Enhanced p-Type Doping in Polycrystalline CdTe Films: Deposition and Activation
Source abstract
Abstract
An in situ nonequilibrium method to increase hole density in polycrystalline CdTe thin films to 10 16 cm -3 using group V substitution on Te is presented. Single-phase CdTe films doped with P, As, and Sb were deposited at 550 °C at 100-200 nm/s onto moving cadmium sulfide/high resistance transparent buffer layer/transparent conductive oxide /glass superstrates by vapor transport deposition in Cd overpressure from high purity compound sources. Doping levels before and after activation were determined by capacitance-voltage analysis of diagnostic devices. Secondary ion mass spectrometry depth profiling confirmed dopant incorporation levels of 10 17 -10 18 atoms/cm 3 in as-deposited films. Electronic activation was carried out by post-deposition annealing in Cd or CdCl 2 vapor with fast cooling, increasing acceptor concentrations to >10 15 cm -3 for P and >10 16 cm -3 for As and Sb, compared with mid -10 14 cm -3 acceptor levels for undoped CdTe films. The activation methods are compatible with post-deposition processing presently used for high-efficiency CdTe solar cells. For the dopants As and Sb, the acceptor concentration increased by substitutional AsTe and SbTe formation, respectively, which was validated by cathodoluminescence spectroscopy.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Advanced Semiconductor Detectors and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. 10.1063/1.496620910.1063/1.4966209 ↗
2. 10.1063/1.128741410.1063/1.1287414 ↗
3. 10.1116/1.221468910.1116/1.2214689 ↗
4. 10.1117/1. JPE.4.04099610.1117/1. JPE.4.040996 ↗
5. Chemical surface deposition of ultra-thin cadmium sulfide films for high performance and high cadmium utilization
6. 10.1063/1.497445910.1063/1.4974459 ↗
7. 10.1088/1361-6463/aaa67e10.1088/1361-6463/aaa67e ↗
8. 10.1109/JPHOTOV.2017.265503310.1109/JPHOTOV.2017.2655033 ↗
9. 10.1109/WCPEC.2006.27949610.1109/WCPEC.2006.279496 ↗
10. 10.1149/1.213331210.1149/1.2133312 ↗
11. 10.1557/opl.2013.101710.1557/opl.2013.1017 ↗
12. 10.1002/adma.20160380110.1002/adma.201603801 ↗
13. 10.1063/1.492672610.1063/1.4926726 ↗
14. 10.1016/j.solmat.2004.02.00510.1016/j.solmat.2004.02.005 ↗
15. 10.1109/JPHOTOV.2015.247806110.1109/JPHOTOV.2015.2478061 ↗
16. 10.1063/1.498432010.1063/1.4984320 ↗
17. 10.1109/JPHOTOV.2016.259826010.1109/JPHOTOV.2016.2598260 ↗
18. Accelerated stress testing and diagnostic analysis of degradation in CdTe solar cells10.1117/12.795360 ↗
19. 10.1063/1.159797410.1063/1.1597974 ↗