journal article·2019-01

Assessing the Impact of Thermal Profiles on the Elimination of Light- and Elevated-Temperature-Induced Degradation

Chandany Sen, Moonyong Kim, Daniel Chen, Utkarshaa Varshney, Shaoyang Liu, Aref Samadi, Alison Ciesla, Stuart Ross Wenham, Catherine Emily Chan, CheeMun Chong, Malcolm David Abbott, Brett Jason Hallam

IEEE Journal of Photovoltaics· Volume 9· Issue 1
Publisher page

Abstract

Light- and elevated-temperature-induced degradation (LeTID) in p-type multicrystalline silicon has a severe impact on the effective minority carrier lifetime of silicon and remains a crucial challenge for solar cell manufacturers. The precise cause of the degradation is yet to be confirmed; however, several approaches have been presented to reduce the extent of degradation. This paper presents insights on the impact of thermal budgets and cooling rates during post-firing illuminated anneals and their role in changing the lifetime and mitigating LeTID for thermal processes between 350 and 500 °C. We demonstrate that the thermal budget of these processes plays a crucial role in LeTID suppression and that the cooling rate only plays a role during short treatment durations (≤1 min). For the parameter space studied, we show that annealing for an appropriate time and temperature can both enhance the minority carrier lifetime and completely suppress the LeTID, with the injection-dependent Shockley-Read-Hall lifetime analysis indicating that the recombination activity of the LeTID defects in the bulk has been eliminated. Finally, this paper demonstrates a process that results in a stable lifetime after 800 h of conventional light-soaking at 75 °C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. 10.1063/1.214058410.1063/1.2140584 ↗
2. 10.1109/JPHOTOV.2017.269549610.1109/JPHOTOV.2017.2695496 ↗
3. 10.1016/j.solmat.2014.06.02710.1016/j.solmat.2014.06.027 ↗
4. 10.1007/s11708-016-0442-610.1007/s11708-016-0442-6 ↗
5. 10.1063/1.34541410.1063/1.345414 ↗
6. 10.1103/PhysRev.87.83510.1103/PhysRev.87.835 ↗
7. 10.1063/1.501685410.1063/1.5016854 ↗
8. Degradation of surface passivation and bulk in p-type monocrystalline silicon wafers at elevated temperature
9. 10.1016/j.egypro.2016.07.06110.1016/j.egypro.2016.07.061 ↗
10. 10.1063/1.183357710.1063/1.1833577 ↗
11. 10.1016/j.solmat.2015.06.01510.1016/j.solmat.2015.06.015 ↗
12. 10.1002/pip.69010.1002/pip.690 ↗
13. 10.1016/j.solmat.2017.08.00310.1016/j.solmat.2017.08.003 ↗
14. 10.1002/pip.295410.1002/pip.2954 ↗
15. 10.1002/solr.20160002810.1002/solr.201600028 ↗
16. 10.1016/j.solmat.2018.04.02410.1016/j.solmat.2018.04.024 ↗
17. 10.1016/j.solmat.2015.06.05510.1016/j.solmat.2015.06.055 ↗
18. 10.1109/JPHOTOV.2016.255698110.1109/JPHOTOV.2016.2556981 ↗
19. 10.1063/1.494483910.1063/1.4944839 ↗
20. Dupont Solamet PV19A Photovoltaic metallization technical datasheet · 2015
21. SOL9631 Series New generation PERC front-side silver paste technical datasheet · 2016
22. 10.1016/S0927-0248(00)00098-210.1016/S0927-0248(00)00098-2 ↗
23. 10.1063/1.138907610.1063/1.1389076 ↗
24. 10.1016/j.egypro.2012.07.03410.1016/j.egypro.2012.07.034 ↗
25. 10.1063/1.37118610.1063/1.371186 ↗
26. 10.1016/j.solmat.2018.05.03410.1016/j.solmat.2018.05.034 ↗
27. 10.1016/S0927-0248(98)00179-210.1016/S0927-0248(98)00179-2 ↗
28. 10.1002/pip.58610.1002/pip.586 ↗
29. 10.1016/j.egypro.2016.07.00810.1016/j.egypro.2016.07.008 ↗
30. 10.1016/j.egypro.2017.09.08510.1016/j.egypro.2017.09.085 ↗
31. 10.1002/pssr.20140942410.1002/pssr.201409424 ↗
32. Oxygen-related trapping and recombination centres in boron-doped crystalline silicon
33. Light induced degradation of rear passivated mc-Si solar cells
34. 10.1002/solr.20170015910.1002/solr.201700159 ↗
35. 10.7567/JJAP.56.08MB1310.7567/JJAP.56.08MB13 ↗
36. 10.1109/JPHOTOV.2016.260670410.1109/JPHOTOV.2016.2606704 ↗
37. 10.1109/PVSC.2018.854788010.1109/PVSC.2018.8547880 ↗
38. Should the refractive index at 633 nm be used to characterize silicon nitride films?
39. 10.1002/solr.20170012910.1002/solr.201700129 ↗
40. 10.1002/pssr.20160027210.1002/pssr.201600272 ↗
41. 10.1063/1.37163310.1063/1.371633 ↗
42. 10.1016/j.solmat.2018.04.03610.1016/j.solmat.2018.04.036 ↗
43. A quasi-steady-state open-circuit voltage method for solar cell characterization