Analysis of the Long-Term Performance Degradation of Crystalline Silicon Photovoltaic Modules in Tropical Climates
Source abstract
Abstract
The long-term performance degradation of five different types of commercial crystalline silicon (c-Si) photovoltaic (PV) modules (one sample for each type) in the tropics, or more specifically the tropical rainforest climate “Af” by the Köppen climate classification (Singapore), is investigated over a period of seven years, based on outdoor I-V measurements at 10-s intervals. The degradation rates of these c-Si PV modules, based on the temperature-corrected performance ratio, range from -0.03 to -0.47%/year, which satisfy the products' performance warranty. Further analysis of the short-circuit current (Isc), open-circuit voltage, and fill factor for these modules shows that the performance degradation is mainly attributed to the Isc loss. The possible causes of the module performance deterioration are also discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies · Photovoltaic Systems and Sustainability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. 10.1016/j.solmat.2015.11.04710.1016/j.solmat.2015.11.047 ↗
2. 2018
3. 10.1109/PVSC.2013.674408710.1109/PVSC.2013.6744087 ↗
4. Procedures for Temperature and Irradiance Corrections to Measured IV Characteristics of Crystalline Silicon Photovoltaic Devices · 2009
5. 10.2172/1218710.2172/12187 ↗
6. Outdoor PV module degradation of current-voltage parameters
7. 10.1109/PVSC.2002.119086910.1109/PVSC.2002.1190869 ↗
8. 10.1109/PVSC.2015.735560710.1109/PVSC.2015.7355607 ↗
9. 10.1109/PVSC.1991.16927510.1109/PVSC.1991.169275 ↗
10. PV degradation methodology comparison—A basis for a standard
11. 10.1109/JPHOTOV.2017.276258710.1109/JPHOTOV.2017.2762587 ↗
12. 10.1109/JPHOTOV.2017.276568010.1109/JPHOTOV.2017.2765680 ↗
13. 10.1109/JPHOTOV.2018.284379110.1109/JPHOTOV.2018.2843791 ↗
14. 10.1002/pip.302810.1002/pip.3028 ↗
15. 10.1039/C6EE02271E10.1039/C6EE02271E ↗
16. 10.1002/pip.118210.1002/pip.1182 ↗
17. 10.1002/pip.274410.1002/pip.2744 ↗
18. 10.1002/pip.62710.1002/pip.627 ↗
19. 10.1002/pip.290410.1002/pip.2904 ↗
20. 10.1002/pip.271710.1002/pip.2717 ↗
21. 10.1002/pip.290310.1002/pip.2903 ↗
22. 10.1109/JPHOTOV.2013.228274110.1109/JPHOTOV.2013.2282741 ↗
23. 10.1109/PVSC.2002.119087910.1109/PVSC.2002.1190879 ↗
24. 2018
25. 2018
26. Assessing the causes of encapsulant delamination in PV modules
27. 10.1016/j.egypro.2012.07.01910.1016/j.egypro.2012.07.019 ↗
28. 10.1002/apmc.1997.05252011410.1002/apmc.1997.052520114 ↗
29. 10.1002/pip.286610.1002/pip.2866 ↗
30. 10.1109/JPHOTOV.2018.281769210.1109/JPHOTOV.2018.2817692 ↗
31. 2018
32. 10.1109/JPHOTOV.2016.262135210.1109/JPHOTOV.2016.2621352 ↗
33. 10.1016/j.solmat.2017.08.04010.1016/j.solmat.2017.08.040 ↗
34. 10.1109/WCPEC.2006.27991410.1109/WCPEC.2006.279914 ↗
35. 10.1109/JPHOTOV.2014.233805110.1109/JPHOTOV.2014.2338051 ↗
36. 10.1002/ese3.15010.1002/ese3.150 ↗
37. 10.1016/j.renene.2016.10.05210.1016/j.renene.2016.10.052 ↗
38. Degradation evaluation of crystalline-silicon photovoltaic modules after a few operation years in a tropical environment10.1016/j.solener.2014.02.006 ↗
39. 10.1109/JPHOTOV.2017.277977910.1109/JPHOTOV.2017.2779779 ↗
40. 10.5194/hessd-4-439-200710.5194/hessd-4-439-2007 ↗