journal article·2018-08-28Open access

Effect of Pre-Oxidation on the Steam Oxidation of Heat-Resistant Steel T92

Xu Hong, Liang Zhiyuan, Ding Jianliang, Zhao Qinxin, Guan Shipian

Abstract

Abstract Effect of pre-oxidation on the steam oxidation of T92 heat-resistant steel at 650 °C was investigated. The results show that the mass gain and the oxide thickness of T92 sample with pre-oxidation treatment were lower than that of T92 sample after exposure in steam at 650 °C. The compact and discrete Cr-rich oxide which formed on the pre-oxidized specimen hindered ion diffusion, leading to the lower oxidation rate. The effect of pre-oxidation worked at the initial stage due to the protective Cr-rich layer formed in air gas. After a long time exposure in steam, the pre-oxidation influence decreased slowly and eventually disappeared. What’s more, the adhesion property of oxide scale was improved by pre-oxidation.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Jiangsu Frontier Electric Technology Co. Ltd. , Nanjing 211102 , PR China

Key Laboratory of Thermal Fluid Science and Engineering of MOE , School of Energy and Power Engineering, Xi’an Jiaotong University , Xi’an 710049 , PR China

References (13)

Show source-provided references
1. F. Masuyama, ISIJ Int., 41 (6) (2001) 612–625.10.2355/isijinternational.41.61210.2355/isijinternational.41.612 ↗
2. R.Viswanathan, J.F. Henry, J. Tanzosh et al., J Mater Eng Perform., 14 (3) (2005) 281–292.10.1361/1059949052403910.1361/10599490524039 ↗
3. P.J. Ennis and A. Czyrska-Filemonowicz, Sadhana, 28 (3-4) (2003) 709–730.10.1007/BF0270645510.1007/BF02706455 ↗
4. Y. Wang, K. Zheng, Z. Wu et al., Journey Chin. Soc. Power Eng., 30 (4) (2010) 245–252.
5. I.G. Wright and R.B. Dooley, Int. Mater. Rev., 55 (3) (2010) 129–167.10.1179/095066010X1264689872816510.1179/095066010X12646898728165 ↗
6. S.R.J.Saunders, M. Monteiro and F. Rizzo, Prog Mater Sci., 53 (5) (2008) 775–837.10.1016/j.pmatsci.2007.11.00110.1016/j.pmatsci.2007.11.001 ↗
7. P.J.Ennis and W.J. Quadakkers, Int. J. Press. Vessels Piping, 84 (1–2) (2007) 75–81.10.1016/j.ijpvp.2006.09.00710.1016/j.ijpvp.2006.09.007 ↗
8. J. Ehlers, D.J. Young, E.J. Smaardijk et al., Corrosion Sci., 48 (11) (2006) 3428–3454.10.1016/j.corsci.2006.02.00210.1016/j.corsci.2006.02.002 ↗
9. R.Viswanathan, J. Sarver and J.M. Tanzosh, J Mater Eng Perform., 15 (3) (2006) 255–274.10.1361/105994906X10875610.1361/105994906X108756 ↗
10. H. Buscail, S.E. Messki, F. Riffard et al., Oxidation Metals, 75 (1) (2011) 27–39.10.1007/s11085-010-9218-210.1007/s11085-010-9218-2 ↗
11. M. Nakai, K. Nagai, Y. Murata et al., Trans. Iron Steel Inst Japan, 45 (7) (2005) 1066–1072.10.2355/isijinternational.45.106610.2355/isijinternational.45.1066 ↗
12. Z. Liang, P.M. Singh, Q. Zhao et al., Oxidation Metals, 84 (3) (2015) 291–305.10.1007/s11085-015-9555-210.1007/s11085-015-9555-2 ↗
13. A. Atkinson, R.I. Taylor and A.E. Hughes., Philosophical Magazine Part., 45 (5) (1982) 823–833.10.1080/0141861820823990510.1080/01418618208239905 ↗