article·2004-07-07

Shrinkage stress of wood during drying under superheated steam above 100°C

Wood-Hi Cheng, T. Morooka, Liu Y, Misato Norimoto

Publisher page

Abstract

Abstract In order to reduce the internal stress of wood during drying, an attempt was made to dry wood with superheated steam above 100°C. Sugi ( Cryptomeria japonica D. Don) wood specimens were dried with radial restraint using superheated steam at up to 180°C, and the resulting restrained shrinkage stress was examined. A load cell capable of measuring shrinkage stress inside an autoclave was developed and the shrinkage stress was measured at temperatures from 80 to 180°C and a relative humidity of 0% to 80%. It was found that the shrinkage stress decreased dramatically with drying above 140°C and above 60% relative humidity. It was also found that the shrinkage stress above 140°C occurred even at 100% RH and was ascribed to the structural change in cell-wall components.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.