–95°C) for 7.5 years. Two were formulated for high temperatures and used polyethylene of raised temperature resistance (PE-RT) resins while two used more conventional HDPE geomembrane formulations. The depletion of protective antioxidants and stabilizers was monitored using standard and high-pressure oxidative induction time (OIT) tests and the notably different depletion times for both OIT tests implied they were detecting different groups of AO-S. Although both PE-RT GMBs showed significantly slower AO-S depletion at 85°C in air compared to the conventional PE GMBs, only one PE-RT GMB maintained this status in 85°C leachate, highlighting the limitation of air aging tests (and importance of fluid immersion tests). The importance of running immersion tests long enough to reveal the residual HP-OIT value is stressed. The roles of stabilizer mobility and solubility in polyethylene and their suspected involvement in residual HP-OIT behavior are also illustrated.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Landfill Environmental Impact Studies · Concrete and Cement Materials Research · Electrokinetic Soil Remediation Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

PhD student, GeoEngineering Centre at Queen's-RMC, Queen's University, Kingston, ON, Canada, K7L 3N6,

Barrington Batchelor Distinguished University Professor and Canada Research Chair in Geotechnical and Geoenvironmental Engineering, GeoEngineering Centre at Queen's-RMC, Queen's University, Ellis Hall, Kingston, ON, Canada K7L 3N6,(corresponding author)

References (62)

Show source-provided references
1. 10.1061/(ASCE)GT.1943-5606.000123410.1061/(ASCE)GT.1943-5606.0001234 ↗
2. 10.1061/(ASCE)HZ.2153-5515.000026210.1061/(ASCE)HZ.2153-5515.0000262 ↗
3. 10.1680/jgein.19.0001610.1680/jgein.19.00016 ↗
4. 10.1680/gein.13.0003110.1680/gein.13.00031 ↗
5. 10.1680/gein.15.0000610.1680/gein.15.00006 ↗
6. 10.1016/j.geotexmem.2019.10349710.1016/j.geotexmem.2019.103497 ↗
7. ASTM D5885
8. ASTM D3895
9. ASTM D883
10. ASTM D5199
11. ASTM D1603
12. ASTM D5721
13. ASTM E794
14. 10.1061/9780784480434.03410.1061/9780784480434.034 ↗
15. Borghi A. · Chemical and Biochemical Engineering Quarterly · 2003 · 17 · 277
16. 10.1016/j.polymdegradstab.2021.10968310.1016/j.polymdegradstab.2021.109683 ↗
17. Damen J. · 2001 · 775
18. 10.1002/(SICI)1099-0488(19980715)36:9<1513::AID-POLB9>3.0.CO;2-K10.1002/(SICI)1099-0488(19980715)36:9<1513::AID-POLB9>3.0.CO;2-K ↗
19. 10.1016/j.polymdegradstab.2014.06.01310.1016/j.polymdegradstab.2014.06.013 ↗
20. 10.1061/(ASCE)GT.1943-5606.000116410.1061/(ASCE)GT.1943-5606.0001164 ↗
21. 10.1016/j.geotexmem.2014.01.00410.1016/j.geotexmem.2014.01.004 ↗
22. 10.1002/pen.76034240210.1002/pen.760342402 ↗
23. 10.1061/(ASCE)1090-0241(1998)124:6(532)10.1061/(ASCE)1090-0241(1998)124:6(532) ↗
24. Hsuan Y. G. · 2008
25. 10.1061/(ASCE)HZ.2153-5515.000018810.1061/(ASCE)HZ.2153-5515.0000188 ↗
26. 10.1016/j.solener.2010.06.00510.1016/j.solener.2010.06.005 ↗
27. 10.1016/0141-3910(92)90136-S10.1016/0141-3910(92)90136-S ↗
28. 10.1080/0091403980804106410.1080/00914039808041064 ↗
29. 10.1016/j.polymdegradstab.2017.09.02010.1016/j.polymdegradstab.2017.09.020 ↗
30. 10.1061/9780784480434.00310.1061/9780784480434.003 ↗
31. Mills A. · 2019
32. 10.1016/j.polymdegradstab.2011.11.00710.1016/j.polymdegradstab.2011.11.007 ↗
33. 10.1139/cgj-2019-004710.1139/cgj-2019-0047 ↗
34. 10.1139/cgj-2019-052010.1139/cgj-2019-0520 ↗
35. 10.1002/pen.2419910.1002/pen.24199 ↗
36. 10.1023/A:101792250103910.1023/A:1017922501039 ↗
37. 10.1016/S0141-3910(03)00210-610.1016/S0141-3910(03)00210-6 ↗
38. Prachoomdang, Y. & Wu, Y. (2016). High temperature geomembrane liners and master batch compositions. Patent No.: US 9,518,176 B2.
39. Rangel E. · 2017 · 1
40. Redhead A. · 2012 · 1
41. 10.1680/geot.2005.55.9.63110.1680/geot.2005.55.9.631 ↗
42. 10.1680/gein.2011.18.6.39110.1680/gein.2011.18.6.391 ↗
43. 10.1139/t11-09210.1139/t11-092 ↗
44. Rowe R. K. · Italian Geotechnical Journal · 2018 · 4 · 8
45. 10.1061/(ASCE)GT.1943-5606.000223910.1061/(ASCE)GT.1943-5606.0002239 ↗
46. 10.1139/cgj-2016-002610.1139/cgj-2016-0026 ↗
47. 10.1016/j.geotexmem.2014.08.00110.1016/j.geotexmem.2014.08.001 ↗
48. Rowe R. K. · 2022 · 187
49. 10.1061/(ASCE)1090-0241(2008)134:1(68)10.1061/(ASCE)1090-0241(2008)134:1(68) ↗
50. 10.1016/j.geotexmem.2019.01.00110.1016/j.geotexmem.2019.01.001 ↗
51. 10.1680/gein.2008.15.2.13610.1680/gein.2008.15.2.136 ↗
52. 10.1061/(ASCE)GT.1943-5606.000020710.1061/(ASCE)GT.1943-5606.0000207 ↗
53. 10.1061/(ASCE)GT.1943-5606.000030210.1061/(ASCE)GT.1943-5606.0000302 ↗
54. Rowe R. K. · 2019 · 3
55. 10.1139/cgj-2019-057210.1139/cgj-2019-0572 ↗
56. 10.1139/t02-07410.1139/t02-074 ↗
57. Scheirs J. · Wiley Series in Polymer Science · 2009
58. Schwetlick K. · Polymer Durability, May 5, 1996 · 1996 · 349
59. 10.1016/0141-3910(91)90077-510.1016/0141-3910(91)90077-5 ↗
60. Thomas R. W. · 1993 · 915
61. Valiya P. S. · 2020 · 201
62. Zweifel H. · 2009