journal article·2021-06-25Open access

In-situ penetration of ionic liquids during surface densification of Scots pine

Benedikt Neyses, Kelly Peeters, Dietrich Buck, Lauri Rautkari, Dick Sandberg

Holzforschung· Volume 75· Issue 6

Abstract

Abstract The moisture-induced recovery of compressed wood is one of the major problems of wood densification technology. Achieving a cost-efficient surface densification process without the need for additional resins to eliminate the set-recovery may lead to an increase in value of low-density wood species. A previous study has shown that a pre-treatment with ionic liquids (ILs) can nearly eliminate the set-recovery. It was however observed that during the pre-treatment process the IL did not penetrate sufficiently deep into the wood to explain the achieved reduction in set-recovery. Based on these findings, the hypothesis was posed that further penetration of the IL into the wood occurs during the densification stage as a consequence of the applied heat and pressure. Thermo-gravimetric analysis (TGA) and gas-chromatography mass-selective-detection (GC-MSD) showed that the depth of penetration of the IL was greater after the densification process than before. Digital image correlation (DIC) showed that in regions with a high IL concentration, there was almost no set-recovery, and it gradually increased with a decrease in the IL concentration, as observed with TGA and GC-MSD analysis.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Advanced Cellulose Research Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Luleå University of Technology , Forskargatan 1, SE-93187 , Skellefteå , Sweden

InnoRenew CoE , Livade 6, SI-6310, Izola , Slovenia

Aalto University , P.O. Box 16300, 00076 , Aalto , Finland

References (32)

Show source-provided references
1. Efimova, A., Hubrig, G., and Schmidt, P. (2013). Thermal stability and crystallization behavior of imidazolium halide ionic liquids. Thermochim. Acta 573: 162–169. https://doi.org/10.1016/j.tca.2013.09.023.10.1016/j.tca.2013.09.023 ↗
2. Gabrielli, C.P., and Kamke, F A. (2010). Phenol–formaldehyde impregnation of densified wood for improved dimensional stability. Wood Sci. Technol. 44: 95–104. https://doi.org/10.1007/s00226-009-0253-6.10.1007/s00226-009-0253-6 ↗
3. Gong, M., Lamason, C., and Li, L. (2010). Interactive effect of surface densification and post-heat-treatment on aspen wood. J. Mater. Process. Technol. 210: 293–296. https://doi.org/10.1016/j.jmatprotec.2009.09.013.10.1016/j.jmatprotec.2009.09.013 ↗
4. Hanabusa, H., Izgorodina, E.I., Suzuki, S., Takeoka, Y., Rikukawa, M., and Yoshizawa-Fujita, M. (2018). Cellulose-dissolving protic ionic liquids as low cost catalysts for direct transesterification reactions of cellulose. Green Chem. 20: 1412–1422. https://doi.org/10.1039/c7gc03603e.10.1039/C7GC03603E ↗
5. Inoue, M., Norimoto, M., Otsuka, Y., Yamada, T., Tanahashi, M., and Rowell, R.M. (1993). Steam or heat fixation of compressed wood. Wood Fiber Sci. 25: 224–235.
6. Khalil, H.A., Dungani, R., Mohammed, I.A., Hossain, M.S., Aprilia, N.S., Budiarso, E., and Rosamah, E. (2014). Determination of the combined effect of chemical modification and compression of agatis wood on the dimensional stability, termite resistance, and morphological structure. BioResources 9: 6614–6626. https://doi.org/10.15376/biores.9.4.6614-6626.10.15376/biores.9.4.6614-6626 ↗
7. Kilpeläinen, I., Xie, H., King, A., Granstrom, M., Heikkinen, S., and Argyropoulos, D.S. (2007). Dissolution of wood in ionic liquids. J. Agric. Food Chem. 55: 9142–9148. https://doi.org/10.1021/jf071692e.10.1021/jf071692e ↗
8. Kutnar, A., and Kamke, F.A. (2012a). Compression of wood under saturated steam, superheated steam, and transient conditions at 150°C, 160°C, and 170°C. Wood Sci. Technol. 46: 73–88. https://doi.org/10.1007/s00226-010-0380-0.10.1007/s00226-010-0380-0 ↗
9. Kutnar, A., and Kamke, F.A. (2012b). Influence of temperature and steam environment on set recovery of compressive deformation of wood. Wood Sci. Technol. 46: 953–964. https://doi.org/10.1007/s00226-011-0456-5.10.1007/s00226-011-0456-5 ↗
10. Lamason, C., and Gong, M. (2007). Optimization of pressing parameters for mechanically surface-densified aspen. For. Prod. J. 57: 64.
11. Laine, K., Rautkari, L., Hughes, M., and Kutnar, A. (2013). Reducing the set-recovery of surface densified solid Scots pine wood by hydrothermal post-treatment. Eur. J. Wood Wood Prod. 71: 17–23. https://doi.org/10.1007/s00107-012-0647-2.10.1007/s00107-012-0647-2 ↗
12. LePage, W.S., Daly, S.H., and Shaw, J.A. (2016). Cross polarization for improved digital image correlation. Exp. Mech. 56: 969–985. https://doi.org/10.1007/s11340-016-0129-2.10.1007/s11340-016-0129-2 ↗
13. Navi, P. and Girardet, F. (2000). Effects of thermo-hydro-mechanical treatment on the structure and properties of wood. Holzforschung 54: 287–293. https://doi.org/10.1515/hf.2000.048.10.1515/HF.2000.048 ↗
14. Navi, P. and Heger, F. (2004). Combined densification and thermo-hydro-mechanical processing of wood. Mat. Res. Soc. Bulletin 29: 332–336. https://doi.org/10.1557/mrs2004.100.10.1557/mrs2004.100 ↗
15. Navi, P. and Sandberg, D. (2012). Thermo-hydro-mechanical processing of wood. EPFL Press, Lausanne.10.1201/b10143 ↗
16. Navi, P., and Pizzi, A. (2014). Property changes in thermo-hydro-mechanical processing. Holzforschung 69: 863–873, https://doi.org/10.1515/hf-2014-0198.10.1515/hf-2014-0198 ↗
17. Neyses, B., Rautkari, L., Yamamoto, A., and Sandberg, D. (2017). Pre-treatment with sodium silicate, sodium hydroxide, ionic liquids or methacrylate resin to reduce the set-recovery and increase the hardness of surface-densified Scots pine. Iforest 10: 857–864. https://doi.org/10.3832/ifor2385-010.10.3832/ifor2385-010 ↗
18. Neyses, B., Karlsson, O., and Sandberg, D. (2020). The effect of ionic liquid and superbase pre-treatment on the spring-back, set-recovery and Brinell hardness of surface-densified Scots pine. Holzforschung 74: 303–312. https://doi.org/10.1515/hf-2019-0158.10.1515/hf-2019-0158 ↗
19. Ngo, H.L., LeCompte, K., Hargens, L., and McEwen, A.B. (2000). Thermal properties of imidazolium ionic liquids. Thermochim. Acta 357: 97–102. https://doi.org/10.1016/s0040-6031(00)00373-7.10.1016/S0040-6031(00)00373-7 ↗
20. Ohtani, H., Ishimura, S., and Kumai, M. (2008). Thermal decomposition behaviors of imidazolium-type ionic liquids studied by pyrolysis-gas chromatography. Anal. Sci. 24: 1335–1340. https://doi.org/10.2116/analsci.24.1335.10.2116/analsci.24.1335 ↗
21. Parviainen, A.P. (2016). Acid-base conjugate ionic liquids in lignocellulose processing: synthesis, properties and applications. Laboratory of Organic Chemistry, Department of Chemistry, Faculty of Science, University of Helsinki, Finland.
22. Pfriem, A., Dietrich, T., and Buchelt, B. (2012). Furfuryl alcohol impregnation for improved plasticization and fixation during the densification of wood. Holzforschung 66: 215–218. https://doi.org/10.1515/hf.2011.134.10.1515/HF.2011.134 ↗
23. Pizzi, A., Leban, J.M., Zanetti, M., Pichelin, F., Wieland, S., and Properzi, M. (2005). Surface finishes by mechanically induced wood surface fusion. Holz Roh Werkst 63: 251–255. https://doi.org/10.1007/s00107-004-0569-8.10.1007/s00107-004-0569-8 ↗
24. Rautkari, L., Properzi, M., Pichelin, F., and Hughes, M. (2009). Surface modification of wood using friction. Wood Sci. Technol. 43: 291–299. https://doi.org/10.1007/s00226-008-0227-0.10.1007/s00226-008-0227-0 ↗
25. Rautkari, L., Laine, K., Laflin, N., and Hughes, M. (2011). Surface modification of Scots pine: the effect of process parameters on the through thickness density profile. J. Mater. Sci. 46: 4780–4786. https://doi.org/10.1007/s10853-011-5388-9.10.1007/s10853-011-5388-9 ↗
26. Rautkari, L., Laine, K., Kutnar, A., Medved, S., and Hughes, M. (2013). Hardness and density profile of surface densified and thermally modified Scots pine in relation to degree of densification. J. Mater. Sci. 48: 2370–2375. https://doi.org/10.1007/s10853-012-7019-5.10.1007/s10853-012-7019-5 ↗
27. Rieland, J.M., and Love, B.J. (2020). Ionic liquids: a milestone on the pathway to greener recycling of cellulose from biomass. Resour. Conserv. Recycl. 155: 104678. https://doi.org/10.1016/j.resconrec.2019.104678.10.1016/j.resconrec.2019.104678 ↗
28. Stamm, A.J. (1964). Wood and cellulose science. The Ronald Press Company, New York.
29. Sutton, M.A., Orteu, J., and Schreier, H.W. (2009). Image correlation for shape, motion and deformation measurements: basic concepts, theory and applications. Springer Science+Business Media, New York.
30. Swatloski, R.P., Spear, S.K., Holbrey, J.D., and Rogers, R.D. (2002). Dissolution of cellulose with ionic liquids. J. Am. Chem. Soc. 124: 4974–4975. https://doi.org/10.1021/ja025790m.10.1021/ja025790m ↗
31. Tanaka, A., Khakalo, A., Hauru, L., Korpela, A., and Orelma, H. (2018). Conversion of paper to film by ionic liquids: manufacturing process and properties. Cellulose 25: 6107–6119. https://doi.org/10.1007/s10570-018-1944-7.10.1007/s10570-018-1944-7 ↗
32. Thuvander, F., Sjödahl, M., and Berglund, L.A. (2000). Measurements of crack tip strain field in wood at the scale of growth rings. J. Mater. Sci. 35: 6267–6275https://doi.org/10.1023/a:1026722521248.10.1023/A:1026722521248 ↗