journal article·2007-01-01

Syntheses and properties of liquefied products of ozone treated wood/epoxy resins having high wood contents

Toshiyuki Asano, Masahiko Kobayashi, Bunichiro Tomita, Mikio Kajiyama

Holzforschung· Volume 61· Issue 1
Publisher page

Abstract

Abstract Liquefied products with high wood content were prepared by pretreating wood with ozone before liquefaction. As a result, the ratio of wood to polyhydric alcohol (W/P ratio) used as solvent could be increased to 2:1. Resin blends were prepared by mixing liquefied products with ethylene glycol diglycidyl ether (EGDGE, water-soluble) and diglycidyl ether of bisphenol A (DGEBA, oily consistency). The wood content of the resin blend could be increased to 53%. The resins were cured by citric acid or triethylene tetramine (TETA), and their mechanical properties were evaluated. Dynamic mechanical measurements revealed that the former had higher glass transition temperatures than the latter. It was found that the resin with DGEBA cured by citric acid had almost the same level of tensile strength as commercial plastics.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Lignin and Wood Chemistry · Polymer composites and self-healing · Material Properties and Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. 10.1515/HF.2000.01410.1515/HF.2000.014 ↗
2. 10.1515/HF.2001.10810.1515/HF.2001.108 ↗
3. 10.1007/s10086-003-0596-910.1007/s10086-003-0596-9 ↗
4. 10.1007/s10086-004-0664-910.1007/s10086-004-0664-9 ↗
5. 10.1016/S0960-8524(00)00009-210.1016/S0960-8524(00)00009-2 ↗
6. 10.1016/S0960-8524(00)00136-X10.1016/S0960-8524(00)00136-X ↗
7. 10.1002/app.1995.07058081110.1002/app.1995.070580811 ↗
8. Shiraishi · Mokuzai Gakkaishi · 1986 · 32 · 755
9. 10.1016/S0960-8524(99)00008-510.1016/S0960-8524(99)00008-5 ↗
10. Yamada · J Adhes. Soc. Jpn. · 2001 · 37 · 47110.11618/adhesion.37.471 ↗
11. Yao · Mokuzai Gakkaishi · 1995 · 41 · 659