Abstract Wood modification is essential to enhance the performance and longevity of wood as a material while maintaining its natural and sustainable characteristics. By modifying wood, its properties can be significantly improved without the need for toxic preservatives. Thus bio-based wood modification is vital for enhancing wood properties sustainably, reducing environmental impact, and meeting the demand for eco-friendly, non-toxic, and renewable material solutions. In this study, bio-based formulae were used on pine sapwood for enhanced decay and weathering resistance. Quebracho tannin solutions (20 %) with different concentrations of citric acid (CA) as a cross-linker were prepared and then vacuum-pressure impregnated in Scots pine sapwood before curing them at 140 °C. The durability performance of untreated and tannin-impregnated wood samples was assessed against accelerated weathering, mould growth and brown rot decay fungus Coniophora puteana (Schumach.) P. Karst. Experimental results showed that the weathering resistance was apparently improved by tannin modification with higher levels of CA, as reflected by color stability, crack formation and contact angle. While tannin modification increased mould susceptibility, the decay resistance was notably enhanced in all modified wood samples. The acidity of the formulas at high CA levels may increase the risks of hydrolytic degradation of wood, and thus, low CA concentrations (e.g. 2 %) appear optimal for balancing performance and chemical stability. These findings underscore the potential of 100 % bio-based tannin–CA systems to enhance wood durability, offering a promising pathway for sustainable wood protection strategies.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Plant Pathogens and Fungal Diseases · Lignin and Wood Chemistry · Forest Insect Ecology and Management
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Forestry and Wood Technology, Faculty of Technology , Linnæus University , Georg Lückligs Plats 1 , Växjö 351 95 , Sweden
TESAF Department , Università degli Studi di Padova – University of Padua , Viale dell’Università 16, 35020 Legnaro (PD) , Veneto , Italy
College of Forest Resources and Environmental Science , Michigan Technological University , Houghton , MI 49931 , USA
Funding
VINNOVA · Stiftelsen för Kunskaps- och Kompetensutveckling
References (81)
Show source-provided references
1. Ahmed, S.A., Sehlstedt-Persson, M., and Morén, T. (2013a). Development of a new rapid method for mould testing in a climate chamber: preliminary tests. Eur. J. Wood Prod. 33: 174–187.
2. Ahmed, S.A., Yang, Q., Sehlstedt-Persson, M., and Morén, T. (2013b). Accelerated mold test on dried pine sapwood boards: impact of contact heat treatment. J. Wood Chem. Technol. 33: 174–187, https://doi.org/10.1080/02773813.2013.773041.10.1080/02773813.2013.773041 ↗
3. Ahmed, S.A., Tondi, G., Rizzo, F., Stöd, R.-M., and Hosseinpourpia, R. (2025). Dimensional stability of Scots pine sapwood modified by tannin-based formulas. In: Goli, G., Negro, F., Cuccui, I., Todaro, L., Jones, D., Militz, H., and Cetera, P. (Eds.). Proceedings of the 11th European conference on wood modification. Springer Nature, Florence, Italy.10.1007/978-3-031-99418-0_25 ↗
4. Arias, A., González-García, S., Feijoo, G., and Moreira, M.T. (2022). Tannin-based bio-adhesives for the wood panel industry as sustainable alternatives to petrochemical resins. J. Ind. Ecol. 26: 627–642.10.1111/jiec.13210 ↗
5. Bariska, M. and Pizzi, A. (1986). The interaction of polyflavonoid tannins with wood cellwalls. Holzforschung 40: 299–302, https://doi.org/10.1515/hfsg.1986.40.5.299.10.1515/hfsg.1986.40.5.299 ↗
6. Bernardis, A.C. and Popoff, O. (2009). Durability of Pinus elliottii wood impregnated with quebracho colorado (Schinopsis balansae) bio-protectives extracts and CCA. Maderas Cienc. Tecnol. 11: 107–115, https://doi.org/10.4067/s0718-221x2009000200002.10.4067/S0718-221X2009000200002 ↗
7. Bianchi, S., Kroslakova, I., Janzon, R., Mayer, I., Saake, B., and Pichelin, F. (2015). Characterization of condensed tannins and carbohydrates in hot water bark extracts of European softwood species. Phytochemistry 120: 53–61, https://doi.org/10.1016/j.phytochem.2015.10.006.10.1016/j.phytochem.2015.10.006 ↗
8. Brient, J.A., Manning, M.J., and Freeman, M.H. (2020). Copper naphthenate- protecting America’s infrastructure for over 100 years and its potential for expanded use in Canada and Europe. Wood Mater. Sci. Eng. 15: 368–376, https://doi.org/10.1080/17480272.2020.1837948.10.1080/17480272.2020.1837948 ↗
9. Broda, M. (2020). Natural compounds for wood protection against fungi: a review. Molecules 25: 3538, https://doi.org/10.3390/molecules25153538.10.3390/molecules25153538 ↗
10. Collet, O. (1992). Comparative tolerance of the brown-rot fungus Antrodia vaillantii (DC. Fr.) Ryv. isolates to copper. Holzforschung 46: 293–298, https://doi.org/10.1515/hfsg.1992.46.4.293.10.1515/hfsg.1992.46.4.293 ↗
11. Craciun, R., Maier, M., and Habicht, J. (2009). A theoretical-industrial correlation and perspective on copper-based wood preservatives. IRG/WP 09-30499. The International Research Group on Wood Preservation, Stockholm.
12. Dhawale, P.V., Vineeth, S.K., Gadhave, R.V., Fatima, M.J.J., Supekar, M.V., Thakur, V.K., and Raghavan, P. (2022). Tannin as a renewable raw material for adhesive applications: a review. Mater. Adv. 3: 3365–3388, https://doi.org/10.1039/d1ma00841b.10.1039/D1MA00841B ↗
13. Dirol, D. and Scalbert, A. (1991). Improvemet of wood decay resistance by tannin impregnation. IRG/WP2380. The International Research Group on Wood Preservation, Stockholm.
14. Essoua Essoua, G.G., Blanchet, P., Landry, V., and Beauregard, R. (2016). Pine wood treated with citric acid and glycerol mixture: biomaterial performance improved by a bio-product. Bioresources 11: 3049–3072, https://doi.org/10.15376/biores.11.2.3049-3072.10.15376/biores.11.2.3049-3072 ↗
15. Fengel, D. and Wegener, G. (1989). Wood chemistry, ultrastructure, reactions. Walter de Gruyter, New York (NY).
16. Freeman, M.H. and Mcintyre, C. (2008). Copper-based wood preservatives a comprehensive review of copper-based wood preservatives. For. Prod. J. 58: 6–27.
17. Ghavidel, A. and Hosseinpourpia, R. (2024). Photodegradation stability of huminated European pine (Pinus sylvestris L.) microveneers. Holzforschung 78: 283–292, https://doi.org/10.1515/hf-2024-0006.10.1515/hf-2024-0006 ↗
18. Ghavidel, A., Eceiza, A., Xie, X., and Hosseinpourpia, R. (2025). Humination modification: a green approach to improve the material properties of Scots pine (Pinus sylvestris L.) Sapwood. ACS Omega 10: 2996–3005, https://doi.org/10.1021/acsomega.4c09540.10.1021/acsomega.4c09540 ↗
19. Hadi, S., Hosseinihashemi, S.K., Latibari, A.J., and Salem, M.Z.M. (2016). Effects of acid copper chromate preservative and hydrothermal treatment on the dimensional stability, hardness, and decay resistance of poplar wood. Bioresources 11: 4850–4864, https://doi.org/10.15376/biores.11.2.4850-4864.10.15376/biores.11.2.4850-4864 ↗
20. Hart, J.H. and Hillis, W.E. (1972). Inhibition of wood-rotting fungi by ellagitannins in the heartwood of Quercus alba. Phytopathology 62: 620–626, https://doi.org/10.1094/phyto-62-620.10.1094/Phyto-62-620 ↗
21. Hill, C.A.S. (2006). Wood modification: chemical, thermal and other processes. Wiley Series in Renewable Resources. Wiley & Sons, Chichester, UK.10.1002/0470021748 ↗
22. Hosseinpourpia, R. and Mai, C. (2016a). Mode of action of brown rot decay resistance of acetylated wood: resistance to Fenton’s reagent. Wood Sci. Technol. 50: 413–426, https://doi.org/10.1007/s00226-015-0790-0.10.1007/s00226-015-0790-0 ↗
23. Hosseinpourpia, R. and Mai, C. (2016b). Mode of action of brown rot decay resistance in phenol-formaldehyde-modified wood: resistance to Fenton’s reagent. Holzforschung 70: 253–259, https://doi.org/10.1515/hf-2015-0045.10.1515/hf-2015-0045 ↗
24. Hosseinpourpia, R. and Mai, C. (2016c). Mode of action of brown rot decay resistance of thermally modified wood: resistance to Fenton’s reagent. Holzforschung 70: 691–697, https://doi.org/10.1515/hf-2015-0141.10.1515/hf-2015-0141 ↗
25. Huang, X., Kocaefe, D., Kocaefe, Y., Boluk, Y., and Krause, C. (2013). Structural analysis of heat-treated birch (Betule papyrifera) surface during artificial weathering. Appl. Surf. Sci. 264: 117–127, https://doi.org/10.1016/j.apsusc.2012.09.137.10.1016/j.apsusc.2012.09.137 ↗
26. Humar, M., Pohleven, F., and Žlindra, D. (2006). Influence of water properties on leaching of copper-based preservatives from treated wood. Wood Res. 51: 69–76.
27. Kalnins, M.A. and Feist, W.C. (1993). Increase in wettability of wood with weathering. For. Prod. J. 43: 55–57.
28. Kanbayashi, T., Kataoka, Y., Ishikawa, A., Matsunaga, M., Kobayashi, M., and Kiguchi, M. (2018). Confocal Raman microscopy reveals changes in chemical composition of wood surfaces exposed to artificial weathering. J. Photochem. Photobiol. B Biol. 187: 136–140, https://doi.org/10.1016/j.jphotobiol.2018.08.016.10.1016/j.jphotobiol.2018.08.016 ↗
29. Kartal, N., Terzi, E., Yilmaz, H., and Goodell, B. (2015). Bioremediation and decay of wood treated with ACQ, micronized ACQ, nano-CuO and CCA wood preservatives. Int. Biodeterior. Biodegrad. 99: 95–101.10.1016/j.ibiod.2015.01.004 ↗
30. Khanbabaee, K. and van Ree, T. (2001). Tannins: classification and definition. Nat. Prod. Rep. 18: 641–649, https://doi.org/10.1039/b101061l.10.1039/b101061l ↗
31. Khviyuzov, S., Gusakova, M., Bogolitsyn, K., and Volkov, A. (2021). Differences in the physicochemical properties of lignins in the heartwood and sapwood of Pinus sylvestris. J. Wood Chem. Technol. 41: 177–184, https://doi.org/10.1080/02773813.2021.1954951.10.1080/02773813.2021.1954951 ↗
32. Kishino, M. and Nakano, T. (2004). Artificial weathering of tropical woods. Part 1: changes in wettability. Holzforschung 58: 552–557, https://doi.org/10.1515/hf.2004.084.10.1515/HF.2004.084 ↗
33. Kránitz, K., Sonderegger, W., Bues, C.T., and Niemz, P. (2016). Effects of aging on wood: a literature review. Wood Sci. Technol. 50: 7–22, https://doi.org/10.1007/s00226-015-0766-0.10.1007/s00226-015-0766-0 ↗
34. Kurkowiak, K., Emmerich, L., and Militz, H. (2021). Sorption behavior and swelling of citric acid and sorbitol (SorCA) treated wood. Holzforschung 75: 1136–1149, https://doi.org/10.1515/hf-2021-0068.10.1515/hf-2021-0068 ↗
35. Kurkowiak, K., Emmerich, L., and Militz, H. (2023). Biological durability and wood-water interactions of sorbitol and citric acid (SorCA) modified wood. J. Wood Sci. 69: 34, https://doi.org/10.1186/s10086-023-02108-y.10.1186/s10086-023-02108-y ↗
36. Laks, P.E., McKaig, P.A., and Hemingway, R.W. (1988). Flavonoid biocides: wood preservatives based on condensed tannins. Holzforschung 42: 299–306, https://doi.org/10.1515/hfsg.1988.42.5.299.10.1515/hfsg.1988.42.5.299 ↗
37. Laskowska, A. (2018). Susceptibility of thermo-mechanically modified Scots pine (Pinus sylvestris L.) sapwood and heartwood to colour change under the influence of ultraviolet radiation. Drv. Ind. 69: 253–264, https://doi.org/10.5552/drind.2018.1756.10.5552/drind.2018.1756 ↗
38. Lee, K., Wi, S., Singh, A., and Kim, Y.S. (2004). Micromorphological characteristics of decayed wood and laccase produced by the brown-rot fungus Coniophora puteana. J. Wood Sci. 50: 281–284, https://doi.org/10.1007/s10086-003-0558-2.10.1007/s10086-003-0558-2 ↗
39. Lee, S.H., Md Tahir, P., Lum, W.C., Tan, L.P., Bawon, P., Park, B.-D., Osman Al Edrus, S.S., and Abdullah, U.H. (2020). A review on citric acid as green modifying agent and binder for wood. Polymers 12: 1692, https://doi.org/10.3390/polym12081692.10.3390/polym12081692 ↗
40. Li, J., Lei, H., Xi, X., li, C., Hou, D., Song, J., and Du, G. (2023). A sustainable tannin-citric acid wood adhesive with favorable bonding properties and water resistance. Ind. Crops Prod. 201: 116933, https://doi.org/10.1016/j.indcrop.2023.116933.10.1016/j.indcrop.2023.116933 ↗
41. Liao, J. and Mubarok, M. (2024). Revolutionizing wood: cutting-edge modifications, functional wood-based composites, and innovative applications. In: Zhou, X. (Ed.). Wood industry- impacts and benefits. IntechOpen, London.10.5772/intechopen.1007302 ↗
42. Lie, S.K., Vestøl, G.I., Høibø, O., and Gobakken, L.R. (2019). Surface mould growth on wood: a comparison of laboratory screening tests and outdoor performance. Eur. J. Wood Prod. 77: 1137–1150, https://doi.org/10.1007/s00107-019-01444-5.10.1007/s00107-019-01444-5 ↗
43. Lu, J., Venäläinen, M., Julkunen-Tiitto, R., and Harju, A. (2016). Stilbene impregnation retards brown-rot decay of Scots pine sapwood. Holzforschung 70: 261–266, https://doi.org/10.1515/hf-2014-0251.10.1515/hf-2014-0251 ↗
44. Martínez-Iñigo, M.J., Immerzeel, P., Gutierrez, A., del Río, J.C., and Sierra-Alvarez, R. (1999). Biodegradability of extractives in sapwood and heartwood from Scots pine by sapstain and white rot fungi. Holzforschung 53: 247–252, https://doi.org/10.1515/hf.1999.042.10.1515/HF.1999.042 ↗
45. Metsä-Kortelainen, S. and Viitanen, H. (2009). Decay resistance of sapwood and heartwood of untreated and thermally modified Scots pine and Norway spruce compared with some other wood species. Wood Mater. Sci. Eng. 4: 105–114, https://doi.org/10.1080/17480270903326140.10.1080/17480270903326140 ↗
46. Mubarok, M., Azadeh, E., Obounou Akong, F., Dumarçay, S., Gérardin, P., and Gérardin-Charbonnier, C. (2023). Effect of tannins addition on thermal stability of furfurylated wood. Polymers 15: 2044, https://doi.org/10.3390/polym15092044.10.3390/polym15092044 ↗
47. Navarrete, P., Mansouri, H.R., Pizzi, A., Tapin-Lingua, S., Benjelloun-Mlayah, B., Pasch, H., and Rigolet, S. (2010). Wood panel adhesives from low molecular mass lignin and tannin without synthetic resins. J. Adhes. Sci. Technol. 24: 1597–1610, https://doi.org/10.1163/016942410x500972.10.1163/016942410X500972 ↗
48. Okuda, T. (2005). Systematics and health effects of chemically distinct tannins in medicinal plants. Phytochemistry 66: 2012–2031, https://doi.org/10.1016/j.phytochem.2005.04.023.10.1016/j.phytochem.2005.04.023 ↗
49. Peng, Y., Wang, Y., Zhang, R., Wang, W., and Cao, J. (2021). Improvement of wood against UV weathering and decay by using plant origin substances: tannin acid and tung oil. Ind. Crops Prod. 168: 113606, https://doi.org/10.1016/j.indcrop.2021.113606.10.1016/j.indcrop.2021.113606 ↗
50. Rajput, H., Rajan, P., Li, S., Stratton, G.W., Murray, G., and He, Q. (2023). Development of wood preservatives to prevent biodeterioration. J. Wood Chem. Technol. 43: 371–389, https://doi.org/10.1080/02773813.2023.2284161.10.1080/02773813.2023.2284161 ↗
51. Rowell, R.M. (2005). Handbook of wood chemistry and wood composites. CRC Press, New York.10.1201/9780203492437 ↗
52. Ryparová, P. and Rácová, Z. (2024). Characteristics of mould growth in pine and spruce sapwood and heartwood under fluctuating humidity. Appl. Sci. 14: 8417, https://doi.org/10.3390/app14188417.10.3390/app14188417 ↗
53. Saranpää, P. and Höll, W. (1989). Soluble carbohydrates of Pinus sylvestris L. sapwood and heartwood. Trees 3: 138–143, https://doi.org/10.1007/bf00226648.10.1007/BF00226648 ↗
54. Schwarze, F.W.M.R., DeFloroio, G., and Fink, S. (2003). Resistance of parenchyma cells in wood to degradation by brown rot fungi. Mycol. Prog. 2: 267–274.10.1007/s11557-006-0064-1 ↗
55. Sehlstedt-Persson, M. and Wamming, T. (2010). Wood drying process: impact on Scots pine lumber durability. J. Wood Sci. 56: 25–32, https://doi.org/10.1007/s10086-009-1066-9.10.1007/s10086-009-1066-9 ↗
56. Sharma, K.P. (2019). Tannin degradation by phytopathogen’s tannase: a plant’s defense perspective. Biocatal. Agric. Biotechnol. 21: 101342, https://doi.org/10.1016/j.bcab.2019.101342.10.1016/j.bcab.2019.101342 ↗
57. Shi, J., Li, J., Zhou, W., and Zhang, D. (2007). Improvement of wood properties by urea-formaldehyde resin and nano-SiO2. Front. For. China 2: 104–109, https://doi.org/10.1007/s11461-007-0017-0.10.1007/s11461-007-0017-0 ↗
58. Sierra-Alvarez, R. (2009). Removal of copper, chromium and arsenic from preservative-treated wood by chemical extraction-fungal bioleaching. Waste Manag. 29: 1885–1891, https://doi.org/10.1016/j.wasman.2008.12.015.10.1016/j.wasman.2008.12.015 ↗
59. Soccol, C.R., Vandenberghe, L.P.S., Rodrigues, C., and Pandey, A. (2006). New perspectives for citric acid production and application. Food Technol. Biotechnol. 44: 141–149.
60. Sommerauer, L., Thevenon, M.F., Petutschnigg, A., and Tondi, G. (2019). Effect of hardening parameters of wood preservatives based on tannin copolymers. Holzforschung 73: 457–467, https://doi.org/10.1515/hf-2018-0130.10.1515/hf-2018-0130 ↗
61. SS-EN 113-1 (2020). Durability of wood and wood-based products – test method against wood destroying basidiomycetes – part 1: assessment of biocidal efficacy of wood preservatives. European Committee for Standardization, Brussels, Belgium.
62. SS-EN 927-6 (2006). Paints and varnishes – coating materials and coating systems for exterior wood – part 6: exposure of wood coatings to artificial weathering using fluorescent UV lamps and water. European Committee for Standardization, Brussels, Belgium.
63. Sun, S. and Zhao, Z. (2018). Influence of acid on the curing process of tannin-sucrose adhesives. Bioresources 13: 7683–7697, https://doi.org/10.15376/biores.13.4.7683-7697.10.15376/biores.13.4.7683-7697 ↗
64. Tascioglu, C., Yalcin, M., de Troya, T., and Sivrikaya, H. (2012). Termiticidal properties of some wood and bark extracts used as wood preservatives. Bioresources 7: 2960–2969, https://doi.org/10.15376/biores.7.3.2960-2969.10.15376/biores.7.3.2960-2969 ↗
65. Tascioglu, C., Yalcin, M., Sen, S., and Akcay, C. (2013). Antifungal properties of some plant extracts used as wood preservatives. Int. Biodeterior. Biodegrad. 85: 23–28, https://doi.org/10.1016/j.ibiod.2013.06.004.10.1016/j.ibiod.2013.06.004 ↗
66. Terziev, N., Boutelje, J., and Söderström, O. (1993). The influence of drying schedules on the redistribution of low-molecular sugars in Pinus sylvestris L. Holzforschung 47: 3–8, https://doi.org/10.1515/hfsg.1993.47.1.3.10.1515/hfsg.1993.47.1.3 ↗
67. Thaler, N., Lesan, B., and Humar, M. (2013). Performance of copper-ethanolamine-impregnated Scots pine wood during exposure to terrestrial microorganisms. Bioresources 8: 3299–3308, https://doi.org/10.15376/biores.8.3.3299-3308.10.15376/biores.8.3.3299-3308 ↗
68. Thévenon, M.F., Tondi, G., and Pizzi, A. (2009). High performance tannin resin-boron wood preservatives for outdoor end-uses. Eur. J. Wood Prod. 67: 89–93, https://doi.org/10.1007/s00107-008-0290-0.10.1007/s00107-008-0290-0 ↗
69. Thybring, E.E. (2013). The decay resistance of modified wood influenced by moisture exclusion and swelling reduction. Int. Biodeterior. Biodegrad. 82: 87–95, https://doi.org/10.1016/j.ibiod.2013.02.004.10.1016/j.ibiod.2013.02.004 ↗
70. Tomak, E.D. and Gonultas, O. (2018). The wood preservative potentials of valonia, chestnut, tara and sulphited oak tannins. J. Wood Chem. Technol. 38: 183–197, https://doi.org/10.1080/02773813.2017.1418379.10.1080/02773813.2017.1418379 ↗
71. Tondi, G., Palanti, S., Wieland, S., Thevenon, M.-F., Petutschnigg, A., and Schnabel, T. (2012). Durability of tannin-boron-treated timber. Bioresources 7: 5138–5151, https://doi.org/10.15376/biores.7.4.5138-5151.10.15376/biores.7.4.5138-5151 ↗
72. Tondi, G., Schnabel, T., Wieland, S., and Petutschnigg, A. (2013). Surface properties of tannin treated wood during natural and artificial weathering. Int. Wood Prod. J. 4: 150–157, https://doi.org/10.1179/2042645313y.0000000047.10.1179/2042645313Y.0000000047 ↗
73. Trosa, A. and Pizzi, A. (1998). Industrial hardboard and other panels binder from tannin/furfuryl alcohol in absence of formaldehyde. Holz Roh- Werkstoff 56: 213–214, https://doi.org/10.1007/s001070050301.10.1007/s001070050301 ↗
74. Venäläinena, M., Harjua, A.M., Kainulainenb, P., Viitanenc, H., and Nikulainenb, H. (2003). Variation in the decay resistance and its relationship with other wood characteristics in old Scots pines. Ann. For. Sci 60: 409–417, https://doi.org/10.1051/forest:2003033.10.1051/forest:2003033 ↗
75. Wang, J., Tan, W., Yang, H., Rao, X., Luo, X., Ma, L., Ren, C., Mol, A., and Zhang, D. (2023). Towards weathering and corrosion resistant, self-warning and self-healing epoxy coatings with tannic acid loaded nanocontainers. npj Mater. Degrad. 7: 39, https://doi.org/10.1038/s41529-023-00360-7.10.1038/s41529-023-00360-7 ↗
76. Xu, D., Li, C., Pizzi, A., Xi, X., Wang, Z., Du, G., Chen, Z., and Lei, H. (2024). Self-neutralizing citric acid−corn starch wood adhesives. ACS Sustain. Chem. Eng. 12: 13382–13391, https://doi.org/10.1021/acssuschemeng.4c05590.10.1021/acssuschemeng.4c05590 ↗
77. Yalcin, M. and Ceylan, H. (2017). The effects of tannins on adhesion strength and surface roughness of varnished wood after accelerated weathering. J. Coat. Technol. Res. 14: 185–193, https://doi.org/10.1007/s11998-016-9841-1.10.1007/s11998-016-9841-1 ↗
78. Yalcin, M., Pelit, H., Akcay, C., and Cakicier, N. (2017). Surface properties of tannin-impregnated and varnished beech wood after exposure to accelerated weathering. Color. Technol. 133: 334–340, https://doi.org/10.1111/cote.12287.10.1111/cote.12287 ↗
79. Zabel, R.A. and Morrell, J.J. (1992). Wood microbiology: decay and its prevention. Academic Press, London.
80. Zhang, B., Petrissans, M., Petrissans, A., Pizzi, A., and Colin, B. (2023). Furanic polymerization causes the change, conservation and recovery of thermally-treated wood hydrophobicity before and after moist conditions exposure. Polymers 15: 221, https://doi.org/10.3390/polym15010221.10.3390/polym15010221 ↗
81. Zhou, Y., Xu, D., Li, C., Pizzi, A., Du, G., and Lei, H. (2025). Self-neutralizing tannin-citric acid wood adhesives. Int. J. Biol. Macromol. 310: 143419, https://doi.org/10.1016/j.ijbiomac.2025.143419.10.1016/j.ijbiomac.2025.143419 ↗