Abstract
A three-state model is used to explore the influence of the accelerated formation of recombination-active defect complexes on the mitigation of carrier-induced degradation in p-type silicon containing boron and oxygen. Defect formation is observed to be a critical factor for the speed at which carrier-induced degradation can be mitigated. Defect formation also plays a critical role in determining the effectiveness of mitigation at elevated temperatures. It is observed that under conventional conditions, at a processing temperature of 200 °C, approximately 170 s are required to form and passivate 99% of possible defects. The experimentally demonstrated improved effectiveness of carrier-induced defect passivation with a process time of 10 s at temperatures over 300 °C is consistent with a substantial acceleration of defect formation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. 10.1109/PVSC.1996.56404210.1109/PVSC.1996.564042 ↗
2. On the degradation of cz-silicon solar cells
3. 10.1063/1.351174110.1063/1.3511741 ↗
4. 10.1063/1.214058410.1063/1.2140584 ↗
5. 10.1109/PVSC.1997.65391410.1109/PVSC.1997.653914 ↗
6. 21% efficient solar cells processed from Czochralski grown silicon
7. 10.1063/1.330986910.1063/1.3309869 ↗
8. 10.1016/j.egypro.2013.07.32710.1016/j.egypro.2013.07.327 ↗
9. 10.1109/JPHOTOV.2013.227866310.1109/JPHOTOV.2013.2278663 ↗
10. 10.1002/pssa.20100014610.1002/pssa.201000146 ↗
11. 10.1016/j.egypro.2011.06.10010.1016/j.egypro.2011.06.100 ↗
12. 10.1063/1.37163310.1063/1.371633 ↗
13. The bolid project: Suppression of the boron-oxygen related light-induced-degradation
14. 10.1016/j.egypro.2013.07.31710.1016/j.egypro.2013.07.317 ↗
15. 10.1016/j.solmat.2014.06.02710.1016/j.solmat.2014.06.027 ↗
16. 10.1063/1.490646510.1063/1.4906465 ↗
17. 10.1016/j.egypro.2015.07.08510.1016/j.egypro.2015.07.085 ↗
18. 10.1063/1.343135910.1063/1.3431359 ↗
19. 10.1063/1.476868810.1063/1.4768688 ↗
20. 10.1063/1.491938510.1063/1.4919385 ↗
21. 10.1063/1.351715510.1063/1.3517155 ↗
22. 10.1063/1.480431010.1063/1.4804310 ↗
23. Light-induced degradation in crystalline silicon solar cells10.4028/www.scientific.net/SSP.95-96.187 ↗
24. 10.1109/JPHOTOV.2014.233949410.1109/JPHOTOV.2014.2339494 ↗
25. Performance comparison between bp solar mono and traditional multicrystalline modules
26. 10.1002/pssr.20130716510.1002/pssr.201307165 ↗
27. 10.1002/pip.77910.1002/pip.779 ↗
28. Boron-oxygen related lifetime degradation in p-type and n-type silicon
29. 10.1109/WCPEC.2006.27961110.1109/WCPEC.2006.279611 ↗
30. 10.1063/1.486367410.1063/1.4863674 ↗
31. 10.1103/PhysRevB.69.02410710.1103/PhysRevB.69.024107 ↗
32. Hydrogenated silicon nitride for regeneration of light induced degradation
33. Investigation of photon and thermal induced changes in silicon solar cells
34. 10.1002/pssr.20151006410.1002/pssr.201510064 ↗
35. 10.1063/1.480699910.1063/1.4806999 ↗
36. 10.1016/j.egypro.2015.07.11310.1016/j.egypro.2015.07.113 ↗
37. 10.1109/JPHOTOV.2013.228173210.1109/JPHOTOV.2013.2281732 ↗
38. High speed regeneration of BO-defects: Improving long-term solar cell performance within seconds
39. 10.1063/1.363349210.1063/1.3633492 ↗
40. Hydrogen passivation mechanisms in silicon solar cells
41. Advanced hydrogenation of silicon solar cells