journal article·2016-11Open access

Application of Photocurrent Model on Polymer Solar Cells Under Forward Bias Stress

Antonio Rizzo, Lorenzo Torto, Nicola Wrachien, Michael Corazza, Frederik C. Krebs, Suren A. Gevorgyan, Andrea Cester

IEEE Journal of Photovoltaics· Volume 6· Issue 6

Abstract

We performed a constant current stress at forward bias on organic heterojunction solar cells. We measured current voltage curves in both dark and light at each stress step to calculate the photocurrent. An existing model applied to photocurrent experimental data allows the estimation of several parameters such as generation, recombination, dissociation rate, and nearly zero field voltage within the active layer as a function of the stress time. The analysis of extrapolated parameters shows that the stress mainly affects the recombination rate of the polaron charge transfer states.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. 10.1039/b805435e10.1039/b805435e ↗
2. 10.1039/b718563d10.1039/b718563d ↗
3. 10.1002/pssa.20052114910.1002/pssa.200521149 ↗
4. 10.1021/am900446x10.1021/am900446x ↗
5. 10.1016/j.solmat.2012.09.00810.1016/j.solmat.2012.09.008 ↗
6. Factors determining large observed increases in power conversion efficiency of P3HT:PCBM solar cells embedded with Mo6S9?xIx nanowires10.1016/j.synthmet.2015.12.009 ↗
7. 10.1021/nl103482n10.1021/nl103482n ↗
8. 10.1038/nphoton.2015.8410.1038/nphoton.2015.84 ↗
9. 10.1016/j.orgel.2015.01.01410.1016/j.orgel.2015.01.014 ↗
10. 10.1109/IRPS.2016.757452310.1109/IRPS.2016.7574523 ↗
11. 10.1016/j.solmat.2008.01.01310.1016/j.solmat.2008.01.013 ↗
12. 10.1016/j.orgel.2012.12.03310.1016/j.orgel.2012.12.033 ↗
13. Analysis based on I-V curve changes of organic photovoltaic mini-modules subjected to degradation under different temperature and humidity conditions
14. 10.1016/j.solmat.2011.01.03610.1016/j.solmat.2011.01.036 ↗
15. 10.1016/j.microrel.2015.06.08210.1016/j.microrel.2015.06.082 ↗
16. 10.1016/j.solmat.2010.06.00710.1016/j.solmat.2010.06.007 ↗
17. 10.1016/j.solmat.2011.08.02710.1016/j.solmat.2011.08.027 ↗
18. 10.1103/PhysRevB.81.08520310.1103/PhysRevB.81.085203 ↗
19. 10.1016/j.solmat.2009.04.02010.1016/j.solmat.2009.04.020 ↗
20. 10.1063/1.33011110.1063/1.330111 ↗
21. 10.1016/j.solmat.2012.01.01310.1016/j.solmat.2012.01.013 ↗
22. 10.1063/1.44724310.1063/1.447243 ↗
23. 10.1016/j.orgel.2010.07.01610.1016/j.orgel.2010.07.016 ↗
24. 10.1016/j.solmat.2012.01.01210.1016/j.solmat.2012.01.012 ↗
25. 10.1002/adma.20110418710.1002/adma.201104187 ↗
26. 10.1016/j.solmat.2008.01.00510.1016/j.solmat.2008.01.005 ↗