Production of Ceramic Materials Based on SiC with Low-Melting Oxide Additives
Source abstract
Abstract
Dense materials based on silicon carbide were obtained by liquid-phase sintering. The oxides MgO, Y2O3 , and Al2O3 , corresponding to the composition of yttrium-aluminum garnet and the triple eutectic point on the line of binary sections garnet-spinel, were used as the sintering additive. The oxides were deposited on the surface of powder by the SiC method of coprecipitation from a solution of salts. The maximum density (ρrel = 99.5%) was attained on SiC materials which include 20% (by weight) sintering additives consisting of a three-component oxide mixture at temperature 1800°C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. V. A. Izhevskyi, L. A. Genova, J. C. Bressiani, and A. H. A. Bressiani, “Silicon carbide. Structure, properties and processing,” Cerâmica, 46(297), 4 – 13 (2000).10.1590/S0366-69132000000100002 ↗
2. K. A. Schwetz, “Silicon carbide based hard materials,” in: Handbook of Ceramic Hard Materials, Wiley-VCH, Weinheim (2000), pp. 683 – 748.
3. A. Can, M. Herrmann, D. S. McLachlan, et al., “Densification of liquid phase sintered silicon carbide,” J. Eur. Ceram. Soc., 26(9), 1707 – 1713 (2006).10.1016/j.jeurceramsoc.2005.03.253 ↗
4. Y.W. Kim, J. Y. Kim, S. H. Rhee, and D. Y. Kim, “Effect of initial particle size on microstructure of liquid-phase sintered σ-silicon carbide,” J. Eur. Ceram. Soc., 20, 945 – 949 (2000).10.1016/S0955-2219(99)00239-3 ↗
5. T. Tachiwaki, M. Yoshinaka, K. Hirota, et al., “Novel synthesis of Y3Al5O12 (YAG) leading to transparent ceramics,” Solid State Comm., 119(10–11), 603 – 606 (2001).10.1016/S0038-1098(01)00293-9 ↗
6. S.-G. Lee,W.-H. Shim, J.-Y. Kim, et al., “Effect of sintering-additive composition on fracture toughness of liquid-phase-sintered SiC ceramics,” J. Mater. Sci. Lett., 20, 143 – 146 (2001).10.1023/A:1006754708677 ↗
7. K.-S. Cho, H.-J. Choi, J.-G. Lee, and Y. W. Kim, “R-curve behavior of layered silicon carbide ceramics with surface fine microstructure,” J. Mater. Sci., 36, 2189 – 2193 (2001).10.1023/A:1017544000562 ↗
8. E. Nogales, A. Montone, F. Cardellini, et al., “Visible cathodoluminescence from mechanically milled germanium,” Semicond. Sci. Techn., 17, 1267 – 1271 (2002).10.1088/0268-1242/17/12/310 ↗
9. Z. Huang, D. C. Jia, Y. Zhou, and Y. G. Liu, “A new sintering additive for silicon carbide ceramic,” Ceram. Int., 29, 13 – 17 (2003).10.1016/S0272-8842(02)00082-2 ↗
10. N. Hidaka, Y. Hirata, S. Sameshima, and H. Sueyoshi, “Hot-pressing and mechanical properties of SiC ceramics with polytitanocarbosilane,” J. Ceram. Proc. Res., 5(4), 331 – 336 (2004).
11. X.-Zh. Guo and H. Yang, “Sintering and microstructure of silicon carbide ceramic with Y3Al5O12 added by sol-gel method,” J. Zhejiang Univ SCI., 6(3), 213 – 218 (2005).10.1631/jzus.2005.B0213 ↗
12. V. G. Sevastyanov, E. P. Simonenko, N. P. Simonenko, and N. T. Kuznetsov, “Synthesis of fine-dispersed yttrium-aluminum garnet Y3Al5O12 via sol-gel technique,” in: 15th European Conference on Composite Materials, Venice, Italy, 24 – 28 June 2012, Venice (2012), Vol. 4, pp. 1 – 8.
13. E. P. Simonenko, N. P. Simonenko, V. G. Sevastyanov, and N. T. Kuznetsov, “Synthesis of ultrafine yttrium aluminum garnet using sol-gel technology,” Russ. J. Inorg. Chem., 57(12), 1521 – 1528 (2012).10.1134/S0036023612120194 ↗
14. Zh. Yongheng, “Surface modification of ceramic powders by complexes of metal ions in aqueous media,” J. Mater. Sci. Lett., 21, 1723 – 1725 (2002).10.1023/A:1020973431245 ↗
15. Y.-T. Nien, Y.-L. Chen, I.-G. Chen, et al., “Synthesis of nanoscaled yttrium aluminum garnet phosphor by coprecipitation method with HMDS treatment,” Mater. Chem. Phys., 93, 79 – 83 (2005).10.1016/j.matchemphys.2005.02.017 ↗
16. S. N. Perevislov, I. B. Panteleev, S. V. Vikhman, et al., “Co-precipitation of oxides from a solution of salts on the surface of silicon carbide particles,” Ogneup. Tekh. Keram., No. 9, 9 – 16 (2005).
17. S. N. Perevislov, I. B. Panteleev, A. P. Shevchik, and M. V. Tomkovich, “Microstructure and mechanical properties of SiC-materials sintered in the liquid phase with the addition of a finely dispersed agent,” Refract. Industr. Ceram., 58(5), 577 – 582 (2018).10.1007/s11148-018-0148-x ↗
18. S. Kikkawa, A. Kijimab, K. Hirotab, and O. Yamaguchi, “Soft solution preparation methods in a ZrO2–Al2O3 binary system,” Solid State Ionics, 151, 359 – 364 (2002).10.1016/S0167-2738(02)00540-4 ↗
19. J. L. Lorca, J. Y. Pastor, and P. Poza, “Influence of the Y2O3 content and temperature on the mechanical properties of melt-grown Al2O3–ZrO2 eutectics,” J. Am. Ceram. Soc., 87(4), 633 – 639 (2004).10.1111/j.1551-2916.2004.00633.x ↗
20. D. D. Nesmelov, O. A. Kozhevnikov, S. S. Ordanyan, and S. N. Perevislov, "Deposition of the eutectic composition Al2O3-ZrO2(Y2O3) on the surface of SiC particles," Steklo Keram., No. 2, 9 - 14 (2017)
21. D. D. Nesmelov, O. A. Kozhevnikov, S. S. Ordanyan, and S. N. Perevislov, "Precipitation of the eutectic composition Al2O3-ZrO2(Y2O3) on the surface of SiC particles," Glass Ceram., 74(1 - 2), 43 - 47 (2017).10.1007/s10717-017-9925-0 ↗
22. H. S. Kim, M. K. Kim, S. B. Kang, et al., “Bending strength and crackhealing behavior of Al2O3 /SiC composites ceramics,” Mater. Sci. Eng. A, 483–484, 672 – 675 (2008).10.1016/j.msea.2006.09.169 ↗
23. W. Nakao, M. Ono, S. Lee, et al., “Critical crack-healing condition for SiC whisker reinforced alumina under stress,” J. Eur. Ceram. Soc., 25, 3649 – 3655 (2005).10.1016/j.jeurceramsoc.2004.09.021 ↗
24. K. Andoa, M.-Ch. Chua, K. Tsujib, et al., “Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics,” J. Eur. Ceram. Soc., 22, 1313 – 1319 (2002).10.1016/S0955-2219(01)00431-9 ↗
25. K. W. Nama, M. K. Kimb, S. W. Parka, et al., “Crack-healing behavior and bending strength of Si3N4 /SiC composite ceramics by SiO2 colloidal,” Mater. Sci. Eng. A, 471, 102 – 105 (2007).10.1016/j.msea.2007.03.005 ↗
26. D.-C. Park, T. Yano, T. Iseki, and K. Urabe, “Effect of nitrate salts as sintering additives during the ball-milling process of silicon nitride powders,” J. Am. Ceram. Soc., 83(12), 2967 – 2973 (2000).10.1111/j.1151-2916.2000.tb01668.x ↗
27. N. S. Akhmetov, General and Inorganic Chemistry [in Russian], Vyssh. Shkola, Moscow (2006).
28. S. N. Perevislov, V. D. Chupov, S. S. Ordanyan, and V. V. Tomkovich, “Obtaining high-density materials of silicon carbide by the method of liquid-phase sintering in the system of components SiC–Al2O3–Y2O3–MgO,” Ogneup. Tekh. Keram., No. 4/5, 26 – 32 (2011).
29. M. Castillo-Rodríguez, A. Munoz, and A. Domínguez-Rodríguez, “Effect of atmosphere and sintering time on the microstructure and mechanical properties at high temperatures of α-SiC sintered with liquid phase Y2O3–Al2O3 ,” J. Europ. Ceram. Soc., 26(12), 2397 – 2405 (2006).10.1016/j.jeurceramsoc.2005.04.018 ↗
30. S. N. Perevislov and D. D. Nesmelov, "Properties of SiC and Si3N4 based composite ceramic with nanosize component," Steklo Keram., No. 7, 15 - 18 (2016)
31. S. N. Perevislov and D. D. Nesmelov, "Properties of SiC and Si3N4 based composite ceramic with nanosize component," Glass Ceram., 73(7 - 8), 249 - 252 (2016).10.1007/s10717-016-9867-y ↗
32. S. N. Perevislov, "Mechanism of liquid-phase sintering of silicon carbide and nitride with oxide activating additives," Steklo Keram., No. 7, 34 - 38 (2013)
33. S. N. Perevislov, "Mechanism of liquid-phase sintering of silicon carbide and nitride with oxide activating additives," Glass Ceram., 70(7 - 8), 265 - 268 (2013).10.1007/s10717-013-9557-y ↗
34. S. N. Perevislov, A. S. Lysenkov, D. D. Titov, and M. V. Tomkovich, “Hot-pressed ceramic SiC–YAG materials,” Inorg. Mater., 53(2), 220 – 225 (2017).10.1134/S0020168517020091 ↗