Sn–3.0Ag–0.5Cu Nanocomposite Solder Reinforced With Bi2Te3Nanoparticles
Source abstract
Abstract
Nanocomposite solders are regarded as one of the most promising interconnect materials for the high-density electronic packaging due to their high mechanical strength and fine microstructure. However, the developments of nanocomposite solders have been limited by the inadequate compatibility between nanoparticles and solder matrix with respect to density, hardness, coefficient of thermal expansion, and surface activity. The compatibility issue will lead to a huge loss of nanoparticles from the solder matrix after the reflow soldering process. The thermal fatigue resistance of solder joint will also become degraded. Therefore, aiming to solve this problem, a novel nanocomposite solder consisting of Bi 2 Te 3 semiconductor nanoparticles and Sn-3.0Ag-0.5Cu (SAC305) solder is presented. The effect of nanoparticles on the viscosity of solder paste and the void content of solder bump was first studied. Then, a series of analysis on the composition and microstructure of the solder bump were completed using transmission electron microscopy, X-ray diffraction, inductively coupled plasma-mass spectrometry, scanning electron microscopy, and energy dispersive X-ray spectroscopy. The survival rate of nanoparticles in the solder bump after reflow soldering process reaches as high as 80%. The refined microstructure was observed from the cross section of the nanocomposite solders. The shear test showed that the average mechanical strength of SAC305 solder after the addition of Bi 2 Te 3 nanoparticles was higher. Meanwhile, no thermal fatigue resistance degradation was detected in the nanocomposite solder after 1000 thermal cycles in the range of -40 °C to 115 °C.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Injection Molding Process and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. 10.1007/s11664-005-0197-z10.1007/s11664-005-0197-z ↗
2. 10.1002/adem.20050010910.1002/adem.200500109 ↗
3. 10.2320/matertrans.MJ20100210.2320/matertrans.MJ201002 ↗
4. 10.1016/S0921-5093(03)00466-010.1016/S0921-5093(03)00466-0 ↗
5. 10.1016/S0167-577X(03)00023-510.1016/S0167-577X(03)00023-5 ↗
6. 10.1108/0954091111114689010.1108/09540911111146890 ↗
7. 10.1108/0954091111109965910.1108/09540911111099659 ↗
8. 10.1134/S0018151X1103014X10.1134/S0018151X1103014X ↗
9. gupta · Processing and Fabrication of Advanced Materials XIII · 2005
10. puttlitz · Handbook of Lead-Free Solder Technology for Microelectronic Assemblies · 200410.1201/9780203021484 ↗
11. 10.1007/s11664-004-0138-210.1007/s11664-004-0138-2 ↗
12. 10.1007/s11664-003-0125-z10.1007/s11664-003-0125-z ↗
13. 10.1016/j.microrel.2010.06.01310.1016/j.microrel.2010.06.013 ↗
14. 10.1007/978-0-387-48433-4_810.1007/978-0-387-48433-4_8 ↗
15. 10.1016/S0167-577X(01)00503-110.1016/S0167-577X(01)00503-1 ↗
16. 10.1016/j.jallcom.2011.05.11610.1016/j.jallcom.2011.05.116 ↗
17. 10.1109/EPTC.2007.446980810.1109/EPTC.2007.4469808 ↗
18. 10.1007/s11664-004-0022-010.1007/s11664-004-0022-0 ↗
19. 10.1109/ECTC.2007.37391310.1109/ECTC.2007.373913 ↗
20. 10.1109/TCAPT.2008.92164710.1109/TCAPT.2008.921647 ↗
21. 10.1063/1.479350210.1063/1.4793502 ↗
22. lee · Reflow Soldering Processes and Troubleshooting SMT BGA CSP and Flip Chip Technologies · 2002
23. 10.1007/BF0270184510.1007/BF02701845 ↗
24. 10.1007/978-0-387-48433-4_310.1007/978-0-387-48433-4_3 ↗
25. engelmaier · Solder Joints in Electronics Design for Reliability · 1997