Deformation and Structure Difference of Steel Droplets during Initial Solidification
Source abstract
Abstract
Abstract The surface quality of slabs is closely related with the initial solidification at very first seconds of molten steel near meniscus in mold during continuous casting. The solidification, structure, and free deformation for given steels have been investigated in droplet experiments by aid of Laser Scanning Confocal Microscope. It is observed that the appearances of solidified shells for high carbon steels and some hyper-peritectic steels with high carbon content show lamellar, while that for other steels show spherical. Convex is formed along the chilling direction for most steels, besides some occasions that concave is formed for high carbon steel at times. The deformation degree decreases gradually in order of hypo-peritectic steel, ultra-low carbon steel, hyper-peritectic steel, low carbon steel, and high carbon steel, which is consistent with the solidification shrinkage in macroscope during continuous casting. Additionally, the microstructure of solidified shell of hypo-peritectic steel is bainite, while that of hyper-peritectic steel is martensite.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Solidification and crystal growth phenomena · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan, China
School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083, China
Shougang Research Institute of Technology, Beijing 100043, China
References (15)
Show source-provided references
1. [1] M.H. Trejo, E.A. Lopez and J.J.R. Mondragon, Metals Mater. Int., 16 (2010) 731–737.10.1007/s12540-010-1006-7 ↗
2. [2] K. Matsuura and M. Kudoh, Metals Mater., 4 (1998) 562–565.10.1007/BF03187828 ↗
3. [3] H. Mizukami, A. Yamanaka and T. Watanabe, ISIJ Int., 42 (2002) 964–973.10.2355/isijinternational.42.964 ↗
4. [4] V. Guyot, J. Martin and A. Ruelle, ISIJ Int., 36 (1996) S223–S227.10.2355/isijinternational.36.Suppl_S223 ↗
5. [5] S.X. Dong, E. Niyama and K. Anzai, Mater. Trans., 35 (1994) 196–198.10.2320/matertrans1989.35.196 ↗
6. [6] H. Esaka, T. Shirakami and T. Mizoguchi, Tetsu to Hagané, 81 (1995) 631–636.10.2355/tetsutohagane1955.81.6_631 ↗
7. [7] M. Suzuki and Y. Yamaoka, Mater. Trans., 44 (2003) 836–844.10.2320/matertrans.44.836 ↗
8. [8] H. Mizukami and A. Yamanaka, ISIJ Int., 50 (2010) 435–444.10.2355/isijinternational.50.435 ↗
9. [9] S. Dong, E. Niyama and K. Anzai, ISIJ Int., 35 (1995) 730–736.10.2355/isijinternational.35.730 ↗
10. [10] M.G. Shen, S.T. Jin and E. Niyama, Acta Metall. Sinica, 36 (2000) 1104–1108 ((In Chinese)).
11. [11] H. Todoroki and N. Phinichka, ISIJ Int., 49 (2009) 1347–1355.10.2355/isijinternational.49.1347 ↗
12. [12] Y. Li, X. Zhang and P. Lan, Int. J. Miner. Metall Mater., 20 (2013) 138–145.10.1007/s12613-013-0705-8 ↗
13. [13] B.G. Thomas, ISIJ Int., 35 (1995) 737–743.10.2355/isijinternational.35.737 ↗
14. [14] H. Murakami and M. Suzuki, Tetsu to Hagane, 78 (1987) 105–112.10.2355/tetsutohagane1955.78.1_105 ↗
15. [15] Y. Sugitani and M. Nakamura, Tetsu to Hagane, 65 (1979) 1702–1711.10.2355/tetsutohagane1955.65.12_1702 ↗