journal article·2017-04

Via-First Process to Enable Copper Metallization of Glass Interposers With High-Aspect-Ratio, Fine-Pitch Through-Package-Vias

Timothy B. Huang, Bruce Chou, Jialing Tong, Tomonori Ogawa, Venky Sundaram, Rao R. Tummala

Publisher page

Abstract

A via-first process for metallizing copper on glass substrates is presented using a thin, patternable polymer film, electroless copper deposition, and semiadditive processing. A procedure for partially precuring the polymer was developed in order to achieve a tented via structure after dry-film lamination and curing. The flexibility of the process is demonstrated by the use of plasma etching, CO 2 , and UV laser ablation as patterning technologies. Metallization by electroless copper deposition and semiadditive processing is shown to be conformal, continuous, and without defects on the surface and in the vias as demonstrated by cross-sectional analysis. Glass of 100 μm thickness with vias of 10-20 μm diameter and 40 μm pitch was metallized to demonstrate the dimensional capability of the process. Thermomechanical reliability was validated by copper peel testing after highly accelerated stress testing and daisy-chain resistance measurements taken throughout thermal cycle testing.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. 10.1109/ECTC.2016.32110.1109/ECTC.2016.321 ↗
2. 10.1109/ECTC.2015.715986910.1109/ECTC.2015.7159869 ↗
3. 10.1109/ECTC.2012.624908010.1109/ECTC.2012.6249080 ↗
4. 10.1109/TCPMT.2014.230342710.1109/TCPMT.2014.2303427 ↗
5. 10.1109/TCPMT.2015.245073110.1109/TCPMT.2015.2450731 ↗
6. 10.1098/rspa.1961.009310.1098/rspa.1961.0093 ↗
7. 10.1111/j.1151-2916.1966.tb13135.x10.1111/j.1151-2916.1966.tb13135.x ↗
8. 10.1116/1.57425910.1116/1.574259 ↗
9. 10.1016/0040-6090(94)05812-110.1016/0040-6090(94)05812-1 ↗
10. 10.1063/1.37241210.1063/1.372412 ↗
11. 10.1109/ECTC.2013.657582510.1109/ECTC.2013.6575825 ↗
12. 10.1149/2.038312jes10.1149/2.038312jes ↗
13. 10.1109/ECTC.2014.689751710.1109/ECTC.2014.6897517 ↗
14. A comparative reliability study of copper-plated glass vias, drilled with CO2 and ArF excimer lasers
15. 10.1016/j.apsusc.2011.04.10010.1016/j.apsusc.2011.04.100 ↗
16. 10.1109/ECTC.2013.657559510.1109/ECTC.2013.6575595 ↗
17. 10.1016/j.colsurfa.2004.10.03610.1016/j.colsurfa.2004.10.036 ↗
18. 10.1889/1.362109110.1889/1.3621091 ↗
19. 10.1109/ECTC.2014.689762010.1109/ECTC.2014.6897620 ↗
20. 10.1109/EPTC.2007.446974710.1109/EPTC.2007.4469747 ↗
21. Non-classical conductor losses due to copper foil roughness and treatment
22. 10.4071/isom-2013-WP1510.4071/isom-2013-WP15 ↗
23. 10.1109/ECTC.2011.589851610.1109/ECTC.2011.5898516 ↗
24. 10.1109/ECTC.2010.549091310.1109/ECTC.2010.5490913 ↗
25. 10.1109/TCPMT.2012.220439210.1109/TCPMT.2012.2204392 ↗
26. 10.4071/isom-WA1410.4071/isom-WA14 ↗
27. 10.1109/IMPACT.2015.736525610.1109/IMPACT.2015.7365256 ↗
28. 10.1109/IMPACT.2014.704846010.1109/IMPACT.2014.7048460 ↗
29. 10.1002/app.2006110.1002/app.20061 ↗
30. 10.4071/isom-2015-WP2110.4071/isom-2015-WP21 ↗
31. 10.1109/96.57556910.1109/96.575569 ↗
32. pozar · Microwave Engineering · 2011