journal article·2018-08-18

A simple recoating repair methodology to improve oxidation resistance of C/SiCs

Hui Mei, Ding Zhang, Junchao Xia, Laifei Cheng

Advances in Applied Ceramics· Volume 117· Issue 6
Publisher page

Abstract

Lots of through SiC coating micro-cracks appeared due to the mismatch of thermal expansion coefficient between fibres and matrix, and this could be the diffusion path for oxidising gases to reduce oxidation resistance of as-cracked C/SiCs. In this paper, a simple recoating repair methodology was achieved by grinding off original coating and depositing coating again. The experimental results pointed out that as-repaired specimens had excellent oxidation resistance with the whole temperature range of 500–1500°C, and at sensitive point of 800°C, the weight loss rate of the as-repaired specimens was decreased by 22.1% compared to the as-cracked specimens. From 700 to 1100°C, the flexural strength of the as-repaired specimens has obviously improved compared to the as-cracked specimens. Microstructural analysis showed that the recoating repair methodology can seal and narrow through-coating micro-cracks, leading to oxidation resistance and mechanical properties improvement for the as-repaired specimens.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Science and Technology on Thermostructural Composite Materials Laboratory, Northwestern Polytechnical University, Xi’an, Shaanxi, People’s Republic of China

Funding

National Natural Science Foundation of China · Program for New Century Excellent Talents in University · Foreign Talents Introduction and Academic Exchange Program of China · Major project of Science and Technology of Jilin Institute of Chemical Technology · Central Universities · Northwestern Polytechnical University

References (16)

Show source-provided references
1. 10.1016/S0266-3538(03)00230-610.1016/S0266-3538(03)00230-6 ↗
2. 10.1016/j.msea.2007.02.03710.1016/j.msea.2007.02.037 ↗
3. 10.1016/j.matlet.2012.05.03010.1016/j.matlet.2012.05.030 ↗
4. Yin X · Int Mater Rev · 2014 · 59 · 32610.1179/1743280414Y.0000000037 ↗
5. 10.1016/j.carbon.2015.08.01110.1016/j.carbon.2015.08.011 ↗
6. 10.1023/B:JMSC.0000048745.18938.d510.1023/B:JMSC.0000048745.18938.d5 ↗
7. 10.1023/A:100474101418510.1023/A:1004741014185 ↗
8. 10.1016/0955-2219(94)90105-810.1016/0955-2219(94)90105-8 ↗
9. 10.1016/0008-6223(93)90086-P10.1016/0008-6223(93)90086-P ↗
10. 10.1016/S0008-6223(00)00068-310.1016/S0008-6223(00)00068-3 ↗
11. 10.1016/S0921-5093(00)01405-210.1016/S0921-5093(00)01405-2 ↗
12. Zhang CR · J Effects of Deposition temperature on the microstructures of SiC coatings by CVD[J]. In Mater · 2007
13. 10.1016/S1359-835X(00)00045-210.1016/S1359-835X(00)00045-2 ↗
14. 10.1016/j.msea.2015.02.03610.1016/j.msea.2015.02.036 ↗
15. 10.1111/j.1551-2916.2007.02170.x10.1111/j.1551-2916.2007.02170.x ↗
16. 10.1080/15685543.2012.76273010.1080/15685543.2012.762730 ↗