Silicon Nitride Deposition: Impact on Lifetime and Light-Induced Degradation at Elevated Temperature in Multicrystalline Silicon
Source abstract
Abstract
Light and elevated temperature induced degradation (LeTID) in multicrystalline (mc) silicon (Si) is known to be sensitive to the silicon nitride (SiN x :H) deposition and the firing, but the reason remains unknown. Three plasma-enhanced chemical vapor deposition (PECVD) tools are used to deposit five different layers, causing significant differences in the initial lifetimes before and after firing. The impact of the different depositions can be effectively compared by replacing the SiN x :H with well-passivating room-temperature iodine ethanol passivation (IE). The IE passivation reveals that the firing of SiN x :H and subsequent bulk hydrogenation leads to a lifetime increase only in the gettered samples. Although the PECVD temperature load affects the bulk lifetime, it does not cause LeTID without SiN x :H deposition. LeTID is only detected in samples fired with SiN x :H, but once the LeTID precursors have been activated, the PECVD layer can be etched and the wafer thinned down without affecting LeTID formation. No link is found between the LeTID defect density and the bulk-hydrogenated lifetime. Instead the LeTID defect density appears to decrease with decreasing PECVD deposition time and temperature.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Hydrogen kinetics in crystalline silicon–PECVD SiN studies in mc and Cz silicon
2. 10.1016/S0022-3093(01)01135-810.1016/S0022-3093(01)01135-8 ↗
3. 10.1007/978-3-642-57121-310.1007/978-3-642-57121-3 ↗
4. 10.1063/1.504933910.1063/1.5049339 ↗
5. 10.1109/JPHOTOV.2014.232227610.1109/JPHOTOV.2014.2322276 ↗
6. 10.1063/1.496791410.1063/1.4967914 ↗
7. 10.1109/JPHOTOV.2019.289667110.1109/JPHOTOV.2019.2896671 ↗
8. 10.1007/s10854-007-9321-610.1007/s10854-007-9321-6 ↗
9. 10.1063/1.192770610.1063/1.1927706 ↗
10. 10.1063/1.34244110.1063/1.342441 ↗
11. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
12. Influence of low-temperature annealing on LeTID in multicrystalline silicon
13. 10.1109/JPHOTOV.2016.255698110.1109/JPHOTOV.2016.2556981 ↗
14. 10.1002/pssr.20160027210.1002/pssr.201600272 ↗
15. 10.1109/JPHOTOV.2016.260670410.1109/JPHOTOV.2016.2606704 ↗
16. 10.1109/JPHOTOV.2016.260669910.1109/JPHOTOV.2016.2606699 ↗
17. Possible candidates for impurities in mc-Si wafers responsible for light-induced lifetime degradation and regeneration
18. 10.1063/1.9293410.1063/1.92934 ↗
19. 10.1016/j.egypro.2016.07.07910.1016/j.egypro.2016.07.079 ↗
20. 10.1109/JPHOTOV.2017.278385110.1109/JPHOTOV.2017.2783851 ↗
21. Modulation of carrier-induced defect kinetics in multi-crystalline PERC cells through dark annealing10.1002/solr.201600028 ↗
22. 10.1063/1.298752110.1063/1.2987521 ↗
23. 10.1016/j.egypro.2017.09.08510.1016/j.egypro.2017.09.085 ↗
24. 10.1016/j.solmat.2017.08.00710.1016/j.solmat.2017.08.007 ↗
25. 10.1002/pip.283210.1002/pip.2832 ↗
26. 10.1002/pip.295410.1002/pip.2954 ↗
27. Microwave induced remote hydrogen plasma (MIRHP) passivation of multicrystalline silicon solar cells
28. 10.1016/j.solmat.2016.05.06110.1016/j.solmat.2016.05.061 ↗
29. 10.1016/j.solmat.2016.05.02210.1016/j.solmat.2016.05.022 ↗
30. 10.1016/j.solmat.2017.05.06610.1016/j.solmat.2017.05.066 ↗
31. 10.1016/j.solmat.2015.06.01510.1016/j.solmat.2015.06.015 ↗
32. 10.1016/j.solmat.2018.12.02110.1016/j.solmat.2018.12.021 ↗
33. Light-induced degradation of rear passivated mc-Si solar cells
34. 10.1063/1.363003110.1063/1.3630031 ↗
35. 10.4028/www.scientific.net/SSP.108-109.65510.4028/www.scientific.net/SSP.108-109.655 ↗
36. 10.1016/j.solmat.2012.05.04210.1016/j.solmat.2012.05.042 ↗
37. 10.1016/j.solmat.2018.04.02410.1016/j.solmat.2018.04.024 ↗
38. 10.1109/JPHOTOV.2017.275507210.1109/JPHOTOV.2017.2755072 ↗
39. 10.1063/1.504175610.1063/1.5041756 ↗
40. 10.1063/1.32509510.1063/1.325095 ↗
41. 10.1109/JPHOTOV.2018.279141110.1109/JPHOTOV.2018.2791411 ↗
42. 10.1063/1.504933410.1063/1.5049334 ↗
43. Hydrogen-induced degradation
44. 10.1016/S0927-0248(00)00098-210.1016/S0927-0248(00)00098-2 ↗