Liquid sorption, swelling and surface energy properties of unmodified and thermally modified Scots pine heartwood after extraction
Source abstract
Abstract
Abstract The effect of extractives removal on liquid sorption, swelling and surface energy properties of unmodified wood (UW) and thermally modified Scots pine heartwood (hW) (TMW) was studied. The extraction was performed by a Soxtec procedure with a series of solvents and the results were observed by the multicycle Wilhelmy plate method, inverse gas chromatography (IGC) and Fourier transform infrared (FTIR) spectroscopy. A significantly lower rate of water uptake was found for the extracted UW, compared with the unextracted one. This is due to a contamination effect in the latter case from water-soluble extractives increasing the capillary flow into the wood voids, proven by the decreased water surface tension. The swelling in water increased after extraction 1.7 and 3 times in the cases of UW and TMW, respectively. The dispersive part of the surface energy was lower for the extracted TMW compared to the other sample groups, indicating an almost complete removal of the extractives. The FTIR spectra of the extracts showed the presence of phenolic compounds but also resin acids and aliphatic compounds.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Adsorption, diffusion, and thermodynamic properties of materials · Wood Treatment and Properties · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. The effect of extractive content on moisture diffusion properties for Scots pine and Norway spruce
2. Measurement of wood wettability by the Wilhelmy method. Part 1. Contamination of probe liquids by extractives
3. Characterization of emissions from thermally modified wood and their reduction by chemical treatment10.15376/biores.3.2.491-502 ↗
4. Chemical analysis of heat treated softwoods10.1007/s00107-005-0078-4 ↗
5. Hot water extracted wood fiber for production of wood plastic composites (WPCs)10.1515/hf-2012-0071 ↗
6. Chemical and ultrastructural changes in compound middle lamella (CML) regions of softwoods thermally modified by the Termovuoto process10.1515/hf-2013-0221 ↗
7. Chemical changes of heat treated pine and eucalypt wood monitored by FTIR
8. The influence of wood polymers and extractives on wood colour induced by hydrothermal treatment10.1007/s00107-002-0320-2 ↗
9. Effects of heat treatment on the behaviour of extractives in softwood studied by FTIR spectroscopic methods10.1007/s00226-003-0178-4 ↗
10. Influence of post-extraction on photostability of thermally modified scots pine wood during artificial weathering
11. Characterization of emissions from thermally modified wood and their reduction by chemical treatment10.15376/biores.3.2.491-502 ↗
12. Natural surface inactivation of Scots pine and Norway spruce evaluated by contact angle measurements10.1007/s001070050067 ↗
13. Effect of extraction on the volume dimensions and specific gravity of solid wood blocks
14. Methods of Wood Chemistry. Vol I · 1967
15. Promotion effect of NP fire retardant pre-treatment on heat-treated poplar wood. Part 2: hygroscopicity, leaching resistance, and thermal stability10.1515/hf-2016-0213 ↗
16. Ageing of modified wood. Part I: wetting properties of acetylated, furfurylated, and thermally modified wood
17. Spectrometric Identification of Organic Compounds · 1998 · 71
18. Methods of Wood Chemistry. Vol I · 1967
19. Relationship of wood surface energy to surface composition10.1021/la970573y ↗
20. Influence of extractives on wood gluing and finishing – a review
21. Water uptake and wetting behaviour of furfurylated, N-methylol melamine modified and heat-treated wood10.1007/s00107-015-0919-8 ↗
22. Chemistry and ecotoxicity of thermally modified pine wood extractives10.1007/s00226-010-0356-0 ↗
23. Swelling of wood. Part III. Effect of temperature and extractives on rate and maximum swelling10.1515/hfsg.1995.49.3.239 ↗
24. Hot water extracted wood fiber for production of wood plastic composites (WPCs)10.1515/hf-2012-0071 ↗
25. Detection of pinosylvins in solid wood of Scots pine using Fourier transform Raman and infrared spectroscopy10.1080/02773819909349604 ↗
26. Surface energetics of extracted and non-extracted spruce wood particles studied by inverse gas chromatography (IGC)
27. Svenskt trä · 1952
28. The locations and morphology of resin compounds in the wood
29. Influence of post-extraction on photostability of thermally modified scots pine wood during artificial weathering
30. Promotion effect of NP fire retardant pre-treatment on heat-treated poplar wood. Part 2: hygroscopicity, leaching resistance, and thermal stability10.1515/hf-2016-0213 ↗
31. A study by X-ray photoelectron spectroscopy (XPS) of the chemistry of the surface of Scots pine (Pinus sylvestris L.) modified by friction
32. Interfacial Forces in Aqueous Media · 1994
33. Relationship of wood surface energy to surface composition10.1021/la970573y ↗
34. Multicycle Wilhelmy plate method for wetting properties, swelling and liquid sorption of wood10.1021/la402605q ↗
35. Influence of extractives on wood gluing and finishing – a review
36. Investigation of wood wettability changes during heat treatment on the basis of chemical analysis10.1016/j.polymdegradstab.2004.10.017 ↗
37. Measurement of wood wettability by the Wilhelmy method. Part 2. Determination of apparent contact angles
38. Natural durability of selected larch and scots pine heartwoods in laboratory and field tests10.1016/j.ibiod.2014.03.018 ↗
39. Measurement of wood wettability by the Wilhelmy method. Part 1. Contamination of probe liquids by extractives
40. FTIR monitoring of chemical changes in softwood during heating10.1080/02773810009349638 ↗
41. The influence of wood polymers and extractives on wood colour induced by hydrothermal treatment10.1007/s00107-002-0320-2 ↗
42. Natural surface inactivation of Scots pine and Norway spruce evaluated by contact angle measurements10.1007/s001070050067 ↗
43. Investigation of wood wettability changes during heat treatment on the basis of chemical analysis10.1016/j.polymdegradstab.2004.10.017 ↗
44. Evaluation of selective extraction methods for recovery of polyphenols from pine10.1515/hf-2013-0002 ↗
45. Chemistry and ecotoxicity of thermally modified pine wood extractives10.1007/s00226-010-0356-0 ↗
46. Wood Modification: Chemical, Thermal and Other Processes · 2006
47. Natural durability of selected larch and scots pine heartwoods in laboratory and field tests10.1016/j.ibiod.2014.03.018 ↗
48. Attractive forces at interfaces10.1021/ie50660a008 ↗
49. Ageing of modified wood. Part I: wetting properties of acetylated, furfurylated, and thermally modified wood
50. CRC Handbook of Chemistry and Physics · 1995 · 6
51. Distribution of extractives in Sitka spruce (Picea sitchensis) grown in the northern UK10.1007/s00107-013-0728-x ↗
52. Determination of chemical changes in heat-treated wood using ATR-FTIR and FT Raman spectrometry10.1016/j.saa.2016.08.026 ↗
53. Seasonal extractive variations in tree, chips and TMP
54. Principles of Wood Science and Technology – I Solid wood · 1968
55. The combined effects of boron and oil heat treatment on beech and Scots pine wood properties. Part 1: Boron leaching, thermogravimetric analysis, and chemical composition10.1007/s10853-010-4859-8 ↗
56. Characterisation of thermally modified wood: molecular reasons for wood performance improvement10.1007/s001070050287 ↗
57. Detection of pinosylvins in solid wood of Scots pine using Fourier transform Raman and infrared spectroscopy10.1080/02773819909349604 ↗
58. Inverse gas chromatographic method for measuring the dispersive surface energy distribution for particulates10.1021/la801676n ↗
59. The time limit to avoid natural inactivation of spruce surfaces intended for painting or gluing10.1007/BF03034905 ↗
60. On-line monitoring of hygroscopicity and dimensional changes of wood during thermal modification by means of neutron imaging methods10.1515/hf-2014-0008 ↗
61. Wettability and swelling of acetylated and furfurylated wood analyzed by multicycle Wilhelmy plate method10.1515/hf-2014-0196 ↗
62. Effect of extractives and thermal modification on antibacterial properties of Scots pine and Norway spruce10.1179/2042645313Y.0000000038 ↗
63. Chemical changes of heat treated pine and eucalypt wood monitored by FTIR
64. On-line monitoring of hygroscopicity and dimensional changes of wood during thermal modification by means of neutron imaging methods10.1515/hf-2014-0008 ↗
65. Extractives composition and summative chemical analysis of thermally treated eucalypt wood
66. Reaction mechanisms inhibiting the release of aqueous extracts from merbau heartwood by iron(II) and copper(II)10.1007/s00226-017-0891-z ↗
67. Effect of extractive removal on adhesion and wettability of some tropical woods
68. Spectrometric Identification of Organic Compounds · 1998 · 71
69. Wettability and swelling of acetylated and furfurylated wood analyzed by multicycle Wilhelmy plate method10.1515/hf-2014-0196 ↗
70. Fibre surface properties of kraft pulp. [Doctoral thesis] · 2009 · 2009 · 29
71. Surface energy characterization of thermally modified spruce using inverse gas chromatography under cyclic humidity conditions
72. The influence of log soaking temperature and thermal modification on the properties of birch veneers
73. Biodegradability of extractives in sapwood and heartwood from scots pine by sapstain and white rot fungi10.1515/HF.1999.042 ↗
74. The effect of extractive content on moisture diffusion properties for Scots pine and Norway spruce
75. Progress in Adhesion and Adhesives · 2015 · 125
76. Seasonal extractive variations in tree, chips and TMP
77. Swelling of wood. Part III. Effect of temperature and extractives on rate and maximum swelling10.1515/hfsg.1995.49.3.239 ↗
78. Heartwood and extractive content of scots pine in southern Finland: models to apply at harvest
79. Distribution of extractives in Sitka spruce (Picea sitchensis) grown in the northern UK10.1007/s00107-013-0728-x ↗
80. Effect of extractives and thermal modification on antibacterial properties of Scots pine and Norway spruce10.1179/2042645313Y.0000000038 ↗
81. Interfacial Forces in Aqueous Media · 1994
82. Progress in Adhesion and Adhesives · 2015 · 125
83. Multicycle Wilhelmy plate method for wetting properties, swelling and liquid sorption of wood10.1021/la402605q ↗
84. Surface energetics of extracted and non-extracted spruce wood particles studied by inverse gas chromatography (IGC)
85. Analysis by gas chromatography of the wood extractives in pulp and water samples from mechanical pulping of spruce10.3183/npprj-1989-04-01-p016-024 ↗
86. CRC Handbook of Chemistry and Physics · 1995 · 6
87. The time limit to avoid natural inactivation of spruce surfaces intended for painting or gluing10.1007/BF03034905 ↗
88. Wood Chemistry. Fundamentals and Applications · 1993
89. Heartwood and extractive content of scots pine in southern Finland: models to apply at harvest
90. Effects of heat treatment on the behaviour of extractives in softwood studied by FTIR spectroscopic methods10.1007/s00226-003-0178-4 ↗
91. Svenskt trä · 1952
92. The temperature dependent effect of extractive content on redwood shrinkage
93. Chemical and ultrastructural changes in compound middle lamella (CML) regions of softwoods thermally modified by the Termovuoto process10.1515/hf-2013-0221 ↗
94. Principles of Wood Science and Technology – I Solid wood · 1968
95. Water vapour sorption characteristics and surface chemical composition of thermally modified spruce10.1080/20426445.2016.1160590 ↗
96. Wood Chemistry. Fundamentals and Applications · 1993
97. Water uptake and wetting behaviour of furfurylated, N-methylol melamine modified and heat-treated wood10.1007/s00107-015-0919-8 ↗
98. The influence of log soaking temperature and thermal modification on the properties of birch veneers
99. Characterisation of thermally modified wood: molecular reasons for wood performance improvement10.1007/s001070050287 ↗
100. Effect of extraction on the volume dimensions and specific gravity of solid wood blocks