Recent Advances in Detection of Failure in Laminated Glass Using Non-Destructive Testing and Structural Health Monitoring Techniques (Review Paper)
Source abstract
Abstract
Using glass as a structural element that could obtain the role of the primary load-bearing elements of iconoclast structures has had a superficial history. Because of its aesthetic and admissible mechanical properties, glass has been considered one of the structural elements in the construction industry. Because of its extra safety, laminated glass on top of the most widely used elements has been appraised with more depth. The study aimed to evaluate the failure modes in laminated glass and the possibility of detecting the pre-failure status of the surveyed elements, referring to the proffered approaches and image processing (IP) procedures in the literature. The outcomes have compared the peculiarity and strength points of various routes and have reached the inference for proper approaches in every procedure. According to the results, image processing (IP) is the most appropriate method of pre-failure detection in load-bearing laminated glass elements. Among the image processing (IP) techniques, digital image correlation has the widest application. The results of this study, in combination with other pieces of research, may propound a database for evaluating the failure status of glass structures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Roughness and Optical Measurements · Smart Materials for Construction · Structural Analysis of Composite Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. H. Bach, and D. Krause, Analysis of the Composition and Structure of Glass and Glass Ceramics, Springer Science & Business Media (2013).
2. C. Bedon, “Structural glass systems under fire: overview of design issues, experimental research, and developments,” Adv. Civ. Eng. (2017).10.1155/2017/2120570 ↗
3. M. A. Kraus, M. Botz, and G. Siebert, Structural Design of Laminated Glass Under Consideration of the Shear Coupling According to German, European and US Standards, Proc. GlassCon Global, Chicago, Illinois (2018).
4. F. Pariafsai, “A review of design considerations in glass buildings,” Front. Archit. Res., 5(2), 171 – 193 (2016).10.1016/j.foar.2016.01.006 ↗
5. J. Sjöström, M. Kozłowski, D. Honfi, D. Lange, J. Albrektsson, P. Lenk, and J. Eriksson, “Fire resistance testing of a timber-glass composite beam,” Int. J. Struct. Glass Adv., 4(1), 24 – 40 (2020).
6. J. Yang, X.-H. Huang, and H.-S. Shen, “Nonlinear flexural behavior of temperature-dependent FG-CNTRC laminated beams with negative Poisson’s ratio resting on the Pasternak foundation,” Eng. Struct., 207, 110250 (2020).10.1016/j.engstruct.2020.110250 ↗
7. J. Yang, X.-H. Huang, and H.-S. Shen, “Nonlinear vibration of temperature-dependent FG-CNTRC laminated plates with negative Poisson’s ratio,” Thin-Walled Struct., 148, 106514 (2020).10.1016/j.tws.2019.106514 ↗
8. E. Frühwald, E. Serrano, T. Toratti, A. Emilsson, and S. Thelandersson, “Design of safe timber structures – How can we learn from structural failures in concrete, steel and timber,” in: Report TVBK-3053, Div. of Struct. Eng., Lund University (2007), p. 270.
9. M. Haldimann, A. Luible, and M. Overend, Structural Use of Glass, Vol. 10, IABSE (2008).10.2749/sed010 ↗
10. F. P. Bos, Safety Concepts in Structural Glass Engineering: Towards an Integrated Approach, Delft University of Technology (2009).
11. S. J. Bennison, C. A. Smith, A. Van Duser, and A. Jagota, “Structural performance of laminated glass made with a “stiff” interlayer,” in: Proc. Symp. Use of Glass in Buildings, ASTM, West Conshohocken, Pennsylvania (2002).10.1520/STP11056S ↗
12. K. Puller, J. Denonville, and W. Sobek, An Innovative Glass Connection Technique Using an Ionomer Interlayer, Glass Performance Days (2011), p. 638 – 641.
13. M. L. Williams, R. F. Landel, and J. D. Ferry, “The temperature dependence of relaxation mechanisms in amorphous polymers and other glass-forming liquids”, J. Am. Chem. Soc., 77(14), 3701 – 3707 (1955).10.1021/ja01619a008 ↗
14. J. Lair, and R. Hage, Failure Mode Effect and Criticality Analysis Application to Windows and Solar Components (2002).
15. X. Li, Z. P. Fang, F. L. Ng, L. P. Zhao, and L. Zhao, “Inspection and image analysis of nickel sulphide inclusions in toughened glass panels,” in: 9th Int. Conf. Control, Automation, Robotics and Vision, IEEE (2006).10.1109/ICARCV.2006.345068 ↗
16. M. Feldmann, R. Kasper, B. Abeln, P. Cruz, Jan Belis, J. Beyer, J. Colvin, F. Ensslen, M. Eliasova, L. Galuppi, and A. Geßler, Guidance for European Structural Design of Glass Components-Support to the Implementation, Harmonization and Further Development of the Eurocodes, Report EUR 26439, Joint Research Centre, Institute for the Protection and Security of the Citizen (2014).
17. K. Takae, and A. Onuki, “Structural phase transition and orientation-strain glass formation in anisotropic particle systems with impurities in two dimensions,” arXiv preprint, arXiv: 1203.2425 (2012).10.1063/1.4794574 ↗
18. S. M. Wiederhorn, “Influence of water vapor on crack propagation in soda-lime glass,” J. Am. Ceram. Soc., 50(8), 407 – 414 (1967).10.1111/j.1151-2916.1967.tb15145.x ↗
19. J. Yu, et al., “On the effect of impurities in metallic glass formation,” Appl. Phys. Lett., 96(14), 141901 (2010).10.1063/1.3373528 ↗
20. A. Bonati, G. Pisano, and G. Royer Carfagni, “A statistical model for the failure of glass plates due to nickel sulfide inclusions,” J. Am. Ceram. Soc., 102(5), 2506 – 2521 (2019).10.1111/jace.16106 ↗
21. S. M. Wiederhorn, et al., “Effects of water and other dielectrics on crack growth,” J. Mater. Sci., 17(12), 3460 – 3478 (1982).10.1007/BF00752191 ↗
22. G. Siebert, WG 1 Glass Structures – Guidelines for Application of Structural Glass, IABSE Symp. Rep., International Association for Bridge and Structural Engineering (2014).10.2749/222137814814068229 ↗
23. G. Siebert, “Aktueller Stand der Glasnormung,” Stahlbau, 85(S1), 113 – 120 (2016).10.1002/stab.201690150 ↗
24. EN 1288-1, Glass in Building – Determination of the Bending Strength of Glass – Part 1: Fundamentals of Testing Glass, Beuth Berlin (2000).
25. DIN EN 16612, Glas im Bauwesen-Bestimmung des Belastungs widerstandes von Glasscheiben durch Berechnung, Deutsche Fassung (2019).
26. DIN EN 16613, Glass in Building – Laminated Glass and Laminated Safety Glass – Determination of Interlayer Viscoelastic Properties, Beuth Verlag GmbH (2020).
27. R. Zarnic, G. Tsionis, E. Gutierrez, A. Pinto, M. Geradin, and S. Dimova, Purpose and Justification for New Design Standards Regarding the Use of Glass Products in Civil Engineering Works, European Commission, Joint Research Centre, Office for Official Publications of the European Communities, Luxembourg (2007).
28. M. Feldmann, R. Kasper, B. Abeln, P. Cruz, J. Belis, and J. Beyer, Guidance for European Structural Design of Glass Components, Publications Office of the European Union (2014), pp. 1 – 196.
29. J. Belis, “Recent, current & near-future research on structural glass,” in: COST Action TU0905 ‘Structural Glass: Novel Design Methods and Next Generation Products,’ Ghent University Press (2012).
30. J. Belis, J. Neugebauer, J. Schneider,M. Overend, and D. Mocibob, “Towards a European structural glass network,” in: COST Action TU0905, Challenging Glass 3 – Conf. Archit. Struct. Applications of Glass, IOS Press (2012).
31. J. Belis, C. Louter, J. Neugebauer, and J. Schneider, “Boosting European education on structural glass,” in: COST Action TU0905 Training School, Proc. Second Int. Conf. Struct. Archit. (ICSA), Guimaraes (2013).
32. G. F. Savineau, C. Butchart, Didier Delincé, and R. Speelman, “Characterization of interlayer properties,” in: TG06 Status Report, COST Action TU0905 Mid-term Conf. Struct. Glass, CRC Press/Balkema (2013).10.1201/b14563-48 ↗
33. M. Vandebroek, N. Jürgen, L. Martin, R. Vlatka, and Z. Roko, “Activity report of COST action TU0905 working Group 1: Predicting complex loads on glass structures,” in: Challenging Glass 4 & COST Action TU0905 Final Conf., CRC Press/Balkema (2014), pp. 11 – 20.10.1201/b16499-5 ↗
34. ASTM-C146-94a, Standard Test Methods for Chemical Analysis of Glass Sand, ASTM International: West Conshohocken, Pennsylvania (2014).
35. ASTM-C158-02, Standard Test Methods for Strength of Glass by Flexure (Determination of Modulus of Rupture), ASTM International: West Conshohocken, Pennsylvania (2017).
36. ASTM-C623-92, Standard Test Method for Young’s Modulus, Shear Modulus, and Poisson’s Ratio for Glass and Glass-Ceramics by Resonance, ASTM International: West Conshohocken, Pennsylvania (2015).
37. ASTM-C1036-16, Standard Specification for Flat Glass, ASTM International: West Conshohocken, Pennsylvania (2016).
38. ASTM-C1279-13, Standard Test Method for Non-Destructive Photoelastic Measurement of Edge and Surface Stresses in Annealed, Heat-Strengthened, and Fully Tempered Flat Glass, ASTM International: West Conshohocken, Pennsylvania (2019).
39. ASTM-C1505-15, Standard Test Method for Determination of Breaking Strength and Modulus of Rupture of Ceramic Tiles and Glass Tiles by Three-Point Loading, ASTM International: West Conshohocken, Pennsylvania (2015).
40. ASTM-E998-84, Standard Test Method for Structural Performance of Glass in Windows, Curtain Walls, and Doors Under the Influence of Uniform Static Loads by Nondestructive Method, ASTM International: West Conshohocken, Pennsylvania (1999).
41. ASTM-E1300-16, Standard Practice for Determining Load Resistance of Glass in Buildings, ASTM International: West Conshohocken, Pennsylvania (2016).
42. ANSI-Z97.1, Standard for Safety Glazing Materials Used in Buildings, Safety Performance Specifications and Methods of Test, American National Standards Institute (1984).
43. GB/T 37780-2019, Test Method for Elastic Modulus, Shear Modulus and Poisson’s Ratio of Glass, China National Standards, The Standardization Administration of the People’s Republic of China (2019).
44. GB/T 37781-2019, Test Methods for Bending Strength of Glass, China National Standards, The Standardization Administration of the People’s Republic of China (2019).
45. GB/T 37784-2019, In-situ Test Method for Detection of Structural Risk of the Insulating Glass, China National Standards, The Standardization Administration of the People’s Republic of China (2019).
46. T. Pyttel, H. Liebertz, and J. Cai, “Failure criterion for laminated glass under impact loading and its application in finite element simulation,” Int. J. Impact Eng., 38(4), 252 – 263 (2011).10.1016/j.ijimpeng.2010.10.035 ↗
47. B. Liu, T. Xu, X. Xu, Y. Wang, Y. Sun, and Y. Li., “Energy absorption mechanism of polyvinyl butyral laminated windshield subjected to head impact: Experiment and numerical simulations,” Int. J. Impact Eng., 90, 26 – 36 (2016).10.1016/j.ijimpeng.2015.11.010 ↗
48. Y. Jung, H. Oh, and M. M. Jeong, “An approach to automated detection of structural failure using chronological image analysis in temporary structures,” Int. J. Constr. Manag., 19(2), 178 – 185 (2019).
49. M. V. Swain, “Nickel sulphide inclusions in glass: an example of microcracking induced by a volumetric expanding phase change,” J. Mater. Sci., 16(1), 151 – 158 (1981).10.1007/BF00552069 ↗
50. A. Kasper, F. Bordeaux, and L. Duffrene, “Nickel sulphide: new results to optimise the heat soak test for thermally toughened building glasses,” Glass Science and Technology (Frankfurt), 73(5), 130 – 142 (2000).
51. J. Schneider and J. Hilcken, “Nickel Sulphide (NiS-) induced failure of glass: fracture mechanics model and verification by fracture data (engineered transparency),” in: Int. Conf. at Glasstec, Düsseldorf, Germany, 30.09.2010 (2010).
52. S. Karlsson, “Spontaneous fracture in thermally strengthened glass-a review and outlook,” Ceram.-Silik., 61(3), 188 – 201 (2017).10.13168/cs.2017.0016 ↗
53. GB/T 36269–2018, Determination of Trace Nickel for Plate Glass, China National Standards, The Standardization Administration of the People’s Republic of China (2018).
54. D. Honfi, A. Reith, L. G. Vigh, and G. Stocker., “Why glass structures fail? — Learning from failures of glass structures,” in: Proc. of the Challenging Glass, Vol. 4 (2014).10.1201/b16499-109 ↗
55. X.-e.Wang, J. Yang, Q. Liu, and C. Zhao, “Experimental investigations into SGP laminated glass under low velocity impact,” Int. J. Impact Eng., 122, 91 – 108 (2018).10.1016/j.ijimpeng.2018.06.010 ↗
56. M. Overend, G. Parke, and D. Buhagiar, “Predicting failure in glass-a general crack growth model,” J. Struct. Eng. (N Y N Y), 133(8), 1146 (2007).10.1061/(ASCE)0733-9445(2007)133:8(1146) ↗
57. M. Govindasamy, G. Kamalakannan, C. Kesavan, and G. K. Meenashisundaram, “Damage detection in glass/epoxy laminated composite plates using modal curvature for structural health monitoring applications,” J. Compos. Sci., 4(4), 185 (2020).10.3390/jcs4040185 ↗
58. U. Starossek, and M. Haberland, “Robustness of structures,” Int. J. Lifecycle Perform. Eng., 1(1), 3 – 21 (2012).10.1504/IJLCPE.2012.051279 ↗
59. R. A. Behr, J. E. Minor, and M. P. Linden, “Load duration and interlayer thickness effects on laminated glass,” J. Struct. Eng., 112(6), 1441 – 1453 (1986).10.1061/(ASCE)0733-9445(1986)112:6(1441) ↗
60. T. Trejos, S. Montero, and J. R. Almirall, “Analysis and comparison of glass fragments by laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) and ICP-MS,” Anal. Bioanal. Chem., 376(8), 1255 – 1264 (2003).10.1007/s00216-003-1968-0 ↗
61. J. E. Minor, and P. L. Reznik, “Failure strengths of laminated glass,” J. Structu. Eng., 116(4), 1030 – 1039 (1990).10.1061/(ASCE)0733-9445(1990)116:4(1030) ↗
62. R. Behr, J. Minor, and H. Norville, “Structural behavior of architectural laminated glass,” J. Struct. Eng., 119(1), 202 – 222 (1993).10.1061/(ASCE)0733-9445(1993)119:1(202) ↗
63. L. R. Dharani, J. Wei, and F. Ji, “Failure analysis of laminated architectural glass panels subjected to blast loading,” WIT Trans. Built Environ., 63 (2002).
64. F. W. Flocker, and L. R. Dharani, “Stresses in laminated glass subject to low velocity impact,” Eng. Struct., 19(10), 851 – 856 (1997).10.1016/S0141-0296(97)00162-4 ↗
65. L. Dharani, and J. Yu, “Failure modes of glass panels subjected to soft missile impact,” WIT Trans. Eng. Sci., 47 (2004).
66. M. S. Shetty, J. Wei, L. R. Dharani, and D. S. Stutts, “Analysis of damage in laminated architectural glazing subjected to wind loading and windborne debris impact,” Buildings, 3(2), 422 – 441 (2013).10.3390/buildings3020422 ↗
67. H. D. Hidallana-Gamage, D. Thambiratnam, and N. Perera, “Failure analysis of laminated glass panels subjected to blast loads,” Eng. Fail. Anal., 36, 14 – 29 (2014).10.1016/j.engfailanal.2013.09.018 ↗
68. E. Orowan, “The fatigue of glass under stress,” Nature, 154(3906), 341 – 343 (1944).10.1038/154341a0 ↗
69. G. R. Irwin, “Analysis of stresses and strains near the end of a crack traversing a plate,” J. Appl. Mech., 24(3), 361 – 364 (1957).10.1115/1.4011547 ↗
70. W. G. Brown, A load Duration Theory for Glass Design, Division of Building Research, National Research Council (1969).
71. W. L. Beason, A Failure Prediction Model for Window Glass, Texas Tech University (1980).
72. A. C. Fischer-Cripps, and R. E. Collins, “Architectural glazings: Design standards and failure models,” Build. Environ., 30(1), 29 – 40 (1995).10.1016/0360-1323(94)E0026-N ↗
73. P. L. Reznik, Failure Strengths of Laminated Glass Units, Texas Tech University (1986).
74. K. W. King, The Effect of Interlayer Thickness on Laminated Glass Strength, Texas Tech University (1996).
75. A. Kott, and T. Vogel, “Safety of laminated glass structures after initial failure,” Struct. Eng. Int., 14(2), 134 – 138 (2004).10.2749/101686604777964099 ↗
76. X. Zhang, H. Hao, and Z.Wang, “Experimental investigation of monolithic tempered glass fragment characteristics subjected to blast loads,” Eng. Struct., 75, 259 – 275 (2014).10.1016/j.engstruct.2014.06.014 ↗
77. C. Zhao, J. Yang, X.Wang, and I. Azim, “Experimental investigation into the post-breakage performance of pre-cracked laminated glass plates,” Constr. Build. Mater., 224, 996 – 1006 (2019).10.1016/j.conbuildmat.2019.07.286 ↗
78. X. Xie, “A review of recent advances in surface defect detection using texture analysis techniques,” Electron. Lett. Comput. Vis. Image Anal., 1 – 22 (2008).10.5565/rev/elcvia.268 ↗
79. V. Hotař, F. Novotný, and H. Reinischová, “Objective evaluation of the corrugation test for sheet glass surfaces,” Glass Technol.: Eur. J. Glass Sci. Technol. A, 52(6), 197 – 202 (2011).
80. Z. Yiyang, “The design of glass crack detection system based on image preprocessing technology,” in: IEEE 7th Joint International Information Technology and Artificial Intelligence Conference (2014).10.1109/ITAIC.2014.7065001 ↗
81. M. Fröling, Strength Design Methods for Glass Structures, Division of Structural Mechanics, Department of Construction Sciences, Lund (2013).
82. C. Fors, Mechanical Properties of Interlayers in Laminated Glass-Experimental and Numerical Evaluation, TVSM (2014).
83. M. Overend, S. De Gaetano, and M. Haldimann, “Diagnostic interpretation of glass failure,” Struct. Eng. Int., 17(2), 151 – 158 (2007).10.2749/101686607780680790 ↗
84. Y. Yuan, P. Tan, and Y. Li, “Dynamic structural response of laminated glass panels to blast loading,” Compos. Struct., 182, 579 – 589 (2017).10.1016/j.compstruct.2017.09.028 ↗
85. B. R. Lawn, “Indentation of ceramics with spheres: a century after Hertz,” J. Am. Ceram. Soc., 81(8), 1977 – 1994 (1998).10.1111/j.1151-2916.1998.tb02580.x ↗
86. G. R. Lachance, F. Claisse, R. Jenkins, R. W. Gould, and D. Gedcke, Thin Films In: Quantitative x-ray Fluorescence analysis: Theory and Practice, JohnWiley and Sons, New York (1995), pp. 211 – 216.
87. E. M. Cahoon, and J. R. Almirall, “Wavelength dependence on the forensic analysis of glass by nanosecond 266 nm and 1064 nm laser induced breakdown spectroscopy,” Appl. Opt., 49(13), C49 – C57 (2010).10.1364/AO.49.000C49 ↗
88. T. Trejos, R. Koons, S. Becker, T. Berman, J. Buscaglia, M. Duecking, T. Eckert-Lumsdon, T. Ernst, C. Hanlon, A. Heydon, and K. Mooney, “Cross-validation and evaluation of the performance of methods for the elemental analysis of forensic glass by μ-XRF, ICP-MS, and LA-ICP-MS,” Anal. Bioanal. Chem., 405(16), 5393 – 5409 (2013).10.1007/s00216-013-6978-y ↗
89. D. Hull, Fractography: Observing, Measuring and Interpreting Fracture Surface Topography, Cambridge University Press (1999).
90. D. Harris, R. Lilly, and T. Willmott, “A consultants toolbox for investigating nickel sulphide failures in toughened glass,” in: Proc. Glass Processing Days (2003).
91. A. Sobhani, and M. Salavati-Niasari, “Synthesis, characterization, optical and magnetic properties of a nickel sulfide series by three different methods,” Superlattices Microstruct., 59, 1 – 12 (2013).10.1016/j.spmi.2013.03.018 ↗
92. B. R. Lawn, Fracture of Brittle Solids, Cambridge Solid State Science Series (1993).10.1017/CBO9780511623127 ↗
93. P. Kuisma-Kursula, “Accuracy, precision and detection limits of SEM–WDS, SEM–EDS and PIXE in the multi-elemental analysis of medieval glass,” Xray Spectrom., 29(1), 111 – 118 (2000).10.1002/(SICI)1097-4539(200001/02)29:1<111::AID-XRS408>3.0.CO;2-W ↗
94. K. Persson, K. Haller, S. Karlsson, and M. Kozłowski, “Non-destructive testing of the strength of glass by a non-linear ultrasonic method,” in: Challenging Glass Conf. Proc. (2020).
95. Z. Zhao, “Review of non-destructive testing methods for defect detection of ceramics,” Ceram. Int., 47(4), 4389 – 4397 (2021).10.1016/j.ceramint.2020.10.065 ↗
96. EN14179-1, Glass in Building – Heat Soaked Thermally Toughened Soda Lime Silicate Safety Glass (2005).
97. ISO 20657, Glass in Building – Heat Soaked Tempered Soda Lime Silicate Safety Glass (2017).
98. A. Bonati, G. Pisano, and G. R. Carfagni, “A probability model for evaluating the effectiveness of the Heat Soak Test,” Glass Struct. Eng., 4(3), 377 – 388 (2019).10.1007/s40940-019-00101-w ↗
99. L. M. Pascoe, D. C. Smith, P. Del Linz, J. Dear, and D. Cormie, “Development of a validated engineering model of laminated glass under blast loading,” in: Structures Congress 2012 (2012), pp. 307 – 321.
100. L. R. Piscitelli, Serviceability and Post-Failure Behaviour of Laminated Glass Structural Elements, Firenze University Press (2019).10.36253/978-88-6453-985-0 ↗