Design, fabrication, and testing of CVI-SiC/SiC turbine blisk under different load spectrums at elevated temperature
Source abstract
Abstract
Abstract In this article, design, fabrication, and testing of SiC/SiC turbine blisk with the fiber’s preform of Spider Web Structure (SWS) subjected to different load spectrums at elevated temperature are conducted. Micro-CT scans are conducted to show the fibers preform and defects inside the SWS-SiC/SiC turbine blisk. For 2D plain-woven SiC/SiC composite under monotonic tensile loading at an elevated temperature of T = 900°C in air atmosphere, the composite ultimate tensile strength is σ uts = 200 MPa with the fracture strain ε f = 0.36%. For SWS-SiC/SiC turbine blisk under the rotation testing, the first and second order natural frequency of the SWS-SiC/SiC turbine blisk are tested using the laser vibration meter. Relationships between the rotation speed, internal damage, and the natural frequency degradation of the SWS-SiC/SiC turbine blisk are established. Under the maximum rotation speed of n = 17,000 rpm at the exhaust temperature of T = 930°C, no damage occurred in the SWS-SiC/SiC turbine blisk. However, multiple coating spalling occurred due to the thermal-chemical coupling failure of the coating under flame impingement. The first natural frequency of the SWS-SiC/SiC turbine blisk decreases by 5% with the increase in the rotating speed from n max = 85,000 rpm to n max = 105,000 rpm, which indicates that there is an internal damage in the SWS-SiC/SiC turbine blisk, which leads to the decrease in the stiffness of the blisk.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fire effects on concrete materials · Electromagnetic Launch and Propulsion Technology · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
AECC Hunan Aviation Powerplant Research Institute , Zhuzhou 412000 , People’s Republic of China
Powder Metallurgy Research Institute, Central South University , Changsha , Hunan 410083 , People’s Republic of China
College of Civil Aviation, Nanjing University of Aeronautics and Astronautics , No. 29 Jiangjun Ave. , Nanjing 211106 , People’s Republic of China
School of Aircraft Engineering, Nanchang Hangkong University , Nanchang 330063 , People’s Republic of China
References (33)
Show source-provided references
1. Li, L. B. High temperature mechanical behavior of ceramic-matrix composites, Wiley-VCH, Weinheim, Germany, 2021.10.1002/9783527831791 ↗
2. Liu, Q. M., S. Z. Huang, and A. J. He. Application requirements and challenges of CMC-SiC composites on aero-engine. Journal of Materials Engineering, Vol. 47, 2019, pp. 1–10.
3. Naslain, R. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: An overview. Composites Science and Technology, Vol. 64, 2004, pp. 155–170.10.1016/S0266-3538(03)00230-6 ↗
4. Li, L. B. Damage, fracture and fatigue of ceramic-matrix composites, Springer Nature, Singapore, 2018.10.1007/978-981-13-1783-5 ↗
5. Li, L. B. Durability of ceramic-matrix composites, Woodhead Publishing, Oxford, UK, 2020.
6. Li, L. B. Thermomechanical fatigue of ceramic-matrix composites, Wiley-VCH, Weinheim, Germany, 2019.10.1002/9783527822614 ↗
7. Udayakumar, A., A. S. Ganesh, S. Raja, and M. Balasubramaian. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI. Journal of the European Ceramic Society, Vol. 31, 2011, pp. 1145–1153.10.1016/j.jeurceramsoc.2010.12.018 ↗
8. Liu, X. C., X. J. Guo, Y. L. Xu, L. B. Li, W. Zhu, Y. Q. Zeng, et al. Cyclic thermal shock damage behavior in CVI SiC/SiC high-pressure turbine twin guide vanes. Materials, Vol. 14, 2021, id. 610410.3390/ma14206104 ↗
9. Liu, H. T., H. F. Cheng, J. Wang, and G. Tang. Effects of the single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process. Ceramics International, Vol. 36, 2010, pp. 2033–2037.10.1016/j.ceramint.2010.05.014 ↗
10. Yu, H. J., X. G. Zhou, W. Zhang, H. X. Peng, and C. R. Zhang. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases. Material and Design, Vol. 44, 2013, pp. 320–324. 10.1016/j.matdes.2012.07.073.10.1016/j.matdes.2012.07.073 ↗
11. Yin, J., S. H. Lee, L. Feng, Y. Zhu, X. Liu, Z. Huang, et al. The effects of SiC precursors on the microstructures and mechanical properties of SiCf/SiC composites prepared via polymer impregnation and pyrolysis process. Ceramics International, Vol. 41, 2015, pp. 4145–4153.10.1016/j.ceramint.2014.11.112 ↗
12. Luo, Z., X. Zhou, and J. S. Yu. Mechanical properties of SiC/SiC composites by PIP process with a new precursor at elevated temperature. Materials Science & Engineering, A: Structural Materials: Properties, Microstructure and Processing, Vol. 607, 2014, pp. 155–16110.1016/j.msea.2014.03.011 ↗
13. Yang, H. T., S. W. Xu, D. X. Zhang, L. B. Li, and X. Z. Huang. In-situ tensile damage and fracture behavior of PIP SiC/SiC minicomposites at room temperature. Journal of the European Ceramic Society, Vol. 41, 2021, pp. 6869–688210.1016/j.jeurceramsoc.2021.06.050 ↗
14. Corman, G. S. and K. L. Luthra. Silicon melt infiltrated ceramic composites (HiPerCompTM). Handbook of ceramic composites, Kluwer Academic Publishers, Boston, 2004.
15. Bhat, B. N. Aerospace materials and applications, American Institute of Aeronautics and Astronautics, USA, 2018.
16. Steibel, J. Ceramic matrix composites taking flight at GE aviation. American Ceramic Society Bulletin, Vol. 98, 2019, pp. 30–33.
17. Ogawa, A. An application study of carbon/carbon composites to turbine rotors, National Aerospace Laboratory, Tokyo, 2001.
18. Nozhnitsky, Y. A. The problem of ensuring reliability of gas turbine engines. IOP Conference Series: Materials Science and Engineering, Vol. 302, 2018, id. 12082.10.1088/1757-899X/302/1/012082 ↗
19. Hilmas, A. M., G. Henson, A. Singhal, Y. Gao, and M. Schuster. In-situ observation of damage in unidirectional CMC laminates under tension. Ceramics International, Vol. 46, 2020, pp. 13502–13510.10.1016/j.ceramint.2020.02.134 ↗
20. Kim, J. and P. K. Liaw. Fracture behavior of ceramic matrix composites during monotonic and cyclic loadings. Key Engineering Materials, Vol. 345–346, 2007, pp. 649–652.10.4028/www.scientific.net/KEM.345-346.649 ↗
21. Chateau, C., L. Gelebart, M. Bornert, J. Crepin, D. Caldemaison, and C. Sauder. Modeling of damage in unidirectional ceramic matrix composites and multi-scale experimental validation on third generation SiC/SiC minicomposites. Journal of the Mechanics and Physics of Solids, Vol. 63, 2014, pp. 298–319.10.1016/j.jmps.2013.09.001 ↗
22. Chateau, C., L. Gelebart, M. Bornert, J. Crepin, E. Boller, C. Sauder, et al. In situ X-ray microtomography characterization of damage in SiCf/SiC minicomposites. Composites Science and Technology, Vol. 71, 2011, pp. 916–924.10.1016/j.compscitech.2011.02.008 ↗
23. Maillet, E., N. Godin, M. R’Mili, P. Reynaud, G. Fantozzi, and J. Lamon. Damage monitoring and identification in SiC/SiC minicomposites using combined acousto-ultralics and acoustic emission. Composites Part A, Vol. 57, 2014, pp. 8–15.10.1016/j.compositesa.2013.10.010 ↗
24. Whitlow, T., E. Jones, and C. Przybyla. In-situ damage monitoring of a SiC/SiC ceramic matrix composite using acoustic emission and digital image correlation. Composite Structures, Vol. 158, 2016, pp. 245–251.10.1016/j.compstruct.2016.09.040 ↗
25. Smith, C. E., G. N. Morscher, and Z. H. Xia. Monitoring damage accumulation in ceramic matrix composites using electrical resistivity. Scripta Mater, Vol. 59, 2008, pp. 463–466.10.1016/j.scriptamat.2008.04.033 ↗
26. Gyekenyesi, A. L., G. N. Morscher, and L. M. Cosgriff. In situ monitoring of damage in SiC/SiC composites using acousto-ultrasonics. Composites Part B, Vol. 37, 2006, pp. 47–53.10.1016/j.compositesb.2005.05.010 ↗
27. Bai, R., J. Chu, M. Wang, and H. Chen. Numerical prediction of frequency of delaminated advanced grid stiffened plate. Journal of Chongqing University, Vol. 28, 2005, pp. 119–124.
28. Li, H. Analysis of vibration and damage test of ceramic matrix composites structure. Master Thesis, Nanchang Hangkong University, Nanchang, China, 2019.
29. Duan, H., Z. W. Zhang, L. B. Li, and W. J. Li. Effect of pyrocarbon interphase texture and thickness on tensile damage and fracture in T-700TM C/SiC minicomposites. Journal of the American Ceramic Society, Vol. 105, 2021, pp. 2171–2181.10.1111/jace.18193 ↗
30. United States Air Force. Engine structural integrity program (ENSIP):MIL-STD-1783, United States Department of Defense, Washington, 1984.
31. United States Department of Defense. General specification for aircraft turbojet, turbofan, turboshaft and turboprop engine: JSSG-87231A, United States Department of Defense, Washington, 1995.
32. Yang, L. Thermalization coupling theory and characterization method of damage mechanism of thermal barrier coatings. Journal of Xiangtan University, Vol. 41, 2019, pp. 17–26.
33. Min, J. B., D. L. Harris, and J. M. Ting. Advances in ceramic matrix composite blade damping characteristics for aerospace turbomachinery applications. The 52nd AIAA/ASME/ASCE/AHS/ASC Structures, Structural Dynamics and Materials Conference, April 4, 2011–April 7, 2011.10.2514/6.2011-1784 ↗