Abstract

Aluminum oxide thin films fabricated via atomic layer deposition are introduced as passivating tunneling interlayers between hole-selective molybdenum oxide contacts and silicon absorbers. Surface recombination velocity and specific contact resistivity are reported as a function of Al 2 O 3 thickness. The effects of substrate chemical pretreatment, the thermal history of the Al 2 O 3 layers prior to MoO x deposition, and the thermal history of the completed Al 2 O 3 /MoO x stacks were also investigated. When an SiO x /Al 2 O 3 passivating stack was incorporated and the completed test structure was annealed at 200 °C, the observed recombination velocities were reduced from ~10 000 cm/s for an unpassivated (initially hydrogen-terminated) Si/MoO x direct contact to ~500 cm/s, while maintaining a contact resistivity at or below 0.1 Ω·cm 2 . The data demonstrate the capability of ultrathin Al 2 O 3 to improve Si/MoOx contact properties and may be of interest in the design of future Si heterojunctions.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. 10.1016/j.mssp.2017.11.03710.1016/j.mssp.2017.11.037 ↗
2. 10.1109/16.4636810.1109/16.46368 ↗
3. 10.1063/1.148390310.1063/1.1483903 ↗
4. 10.1063/1.224073610.1063/1.2240736 ↗
5. 10.1063/1.333472910.1063/1.3334729 ↗
6. 10.1063/1.302109110.1063/1.3021091 ↗
7. 10.1116/1.484359510.1116/1.4843595 ↗
8. 10.1016/j.solmat.2018.11.01110.1016/j.solmat.2018.11.011 ↗
9. 10.1063/1.477559510.1063/1.4775595 ↗
10. 10.1063/1.161891810.1063/1.1618918 ↗
11. 10.1103/PhysRevB.83.23330110.1103/PhysRevB.83.233301 ↗
12. 10.1063/1.291332010.1063/1.2913320 ↗
13. 10.1063/1.496483510.1063/1.4964835 ↗
14. 10.1016/j.solmat.2018.06.04710.1016/j.solmat.2018.06.047 ↗
15. 10.1109/JPHOTOV.2018.279710610.1109/JPHOTOV.2018.2797106 ↗
16. 10.1002/pssr.20190068810.1002/pssr.201900688 ↗
17. 10.1557/jmr.2016.45310.1557/jmr.2016.453 ↗
18. 10.1557/JMR.1996.035010.1557/JMR.1996.0350 ↗
19. 10.1016/j.mssp.2018.11.02810.1016/j.mssp.2018.11.028 ↗
20. 10.1063/1.504177410.1063/1.5041774 ↗
21. 10.1002/solr.20170022710.1002/solr.201700227 ↗
22. 10.1016/j.egypro.2017.09.26810.1016/j.egypro.2017.09.268 ↗
23. 10.1109/ICEngTechnol.2017.830815510.1109/ICEngTechnol.2017.8308155 ↗
24. 10.1063/1.337433310.1063/1.3374333 ↗
25. 10.1063/1.311096810.1063/1.3110968 ↗
26. 10.1063/1.326371910.1063/1.3263719 ↗
27. 10.1063/1.510059910.1063/1.5100599 ↗
28. 10.1109/TNANO.2003.82077410.1109/TNANO.2003.820774 ↗
29. 10.1021/nl404389u10.1021/nl404389u ↗
30. 10.1063/1.486888010.1063/1.4868880 ↗
31. 10.1016/0038-1101(67)90063-910.1016/0038-1101(67)90063-9 ↗
32. 10.1063/1.490346710.1063/1.4903467 ↗
33. 10.1016/j.materresbull.2018.10.01810.1016/j.materresbull.2018.10.018 ↗
34. 10.1063/1.504525010.1063/1.5045250 ↗
35. 10.1002/pssr.20170010710.1002/pssr.201700107 ↗
36. 10.1109/JPHOTOV.2018.279613110.1109/JPHOTOV.2018.2796131 ↗
37. 10.1063/1.492874710.1063/1.4928747 ↗
38. 10.1021/acsenergylett.7b0127910.1021/acsenergylett.7b01279 ↗
39. Mitigating plasmonic absorption losses at rear electrodes in high-efficiency silicon solar cells using dopant-free contact stacks
40. 10.1016/j.solmat.2017.06.02410.1016/j.solmat.2017.06.024 ↗
41. 10.1038/s41560-019-0463-610.1038/s41560-019-0463-6 ↗
42. 10.1016/j.materresbull.2017.09.00510.1016/j.materresbull.2017.09.005 ↗
43. 10.1109/JPHOTOV.2016.260457410.1109/JPHOTOV.2016.2604574 ↗
44. 10.1109/JPHOTOV.2011.217496710.1109/JPHOTOV.2011.2174967 ↗
45. 10.1063/1.312957810.1063/1.3129578 ↗
46. 10.1063/1.496009710.1063/1.4960097 ↗
47. 10.1007/s42341-018-00089-010.1007/s42341-018-00089-0 ↗
48. 10.1063/1.492226710.1063/1.4922267 ↗
49. 10.1016/j.egypro.2016.07.12510.1016/j.egypro.2016.07.125 ↗
50. 10.1002/pssr.20130811510.1002/pssr.201308115 ↗
51. Hydrogen passivation of poly-Si/SiOx contacts for Si solar cells using Al2O3 studied with deuterium
52. 10.1109/JPHOTOV.2019.291738610.1109/JPHOTOV.2019.2917386 ↗
53. 10.1063/1.9735910.1063/1.97359 ↗
54. 10.1116/1.493016110.1116/1.4930161 ↗
55. haynes · CRC Handbook of Chemistry and Physics · 2011