journal article·2022-07Open access

Improving ALD-Al2O3 Surface Passivation of Si Utilizing Pre-Existing SiOx

Michael N. Getz, Marco Povoli, Eduard Monakhov

IEEE Journal of Photovoltaics· Volume 12· Issue 4

Abstract

Al 2 O 3 has rapidly become the surface passivation material of choice for p + layers of solar cells because of its high negative fixed charge, good long-term and thermal stability, and no parasitic absorption. In this article, the surface saturation current density, fixed charge, and interface state density are compared for Al 2 O 3 deposited on Si substrates where the pre-existing out-of-the-box SiO x layer was not removed, with substrates where the SiO x was removed by hydrofluoric acid. The depositions are performed by atomic layer deposition at temperatures in the 150–300 °C range, using trimethylaluminium, H 2 O, and O 3 as precursors. The samples where the native oxide was not removed achieve a higher level of surface passivation for every tested deposition temperature, with the sample deposited at 200 °C exhibiting a surface saturation current density of only 0.9 fA/cm 2 after annealing, a fixed charge of −4.2 × 10 12 cm −2 , and a density of interface states of 9.8 × 10 9 cm −2 eV −1 . Capacitance and conductance voltage characteristics reveal a strong correlation between the surface saturation current density and the density of interface states and fixed charges. It is also determined that the long-term stability of the surface passivation depends on the deposition temperature, with higher deposition temperatures resulting in improved long-term stability. The results indicate that H-terminated Si prior to Al 2 O 3 deposition may have a detrimental effect on the surface passivation.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Microsystems and Nanotechnology (MiNaLab), SINTEF Digital, Oslo, Norway

Department of Physics, University of Oslo, Oslo, Norway

Funding

The Research Council of Norway · The Norwegian Micro- and Nano-Fabrication Facility · NorFab

References (58)

Show source-provided references
1. Fischer · 2000
2. 10.1063/1.224073610.1063/1.2240736 ↗
3. 10.1116/1.472820510.1116/1.4728205 ↗
4. 10.1002/pssr.20090327210.1002/pssr.200903272 ↗
5. 10.1016/j.solmat.2014.06.00510.1016/j.solmat.2014.06.005 ↗
6. 10.1063/1.492226710.1063/1.4922267 ↗
7. 10.1002/pssa.20170029310.1002/pssa.201700293 ↗
8. 10.1016/j.solmat.2018.06.04710.1016/j.solmat.2018.06.047 ↗
9. Progress in the surface passivation of silicon solar cells
10. 10.1063/1.326457210.1063/1.3264572 ↗
11. 10.1088/1361-6528/ab045010.1088/1361-6528/ab0450 ↗
12. 10.1116/1.366409010.1116/1.3664090 ↗
13. 10.1016/j.apsusc.2011.08.03510.1016/j.apsusc.2011.08.035 ↗
14. 10.1063/1.505470310.1063/1.5054703 ↗
15. 10.1038/srep4670310.1038/srep46703 ↗
16. 10.1063/1.278416810.1063/1.2784168 ↗
17. 10.1021/acsami.5b0660610.1021/acsami.5b06606 ↗
18. 10.1016/j.solmat.2018.05.04010.1016/j.solmat.2018.05.040 ↗
19. 10.1109/JPHOTOV.2013.223828910.1109/JPHOTOV.2013.2238289 ↗
20. 10.1063/1.302109110.1063/1.3021091 ↗
21. 10.1063/1.370128010.1063/1.3701280 ↗
22. 10.1149/1.350197010.1149/1.3501970 ↗
23. 10.1016/j.apsusc.2015.09.26310.1016/j.apsusc.2015.09.263 ↗
24. 10.1063/1.365824610.1063/1.3658246 ↗
25. 10.1002/pssc.20120024410.1002/pssc.201200244 ↗
26. 10.1016/j.egypro.2014.08.06710.1016/j.egypro.2014.08.067 ↗
27. 10.1016/j.solmat.2018.07.00310.1016/j.solmat.2018.07.003 ↗
28. 10.1016/j.apsusc.2014.05.08710.1016/j.apsusc.2014.05.087 ↗
29. 10.1116/1.490145610.1116/1.4901456 ↗
30. Studies on wet-chemical surface conditioning for Al2O3 passivation layers deposited with ALD
31. 10.1063/1.488659510.1063/1.4886595 ↗
32. 10.1063/5.005121510.1063/5.0051215 ↗
33. 10.1002/solr.20210060510.1002/solr.202100605 ↗
34. 10.1063/1.486764310.1063/1.4867643 ↗
35. 10.1063/1.36710110.1063/1.367101 ↗
36. Comparison between Al2O3 thin films grown by ALD using H2O or O3 as oxidant source
37. 10.1116/1.368305710.1116/1.3683057 ↗
38. 10.1016/j.dib.2016.12.03010.1016/j.dib.2016.12.030 ↗
39. Measurement of the emitter saturation current by a contactless photoconductivity decay method
40. 10.1103/PhysRevB.86.16520210.1103/PhysRevB.86.165202 ↗
41. 10.1149/1.327604010.1149/1.3276040 ↗
42. 10.1016/j.egypro.2014.08.06810.1016/j.egypro.2014.08.068 ↗
43. 10.1016/0038-1101(80)90064-710.1016/0038-1101(80)90064-7 ↗
44. 10.1149/1.209667310.1149/1.2096673 ↗
45. 10.1109/PVSC.2010.561414810.1109/PVSC.2010.5614148 ↗
46. 10.1063/1.194072710.1063/1.1940727 ↗
47. 10.1063/1.178762410.1063/1.1787624 ↗
48. 10.1063/1.159571910.1063/1.1595719 ↗
49. 10.1039/b100704l10.1039/b100704l ↗
50. 10.1073/pnas.101129510710.1073/pnas.1011295107 ↗
51. 10.1149/1.139332510.1149/1.1393325 ↗
52. 10.1039/D0NR03860A10.1039/D0NR03860A ↗
53. 10.1007/s10854-018-0383-410.1007/s10854-018-0383-4 ↗
54. 10.1063/1.162939710.1063/1.1629397 ↗
55. 10.1103/PhysRevApplied.16.01402610.1103/PhysRevApplied.16.014026 ↗
56. 10.1063/1.358722710.1063/1.3587227 ↗
57. 10.1007/s11082-020-02689-810.1007/s11082-020-02689-8 ↗
58. 10.1021/cm030454610.1021/cm0304546 ↗