journal article·2019-02-25Open access

The effect of MgTiO 3 Adding on Inclusion Characteristics

Xu Chen, Zhang Mingya, Li Jianli, Ran Songlin, Shan Mengwei, Yue Qiang, Kong Hui

Abstract

Abstract MgTiO 3 powder was directly added into molten steel at 1873K, and its effect on inclusion characteristics was studied by a scanning electron microscope and an energy dispersive spectrometer. Thermodynamic calculation indicates that MgTiO 3 is unstable in molten steel and may decompose into [Ti], [O] and MgO. However, only Ti-bearing inclusions were observed in the treated sample, and Mg-bearing inclusions were absent. This can be explained by the features of wettability and stability for MgO. Compared with a Non-treated sample, both oxide and coarse MnS in treated sample were refined. For the oxide, this originates from the formation of Ti-bearing inclusion. For coarse MnS, this may be due to the fact that Ti can aggravate S segregation. Besides, this aggravation makes coarse MnS less globular. After etching, it was found that in the treated sample, Ti-bearing inclusion can induce the nucleation of intragranular acicular ferrites. This appearance was totally different from that of Non-treated sample, and indicates the effectiveness of external adding method in oxide metallurgy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Aluminum Alloy Microstructure Properties · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Metallurgical Engineering, Anhui University of Technology , Maanshan, Anhui , 243002, P R China

Key Laboratory of Metallurgical Emission Reduction & Resources Recycling (Anhui University of Technology), Ministry of Education , Maanshan, Anhui , 243002 , P R China )

The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology , Wuhan, Hubei , 430081 , P R China

References (30)

Show source-provided references
1. J.Takamura and S. Mizoguchi, Proceedings of the sixth international iron and steel congress, Nagoya, 1(1990) 591-597.
2. T. Koseki, and G.Thewlis, Mater. Sci. Technol., 21(2005) 867-879.10.1179/174328405X5170310.1179/174328405X51703 ↗
3. X.L.Wan XL, R.Wei, and K.M.Wu, Mater. Charact., 61(2010) 726-731.10.1016/j.matchar.2010.04.00410.1016/j.matchar.2010.04.004 ↗
4. J.-S.Byun, J.-H Shim, and Y.W Cho, Scripta Mater., 48(2003) 449-454.10.1016/S1359-6462(02)00437-210.1016/S1359-6462(02)00437-2 ↗
5. N.Kikuchi, S.Nabeshima, Y.Kishimoto, T.Matsushita, and S. Sridhar, ISIJ. Int., 47(2007) 1255-1264.10.2355/isijinternational.47.125510.2355/isijinternational.47.1255 ↗
6. W.Z.Mu, P.G.Jönsson, and K.Nakajima, High Temp. Mater. Proc. 36(2017) 309-325.10.1515/htmp-2016-0175 ↗
7. J.M.Gregg, and H.K.D.H.Bhadeshia, Metall. Mater. Trans. A, 25(1994) 1603-1611.10.1007/BF0266852610.1007/BF02668526 ↗
8. S.H.Zhang, N.Hattori, M.Enomoto, and T.Tarui, ISIJ. Int., 36(1996) 1301-1309.10.2355/isijinternational.36.130110.2355/isijinternational.36.1301 ↗
9. W.Z.Mu, P.G.Jönsson, and K.Nakajima, ISIJ. Int., 52(2014) 2907-2916.10.2355/isijinternational.54.2907 ↗
10. W.Z.Mu, P.G.Jönsson, H.Shibata, and K.Nakajima, STEEL RES INT, 87(2016), 339-348.10.1002/srin.20150006110.1002/srin.201500061 ↗
11. J.M.Gregg, and H.K.D.H.Bhadeshia, Acta Mater., 45(1997) 739-748.10.1016/S1359-6454(96)00187-510.1016/S1359-6454(96)00187-5 ↗
12. S.H.Nedjad, and A.Farzaneh, Scripta Mater., 57(2007) 937-940.10.1016/j.scriptamat.2007.07.01610.1016/j.scriptamat.2007.07.016 ↗
13. Ø.Grong, L.Kolbeinsen, C.Van Der Eijk, and G.Tranell, ISIJ. Int., 46(2006) 824-831.10.2355/isijinternational.46.82410.2355/isijinternational.46.824 ↗
14. M.Kiviö, L.Holappa, and T.Iung, Metall. Mater. Trans. B, 41(2010) 1194-1204.10.1007/s11663-010-9416-y10.1007/s11663-010-9416-y ↗
15. X.Z.Gao, S.F.Yang, J.S.Li, Y.D.Yang, K.Chattopadhyay, and A.Mclean, Metall. Mater. Trans. A, 47(2016) 461-470.10.1007/s11661-015-3237-110.1007/s11661-015-3237-1 ↗
16. X.Z.Gao, S.F.Yang, J.S.Li, H.Liao, W.Gao, and T.Wu, Metall. Mater. Trans. B, 47(2016) 1124-1136.10.1007/s11663-015-0552-210.1007/s11663-015-0552-2 ↗
17. H.Guo, S.F.Yang, J.S.Li, M.J.Zhao, Z.Y.Chen, X.L.Zhang, and J.K.Li, JOM, 70(2018) 1136-1142.10.1007/s11837-018-2892-210.1007/s11837-018-2892-2 ↗
18. S.-J.Zhuo, Y.-Q.Wang, X.-H.Wang, and H.-G.Lee, J Iron Steel Res Int., 17(2010) 10-16.10.1016/S1006-706X(10)60051-9 ↗
19. X.B.Li, M.Yi, C.J.Liu, and M.F.Jiang, STEEL RES INT, 87(2016) 622-632.10.1002/srin.20150016710.1002/srin.201500167 ↗
20. Y.Liu, X.L.Wan, G.Q.Lia, Y.Wang, W.Zheng and Y.H.Hou, SCI TECH-NOL WELD, 27(1996) 848-853.
21. X.X.Deng, J.Min, and X.-H.Wang, Acta Metall. Sin.(Engl. Lett.), 25(2012) 241-248.
22. B.L.Cai, and M.X.Jiang, REFRACT, 43(2009) 346-349.10.1080/02844310701822826 ↗
23. T.S.Zhang, C.J.Liu, J.Y.Qiu, X.B.Li, and M.F.Jiang, ISIJ. Int., 57(2017) 314-321.10.2355/isijinternational.ISIJINT-2016-41710.2355/isijinternational.ISIJINT-2016-417 ↗
24. P.Shen, L.F.Zhang, H.Zhou, Y.Ren, and Y.Wang, Ceram. Int., 43(2017) 7674-7681.10.1016/j.ceramint.2017.03.06710.1016/j.ceramint.2017.03.067 ↗
25. L.C.Zheng, A.Malfliet, P.Wollants, B.Blanpain, and M.Guo, Metall. Mater. Trans. B, 48(2017) 2447-2458.10.1007/s11663-017-1050-510.1007/s11663-017-1050-5 ↗
26. Y.Ueshima, S.Mizoguchi, T.Matsumiya, and H.Kajioka, Metall. Mater. Trans. B, 17(1986) 845-859.10.1007/BF0265714810.1007/BF02657148 ↗
27. T.Yokoyama, Y.Ueshima, K.Sasai, Y.Mizukami, H.Kakimi and M.Kato, Tetsu-to-Hagané, 83(1997) 25-30.10.2355/tetsutohagane1955.83.9_557 ↗
28. H.Ono, K.Morita, and N.Sano, Metall. Mater. Trans. B, 26(1995) 991-995.10.1007/BF02654100 ↗
29. H.Ono, H.Fukagawa, K.Morita, and N.Sano, Metall. Mater. Trans. B, 24(2018) 43-51.
30. K.Ogino, K.Nogi, and O.Yamase, Transactions ISIJ, 23(1983) 234-239.10.2355/isijinternational1966.23.23410.2355/isijinternational1966.23.234 ↗