journal article·2019-11-01

Durability of Concrete Containing Liquid Crystal Display Glass Powder for Pavement

Authors not provided

ACI Materials Journal· Volume 116· Issue 6
Publisher page

Abstract

First Name is required invalid characters Last Name is required invalid characters Email Address is required Invalid Email Address Invalid Email Address
Only a short abstract or summary was supplied by the source.
Source: openalex_inverted_index · Quality: short

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. ASTM C618-12, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use,” ASTM International, West Conshohocken, PA, 2012, 3 pp.
2. Hall, M. L., and Livingston, W. R., “Fly Ash Quality, Past, Present and Future, and the Effect of Ash on the Development of Novel Products,” Journal of Chemical Technology and Biotechnology (Oxford, Oxfordshire), V. 77, No. 3, 2002, pp. 234-239. doi: 10.1002/jctb.53810.1002/jctb.538 ↗
3. Greenpeace, “Global Shift—Countries and Subnational Entities Phasing Out Existing Coal Power Plants and Shrinking the Proposed Coal Power Pipeline,” Report, Oct. 2017, 18 pp.
4. Bažant, Z. P.; Zi, G.; and Meyer, C., “Fracture Mechanics of ASR in Concretes with Waste Glass Particles of Different Sizes,” Journal of Engineering Mechanics, ASCE, V. 126, No. 3, 2000, pp. 226-232. doi: 10.1061/(ASCE)0733-9399(2000)126:3(226)10.1061/(ASCE)0733-9399(2000)126:3(226) ↗
5. You, I.; Choi, J.; Lange, D. A.; and Zi, G., “Pozzolanic Reaction of the Waste Glass Sludge Incorporating Precipitation Additives,” Computers and Concrete, V. 17, No. 2, 2016, pp. 255-269. doi: 10.12989/cac.2016.17.2.25510.12989/cac.2016.17.2.255 ↗
6. Shi, C.; Wu, Y.; Riefler, C.; and Wang, H., “Characteristics and Pozzolanic Reactivity of Glass Powders,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 987-993. doi: 10.1016/j.cemconres.2004.05.01510.1016/j.cemconres.2004.05.015 ↗
7. Du, H., and Tan, K. H., “Transport Properties of Concrete with Glass Powder as Supplementary Cementitious Material,” ACI Materials Journal, V. 112, No. 3, May-June 2015, pp. 429-437. doi: 10.14359/5168736310.14359/51687363 ↗
8. Du, H., and Tan, K. H., “Properties of High Volume Glass Powder Concrete,” Cement and Concrete Composites, V. 75, 2017, pp. 22-29. doi: 10.1016/j.cemconcomp.2016.10.01010.1016/j.cemconcomp.2016.10.010 ↗
9. Kim, J.; Yi, C.; and Zi, G., “Waste Glass Sludge as a Partial Cement Replacement in Mortar,” Construction and Building Materials, V. 75, 2015, pp. 242-246. doi: 10.1016/j.conbuildmat.2014.11.00710.1016/j.conbuildmat.2014.11.007 ↗
10. Kim, J.; Moon, J. H.; Shim, J. W.; Sim, J.; Lee, H. G.; and Zi, G., “Durability Properties of a Concrete with Waste Glass Sludge Exposed to Freeze-and-Thaw Condition and De-Icing Salt,” Construction and Building Materials, V. 66, 2014, pp. 398-402. doi: 10.1016/j.conbuildmat.2014.05.08110.1016/j.conbuildmat.2014.05.081 ↗
11. Maraghechi, H.; Maraghechi, M.; Rajabipour, F.; and Pantano, C. G., “Pozzolanic Reactivity of Recycled Glass Powder at Elevated Temperatures: Reaction Stoichiometry, Reaction Products and Effect of Alkali Activation,” Cement and Concrete Composites, V. 53, 2014, pp. 105-114. doi: 10.1016/j.cemconcomp.2014.06.01510.1016/j.cemconcomp.2014.06.015 ↗
12. Shao, Y.; Lefort, T.; Moras, S.; and Rodriguez, D., “Studies on Concrete Containing Ground Waste Glass,” Cement and Concrete Research, V. 30, No. 1, 2000, pp. 91-100. doi: 10.1016/S0008-8846(99)00213-610.1016/S0008-8846(99)00213-6 ↗
13. Idir, R.; Cyr, M.; and Tagnit-Hamou, A., “Pozzolanic Properties of Fine and Coarse Color-Mixed Glass Cullet,” Cement and Concrete Composites, V. 33, No. 1, 2011, pp. 19-29. doi: 10.1016/j.cemconcomp.2010.09.01310.1016/j.cemconcomp.2010.09.013 ↗
14. Maraghechi, H., “Development and Assessment of Alkali Activated Recycled Glass-Based Concretes for Civil Infrastructure,” PhD dissertation, Pennsylvania State University, University Park, PA, 2014.
15. Polley, C.; Cramer, S. M.; and Cruz, R. V., “Potential for Using Waste Glass in Portland Cement Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 10, No. 4, 1998, pp. 210-219. doi: 10.1061/(ASCE)0899-1561(1998)10:4(210)10.1061/(ASCE)0899-1561(1998)10:4(210) ↗
16. Electronics360 News Desk, “Samsung, LG, Sony to Dominate Flat Panel Shipments in 2015,” https://electronics360.globalspec.com/article/5067/samsung-lg-sony-to-dominate-flat-panel-shipments-in-2015. (last accessed Nov. 19, 2019)
17. Kim, K., and Kim, K., “Valuable Recycling of Waste Glass Generated from the Liquid Crystal Display Panel Industry,” Journal of Cleaner Production, V. 174, 2018, pp. 191-198. doi: 10.1016/j.jclepro.2017.10.32610.1016/j.jclepro.2017.10.326 ↗
18. Fan, C. S., and Li, K. C., “Production of Insulating Glass Ceramics from Thin Film Transistor-Liquid Crystal Display (TFT-LCD) Waste Glass and Calcium Fluoride Sludge,” Journal of Cleaner Production, V. 57, 2013, pp. 335-341. doi: 10.1016/j.jclepro.2013.06.00210.1016/j.jclepro.2013.06.002 ↗
19. Lin, K. L., “Use of Thin Film Transistor Liquid Crystal Display (TFT-LCD) Waste Glass in the Production of Ceramic Tiles,” Journal of Hazardous Materials, V. 148, No. 1-2, 2007, pp. 91-97. doi: 10.1016/j.jhazmat.2007.02.00410.1016/j.jhazmat.2007.02.004 ↗
20. Lin, K. L.; Wang, N. F.; Shie, J. L.; Lee, T. C.; and Lee, C., “Elucidating the Hydration Properties of Paste Containing Thin Film Transistor Liquid Crystal Display Waste Glass,” Journal of Hazardous Materials, V. 159, No. 2-3, 2008, pp. 471-475. doi: 10.1016/j.jhazmat.2008.02.04410.1016/j.jhazmat.2008.02.044 ↗
21. Lin, K. L.; Huang, W. J.; Shie, J. L.; Lee, T. C.; Wang, K. S.; and Lee, C. H., “The Utilization of Thin Film Transistor Liquid Crystal Display Waste Glass as a Pozzolanic Material,” Journal of Hazardous Materials, V. 163, No. 2-3, 2009, pp. 916-921. doi: 10.1016/j.jhazmat.2008.07.04410.1016/j.jhazmat.2008.07.044 ↗
22. Kim, K.; Kim, K.; and Hwang, J., “LCD Waste Glass as a Substitute for Feldspar in the Porcelain Sanitary Ware Production,” Ceramics International, V. 41, No. 5, 2015, pp. 7097-7102. doi: 10.1016/j.ceramint.2015.02.01810.1016/j.ceramint.2015.02.018 ↗
23. Lee, C. T., “Production of Alumino-Borosilicate Foamed Glass Body from Waste LCD Glass,” Journal of Industrial and Engineering Chemistry, V. 19, No. 6, 2013, pp. 1916-1925. doi: 10.1016/j.jiec.2013.02.03810.1016/j.jiec.2013.02.038 ↗
24. Jang, H.; Jeon, S.; So, H.; and So, S., “A Study of the Possibility of Using TFT-LCD Waste Glass as an Admixture for Steam-Cured PHC Piles,” Magazine of Concrete Research, V. 66, No. 4, 2014, pp. 196-208. doi: 10.1680/macr.13.0025410.1680/macr.13.00254 ↗
25. Wang, H. Y.; Zeng, H. H.; and Wu, J. Y., “A Study of the Possibility of Using TFT-LCD Waste Glass as an Admixture for Steam-Cured PHC Piles,” Construction and Building Materials, V. 66, No. 4, Feb. 2014, pp. 196-208.10.1680/macr.13.00254 ↗
26. Brouwers, H. J. H., “Packing Fraction of Geometric Random Packings of Discretely Sized Particles,” Physical Review E: Statistical, Nonlinear, and Soft Matter Physics, V. 84, No. 4, 2011, pp. 1-14. doi: 10.1103/PhysRevE.84.04230110.1103/PhysRevE.84.042301 ↗
27. Hüsken, G., “A Multifunctional Design Approach for Sustainable Concrete with Application to Concrete Mass Products,” PhD dissertation, Eindhoven University of Technology, Eindhoven, the Netherlands, 2010.
28. Koutný, O.; Kratochvíl, J.; Švec, J.; and Bednárek, J., “Modelling of Packing Density for Particle Composites Design,” Procedia Engineering, V. 151, 2016, pp. 198-205. doi: 10.1016/j.proeng.2016.07.38610.1016/j.proeng.2016.07.386 ↗
29. Nimmo, J. R., “Porosity and Pore Size Distribution,” Encyclopedia of Soils in the Environment, 2004, pp. 295-303. doi:10.1016/B978-0-12-409548-9.05265-910.1016/B978-0-12-409548-9.05265-910.1016/B0-12-348530-4/00404-5 ↗
30. ASTM C311-11b, “Standard Test Methods for sampling and Testing Fly Ash or Natural Pozzolans for Use in Portland Cement Concrete,” ASTM International, West Conshohocken, PA, 2011, 10 pp.
31. ASTM C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018, 8 pp.
32. ASTM C78-16, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2016, 5 pp.
33. ASTM C779M-12, “Standard Test Method for Abrasion Resistance of Horizontal Concrete Surfaces,” ASTM International, West Conshohocken, PA, 2012, 7 pp.
34. ASTM C1260-07, “Standard Test Method for Potential Alkali Reactivity of Cement-Aggregate Combinations (Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2007, 6 pp.
35. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 9 pp.
36. ASTM C666M-15, “Standard Test Method for Resistance of Concrete to Rapid Freezing and Thawing,” ASTM International, West Conshohocken, PA, 2015, 7 pp.
37. Ishida, T.; Miyahara, S.; and Maruya, T., “Chloride Binding Capacity of Mortars Made with Various Portland Cements and Mineral Admixtures,” Journal of Advanced Concrete Technology, V. 6, No. 2, 2008, pp. 287-301. doi: 10.3151/jact.6.28710.3151/jact.6.287 ↗
38. Jain, J. A., and Neithalath, N., “Chloride Transport in Fly Ash and Glass Powder Modified Concretes—Influence of Test Methods on Microstructure,” Cement and Concrete Composites, V. 32, No. 2, 2010, pp. 148-156. doi: 10.1016/j.cemconcomp.2009.11.01010.1016/j.cemconcomp.2009.11.010 ↗
39. Shi, Z.; Geiker, M. R.; De Weerdt, K.; Østnor, T. A.; Lothenbach, B.; Winnefeld, F.; and Skibsted, J., “Role of Calcium on Chloride Binding in Hydrated Portland Cement–Metakaolin–Limestone Blends,” Cement and Concrete Research, V. 95, 2017, pp. 205-216. doi: 10.1016/j.cemconres.2017.02.00310.1016/j.cemconres.2017.02.003 ↗
40. Thomas, M. D. A.; Hooton, R. D.; Scott, A.; and Zibara, H., “The Effect of Supplementary Cementitious Materials on Chloride Binding in Hardened Cement Paste,” Cement and Concrete Research, V. 42, No. 1, 2012, pp. 1-7. doi: 10.1016/j.cemconres.2011.01.00110.1016/j.cemconres.2011.01.001 ↗
41. ASTM C150M-17, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2017, 9 pp.
42. Metha, P., and Monteiro, P. J., Concrete: Microstructure, Properties, and Materials, third edition, Prentice Hall, Englewood Cliffs, NJ, 1994, 659 pp.
43. Khmiri, A.; Chaabouni, M.; and Samet, B., “Chemical Behaviour of Ground Waste Glass When Used as Partial Cement Replacement in Mortars,” Construction and Building Materials, V. 44, 2013, pp. 74-80. doi: 10.1016/j.conbuildmat.2013.02.04010.1016/j.conbuildmat.2013.02.040 ↗
44. Schwarz, N., and Neithalath, N., “Influence of a Fine Glass Powder on Cement Hydration: Comparison to Fly Ash and Modeling the Degree of Hydration,” Cement and Concrete Research, V. 38, No. 4, 2008, pp. 429-436. doi: 10.1016/j.cemconres.2007.12.00110.1016/j.cemconres.2007.12.001 ↗
45. Korea Expressway Corporation, “Expressway Construction Guide Specification,” V. 2012, Gimcheon, Korea, 2012.
46. Matos, A. M., and Sousa-Coutinho, J., “Durability of Mortar Using Waste Glass Powder as Cement Replacement,” Construction and Building Materials, V. 36, 2012, pp. 205-215. doi: 10.1016/j.conbuildmat.2012.04.02710.1016/j.conbuildmat.2012.04.027 ↗
47. Matos, A. M., and Sousa Coutinho, J., “Waste Glass Powder in Cement: Macro and Micro Scale Study,” Advances in Cement Research, V. 28, No. 7, 2016, pp. 423-432. doi: 10.1680/jadcr.14.0002510.1680/jadcr.14.00025 ↗
48. Nassar, R. U. D., and Soroushian, P., “Strength and Durability of Recycled Aggregate Concrete Containing Milled Glass as Partial Replacement for Cement,” Construction and Building Materials, V. 29, 2012, pp. 368-377. doi: 10.1016/j.conbuildmat.2011.10.06110.1016/j.conbuildmat.2011.10.061 ↗
49. Serpa, D.; Santos Silva, A.; De Brito, J.; Pontes, J.; and Soares, D., “ASR of Mortars Containing Glass,” Construction and Building Materials, V. 47, 2013, pp. 489-495. doi: 10.1016/j.conbuildmat.2013.05.05810.1016/j.conbuildmat.2013.05.058 ↗
50. Shayan, A., and Xu, A., “Performance of Glass Powder as a Pozzolanic Material in Concrete: A Field Trial on Concrete Slabs,” Cement and Concrete Research, V. 36, No. 3, 2006, pp. 457-468. doi: 10.1016/j.cemconres.2005.12.01210.1016/j.cemconres.2005.12.012 ↗
51. Shayan, A., and Xu, A., “Value-Added Utilisation of Waste Glass in Concrete,” Cement and Concrete Research, V. 34, No. 1, 2004, pp. 81-89. doi: 10.1016/S0008-8846(03)00251-510.1016/S0008-8846(03)00251-5 ↗
52. Schwarz, N.; Cam, H.; and Neithalath, N., “Influence of a Fine Glass Powder on the Durability Characteristics of Concrete and Its Comparison to Fly Ash,” Cement and Concrete Composites, V. 30, No. 6, 2008, pp. 486-496. doi: 10.1016/j.cemconcomp.2008.02.00110.1016/j.cemconcomp.2008.02.001 ↗
53. Zhu, X.; Zi, G.; Cao, Z.; and Cheng, X., “Combined Effect of Carbonation and Chloride Ingress in Concrete,” Construction and Building Materials, V. 110, 2016, pp. 369-380. doi: 10.1016/j.conbuildmat.2016.02.03410.1016/j.conbuildmat.2016.02.034 ↗