Using Cross-Linked SU-8 to Flip-Chip Bond, Assemble, and Package MEMS Devices
Source abstract
Abstract
This paper investigates using an SU-8 photoresist as an adhesive material for flip-chip bonding, assembling, and packaging microelectromechanical systems devices. An important factor, when using SU-8 as an adhesive material is to control ultraviolet (UV) exposure during fabrication to maximize bond strength due to material cross linking. This approach is much improved over previous efforts where SU-8 bake times and temperatures where changed to alter material cross-linking. In this paper, bake times and temperatures were maintained constant and total UV exposure energy was varied. Once fabricated, bond strength was systematically tested to determine the tensile loads needed to separate bonded structures. The resulting separation force was shown to increase with UV exposure and ranged from 0.25 (5-s exposure) to 1.25 N (15-s exposure). The separation test data were then analyzed to determine the statistical significance of varying UV exposure time and its effect on SU-8 cross-linking and bond strength. The data show that total UV exposure dose is directly correlated with the bond strength of SU-8 bonded structures. By varying only UV dose, the separation force data exhibited a statistically significant dependence on SU-8 cross linking with a 5% probability of error. Further, SU-8 etch resiliency increased by approximately 40%-60% as cross linking was increased with UV exposures ranging from 5 to 15 s.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Advanced MEMS and NEMS Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. 10.1109/JMEMS.2005.85910210.1109/JMEMS.2005.859102 ↗
2. 10.1109/6040.88374910.1109/6040.883749 ↗
3. Low temperature polymer bonding processes for MEMS encapsulation
4. 10.1088/0960-1317/12/5/31510.1088/0960-1317/12/5/315 ↗
5. 10.1117/1.276732610.1117/1.2767326 ↗
6. 10.1016/j.proeng.2011.12.11710.1016/j.proeng.2011.12.117 ↗
7. 10.1109/JMEMS.2010.205554110.1109/JMEMS.2010.2055541 ↗
8. 10.1088/0960-1317/7/3/01010.1088/0960-1317/7/3/010 ↗
9. 10.1088/0960-1317/13/5/31810.1088/0960-1317/13/5/318 ↗
10. 10.1109/84.82577010.1109/84.825770 ↗
11. 10.1109/JMEMS.2007.91271110.1109/JMEMS.2007.912711 ↗
12. Encapsulation of vacuum sensors in a wafer level package using a gold-silicon eutectic
13. 10.1117/1.362563310.1117/1.3625633 ↗
14. SU-8 2000 Permanent Epoxy Photoresist Processing Guidelines · 2014
15. 10.1088/0960-1317/15/8/02610.1088/0960-1317/15/8/026 ↗