Phase Composition, Structure, and Hydrolytic Stability of Sodium-Aluminum(Iron) Phosphate Glass Containing Rare-Earth Oxides
Source abstract
Abstract
The phase composition, structure, elemental distribution, and hydrolytic stability of quench-hardened and tempered sodium-aluminum-phosphate (SAP) and sodium-aluminum(iron) phosphate (SAIP) glass materials containing 10 wt.% (above 100%) oxides of rare earth elements (REE) were studied. It is shown that all materials obtained by quench-hardening melts (except La-containing melts) were x-ray amorphous, while slowly cooled (tempered) melts partially or completely crystallized with different phases of orthophosphates being released. The rate of leaching of elements from tempered SAP glasses determined at 90°C is approximately one or two orders of magnitude higher than then for the quench-hardened glasses, and the leach rate of elements from quench-hardened SAIP glasses is lower than from quench-hardened SAP glasses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Pigment Synthesis and Properties · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. D. Hewak (ed.), Properties, Processing and Applications of Glass and Rare Earth-Doped Glasses for Optical Fibers, Stevenage, UK (1998).
2. S. V. Stefanovsky, S. V. Yudintsev, R. Giere, and G. R. Lumpkin, “Nuclear waste forms,” in: Energy, Waste and the Environment: A Geological Perspective, Geological Society, London (2004), Special Publication, Vol. 236, pp. 37 – 63.
3. B. C. Sales and L. A. Boatner, “Physical and chemical characteristics of lead-iron phosphate nuclear waste glasses,” J. Non-Cryst. Solids, 79, 83 – 116 (1986).10.1016/0022-3093(86)90040-2 ↗
4. D. E. Day, Z. Wu, C. S. Ray, and P. Hrma, “Chemically durable iron phosphate glass wasteforms,” J. Non-Cryst. Solids, 241, 1 – 12 (1998).10.1016/S0022-3093(98)00759-5 ↗
5. R. Anderson, T. Brennan, G. Mountjoy, et al., “An EXAFS study of rare earth phosphate glasses in the vicinity of the metaphosphate composition,” J. Non-Cryst. Solids, 232–234, 286 – 292 (1998).10.1016/S0022-3093(98)00466-9 ↗
6. M. Karabulut, E. Metwalli, and R. K. Brow, “Structure and properties of lanthanum-aluminum-phosphate glasses,” J. Non-Cryst. Solids, 283, 211 – 219 (2001).10.1016/S0022-3093(01)00420-3 ↗
7. Y. M. Lai, X. F. Liang, S. Y. Yang, et al., “Raman and FTIR spectra of iron phosphate glasses containing cerium,” J. Mol. Struct., 992, 84 – 88 (2011).10.1016/j.molstruc.2011.02.049 ↗
8. Y. Lai, X. Liang, G. Yin, et al., “Infrared spectra of iron phosphate glasses with gadolinium oxide,” J. Mol. Struct., 1004, 188 – 192 (2011).10.1016/j.molstruc.2011.08.003 ↗
9. V. N. Rai, B. N. Raja Sekhar, P. Tiwari, et al., “Spectroscopic Studies of Gamma Irradiated Nd Doped Phosphate Glasses,” J. Non-Cryst. Solids, 357, 3757 – 3764 (2011).10.1016/j.jnoncrysol.2011.07.036 ↗
10. B. Qian, X. Liang, S. Yang, et al., “Effects of lanthanum addition on the structure and properties of iron phosphate glasses,” J. Mol. Struct., 1027, 31 – 35 (2012).10.1016/j.molstruc.2012.05.078 ↗
11. H. Shinozaki, S. Nakashima, S. Takahashi, et al., “Water resistance of cerium phosphate glasses as studied by in situ high temperature IR microspectroscopy,” J. Non-Cryst. Solids, 378, 55 – 60 (2013).10.1016/j.jnoncrysol.2013.06.016 ↗
12. S. V. Stefanovsky, O. I. Stefanovskaya, S. E. Vinokurov, et al., “Phase composition, structure, and hydrolytic durability of glasses in the Na2O–Al2O3–(Fe2O3)–P2O5 system at replacement of Al2O3 by Fe2O3,” Radiochemistry, 57, 348 – 355 (2015).10.1134/S1066362215040037 ↗
13. B. N. Litvin and V. A. Masloboev, Rare-Earth Phosphates [in Russian], Nauka, Leningrad (1989).
14. S. V. Stefanovsky, O. I. Stefanovsky, M. B. Remizov, et al. “Sodium- aluminum-iron phosphate glasses as legacy high level waste forms,” Progr. Nucl. Energy, 94, 229 – 234 (2017).10.1016/j.pnucene.2016.01.022 ↗
15. ASTM Standard C 1285–94: Standard Test Methods for Determining Chemical Durability of Nuclear Waste Glasses: The Product Consistency Test (PCT), ASTM, Philadelphia, PA (1994).
16. C. M. Jantzen, N. E. Bibler, and D. C. Beam, Characterization of the Defense Waste Processing Facility (DWPF) Environmental Assessment (EA) Glass Standard Reference Material, WSRCTR-92-346 (1992).10.2172/6876372 ↗
17. S. V. Stefanovsky, O. I. Stefanovsky, M. I. Kadyko, et al., “The effect of Fe2O3 substitution for Al2O3 on the phase composition and structure of sodium-aluminum-iron phosphate glasses,” J. Non-Cryst. Solids, 425, 138 – 145 (2015).10.1016/j.jnoncrysol.2015.05.039 ↗
18. S. D. Gabelnick, G. T. Reedy, and M. G. Chasanov, “Infrared spectra and structure of some matrix-isolated lanthanide and actinide oxides,” J. Chem. Phys., 60, 1167 – 1171 (1974).10.1063/1.1681128 ↗
19. T. Fukui, T. Ishinomori, Y. Endo, et al., “Iron phosphate glass as potential waste matrix for high-level radioactive waste,” in: Waste Management’03 Conference, February 23 – 27, 2003, Tucson, AZ (2003).