journal article·2020-01-02

Strengthening of 2D-C/SiC composite through creep with low stress and high temperature

Meng Li, Chengyu Zhang, Kejie Wang, Xiao Zhang, Xi Wang, Dong Han, Mei Li

Advances in Applied Ceramics· Volume 119· Issue 1
Publisher page

Abstract

To improve the resistance to matrix cracking of 2D-C/SiC composite, the composite was treated at certain creep conditions, which involve relative lower stress, higher temperature. The creep strain and matrix cracking stress (σmc) were used to determine the creep strengthening effect. Moreover, the stress redistribution model was applied to explain the stress transfer from the matrix to fibre, and therefore the creep strengthening mechanisms. The results indicate that 2D-C/SiC can be strengthened by creep at certain conditions. The ability to resist the creep strain and σmc can be improved by certain creep treatments with creep temperature of 1400°C, lower stress and longer time. The strengthening effect is resulted from the stress redistribution during the creep. The tensile residual stress is relaxed in the matrix and transferred to the fibre. The stress redistribution leads to compressive stress in the matrix and takes the advantage of superior creep resistance of carbon fibres.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Science and Technology on Thermostructural Composite Materials Laboratory, Northwestern Polytechnical University, Xi’an, People’s Republic of China

NPU-SAS Joint Research Center, Northwestern Polytechnical University, Xi’an, People’s Republic of China

References (17)

Show source-provided references
1. Zhang LT · Acta Materiae Compositae Sinica · 2007 · 24 · 1
2. Zhang LT · Aeronaut Manufact Technol · 2003 · 1 · 24
3. Naslain R. · Compos Sci Technol · 2004 · 64 · 15510.1016/S0266-3538(03)00230-6 ↗
4. Boitier G · Mater Sci Eng A · 2000 · 289 · 26510.1016/S0921-5093(00)00922-9 ↗
5. 10.1111/j.1744-7402.2009.02422.x10.1111/j.1744-7402.2009.02422.x ↗
6. Hinoki T · Sci Rep RITU · 1997 · 45 · 133
7. Morscher GN · Compos Sci Technol · 2008 · 68 · 330510.1016/j.compscitech.2008.08.028 ↗
8. Widjaja S · J Am Ceram Soc · 1999 · 82 · 65710.1111/j.1151-2916.1999.tb01814.x ↗
9. Richard W. · 2000
10. 10.1007/BF0114472310.1007/BF01144723 ↗
11. Morscher GN · Compos Sci Technol · 2007 · 67 · 100910.1016/j.compscitech.2006.06.007 ↗
12. Jiang YQ · 1995 · 665
13. Boitier G · Mater Sci Eng A · 2000 · 279 · 7310.1016/S0921-5093(99)00626-7 ↗
14. Boitier G · Mater Sci Eng A · 2001 · 313 · 5310.1016/S0921-5093(01)01137-6 ↗
15. Boitier G · J Eur Ceram Soc · 1998 · 18 · 183510.1016/S0955-2219(98)00123-X ↗
16. Morscher GN · J Am Ceram Soc · 2006 · 89 · 165210.1111/j.1551-2916.2006.00939.x ↗
17. Kumaria S · Acta Mater · 1997 · 45 · 517710.1016/S1359-6454(97)00177-8 ↗