Abstract

In a series of articles, we consider the effects of the microstructure and the associated anisotropy of Sn grains on electromigration in lead-free solder bumps. In this article, we carried out experiments to characterize microstructures of tin-based solder bumps and to investigate their effects on electromigration-induced failure. Accelerated electromigration tests and electron backscatter diffraction (EBSD) tests are performed on tin-based solder bumps in wafer-level chip-scale packages (WLCSPs). EBSD analysis, together with the results of time to failure from accelerated electromigration tests, provides valuable information on the effects of the microstructure on electromigration-induced failure that can be used for predictive modeling. For Ni-based metallization, we find that tin self-diffusion is the dominant degradation mechanism and a strong effect of the grain orientation in the solder on the time to failure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. 10.1016/j.cap.2013.01.00210.1016/j.cap.2013.01.002 ↗
2. 10.1109/TCPMT.2018.288681310.1109/TCPMT.2018.2886813 ↗
3. A study of electromigration failure in Pb-free solder joints
4. 10.1016/j.pmatsci.2010.01.00110.1016/j.pmatsci.2010.01.001 ↗
5. 10.1063/1.161699310.1063/1.1616993 ↗
6. 10.1557/JMR.2010.023010.1557/JMR.2010.0230 ↗
7. Electromigration and thermomigration reliability of lead-free solder joints for advanced packaging applications
8. 10.1063/1.32264710.1063/1.322647 ↗
9. 10.1103/PhysRevB.9.147910.1103/PhysRevB.9.1479 ↗
10. 10.1063/1.171012710.1063/1.1710127 ↗
11. 10.1007/s11664-004-0083-010.1007/s11664-004-0083-0 ↗
12. 10.1557/JMR.2004.022210.1557/JMR.2004.0222 ↗
13. 10.1063/1.293699610.1063/1.2936996 ↗
14. 10.1007/s11664-008-0481-910.1007/s11664-008-0481-9 ↗
15. 10.1557/jmr.2012.1010.1557/jmr.2012.10 ↗
16. 10.1557/jmr.2010.8610.1557/jmr.2010.86 ↗
17. 10.1016/j.microrel.2010.01.00710.1016/j.microrel.2010.01.007 ↗
18. 10.1109/T-ED.1969.1675410.1109/T-ED.1969.16754 ↗
19. 10.1016/j.jallcom.2016.04.02410.1016/j.jallcom.2016.04.024 ↗
20. 10.1063/1.170882110.1063/1.1708821 ↗
21. lewis · WLCSP tin-based solder bump sample preparation instructions · 0
22. EBSD based analysis of lead free solders
23. 10.1016/j.actamat.2010.01.03010.1016/j.actamat.2010.01.030 ↗