journal article·2018-04-25Open access

Study on the Growth Mechanism of K 2 Ti 4 O 9 Crystal

Xuesong Zhou, Jing Fan, Xiaoli Wei, Yi Shen, Yanzhi Meng

Abstract

Abstract Potassium hexatitanate (K 2 Ti 4 O 9 ) whiskers were prepared by the kneading–drying–calcination method. After the preparation of products under different calcination temperatures and holding times, their morphology and structure were characterized by thermogravimetric and differential thermal, X-ray diffraction (XRD), scanning electron microscopy and transmission electron microscopy. The XRD analysis showed that the reaction mixture was completely converted to K 2 Ti 4 O 9 crystals at 800 °C when the T/K ratio was 3. Based on the analysis of LS (liquid–solid) growth mechanism, the corresponding transformation reaction mechanism during the roasting was elucidated. K 2 Ti 4 O 9 whiskers grow mainly through the parallel action at a low temperature. With the increase in temperature, the series effect is obvious.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Hebei Provincial Key Laboratory of Inorganic Nonmetallic Materials, College of Materials Science and Engineering , North China University of Science and Technology , Tangshan , Hebei 063009 , PR China

References (15)

Show source-provided references
1. N. Bao, X. Feng, X. Lu and Z. Yang, J. Mater. Sci., 37 (2002) 3035–3043.10.1023/A:101608541799010.1023/A:1016085417990 ↗
2. T. Zaremba, J. Therm, Anal. Calorim., 91 (2008) 911–913.10.1007/s10973-007-8608-410.1007/s10973-007-8608-4 ↗
3. S. Tan, Y. Zhang and H. Gong, J-Stage., 5 (2007) 13–18.10.2965/jwet.2007.13 ↗
4. B.B. Zhang, L.I. Hua-Ming, H. Liu, et al., Environ. Sci. Technol., 34 (2011) 40–43.
5. J. Zhang, Y.A. Wang, J. Yang, et al., Mater. Lett., 60 (2006) 3015–3017.10.1016/j.matlet.2006.02.03610.1016/j.matlet.2006.02.036 ↗
6. S.O. Kang, H.S. Jang, Y. Kim, et al., Mater. Lett., 61 (2007) 473–477.10.1016/j.matlet.2006.04.09110.1016/j.matlet.2006.04.091 ↗
7. Y.X. Zhou, C. Liu, M. He, et al., Chin. J. Chem. Eng., 15 (2007) 742–747.10.1016/S1004-9541(07)60156-610.1016/S1004-9541(07)60156-6 ↗
8. K. Chen and G. Wang, Refractories., 28 (2010) 909–919.10.1080/02640414.2010.484065 ↗
9. C.Y. Liu, Y.M. Liu, Q.I. Lin, et al., Zhongguo Youse Jinshu Xuebao., 18 (2008) 2270–2274.10.1016/j.juro.2008.01.146 ↗
10. T. Zaremba and D. Witkowska, Mater. Sci.-Pol., 28 (2010) 25–41.
11. H.Y. Zhu, Y. Lan, X.P. Gao, et al., J. Am. Chem. Soc., 127 (2005) 6730–6736.10.1021/ja044689+10.1021/ja044689+ ↗
12. C. Liu, H. Yin, Y. Liu, et al., Mater. Res. Bull., 44 (2009) 1173–1178.10.1016/j.materresbull.2008.09.03810.1016/j.materresbull.2008.09.038 ↗
13. S. Zhang, J. Wu, X.L. Ji, et al., Taylor and Francis Online., 19 (2015) 340–344.10.1179/1432891715Z.0000000002190 ↗
14. X. Ji, S. Wu, S. Zhang, et al., Integr. Ferroelectr., 153 (2014) 156–163.10.1080/10584587.2014.90313210.1080/10584587.2014.903132 ↗
15. K.K. Chen, G. Wang and L.W. Wang. Guisuanyan Tongbao, (2010).