journal article·2014-12

Creep Behaviors of Sn0.7Cu0.1Co0.05Ni/Cu Soldering Joints

Fangjie Cheng, Zhaolong Ma, Ying Wang, Qingbin Zou

Publisher page

Abstract

The creep behaviors of as-soldered and aged Sn0.7Cu0.1Co0.05Ni/Cu joints were studied in this paper. The results indicate that the creep behaviors of as-soldered Sn0.7Cu0.1Co0.05Ni/Cu joints are inferior to those of as-soldered Sn0.7Cu/Cu joints under shear stress of 15-22.5 MPa at 293 and 333 K, respectively. However, the creep behaviors of Sn0.7Cu0.1Co0.05Ni/Cu joints are superior to those of Sn0.7Cu/Cu joints after aging at 423 K for 24 h. The underlying creep mechanisms of the Sn0.7Cu and Sn0.7Cu0.1Co0.05Ni/Cu solder joints at experimental condition are suggested. Meanwhile, the microstructure analysis indicates that the superior creep properties of aged Sn0.7Cu0.1Co0.05Ni/Cu joints may mainly attribute to the coarsening resistance of interfacial intermetallic compounds during aging.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. christian · The Theory of Transformations in Metals and Alloys Part I · 2002
2. shewmon · Diffusion in Solids · 1989
3. 10.1109/33.5617910.1109/33.56179 ↗
4. 10.1016/0036-9748(73)90192-010.1016/0036-9748(73)90192-0 ↗
5. 10.2320/matertrans.43.184710.2320/matertrans.43.1847 ↗
6. 10.1115/1.152525410.1115/1.1525254 ↗
7. shewmon · Transformations in Metals · 1969
8. smithells · Smithells Metals Reference Book · 1991
9. askill · Tracer Diffusion Data for Metals Alloys and Simple Oxides · 2012
10. mishra · Creep Behavior of Advanced Materials for the 21st Century 1999 TMS · 1999 · 51
11. 10.1007/s11664-002-0185-510.1007/s11664-002-0185-5 ↗
12. canumalla · Portable Consumer Electronics Packaging Materials and Reliability · 2010
13. 10.2320/matertrans.46.241910.2320/matertrans.46.2419 ↗
14. 10.1016/j.jallcom.2007.03.02810.1016/j.jallcom.2007.03.028 ↗
15. 10.1109/ESTC.2006.27999310.1109/ESTC.2006.279993 ↗
16. 10.1007/s11664-002-0006-x10.1007/s11664-002-0006-x ↗
17. 10.1016/j.intermet.2009.07.00510.1016/j.intermet.2009.07.005 ↗
18. 10.1007/s11664-999-0167-y10.1007/s11664-999-0167-y ↗
19. 10.1007/s10853-008-2580-710.1007/s10853-008-2580-7 ↗
20. 10.1007/BF0269257610.1007/BF02692576 ↗
21. 10.1007/s11837-009-0087-610.1007/s11837-009-0087-6 ↗
22. 10.1115/1.146262410.1115/1.1462624 ↗
23. Get the lead out, lead-free electronics come of age
24. garofalo · Fundamentals of Creep and Creep-Rupture in Metals · 1965
25. 10.1109/ECTC.2001.92780810.1109/ECTC.2001.927808 ↗
26. 10.1007/s11664-001-0147-310.1007/s11664-001-0147-3 ↗
27. 10.1007/s11664-002-0098-310.1007/s11664-002-0098-3 ↗
28. 10.1007/BF0265136110.1007/BF02651361 ↗
29. ?adek · Creep in Metallic Materials · 1988
30. Characterization of lead-free solders and under bump metallurgies for flip-chip package
31. 10.1557/JMR.2002.010810.1557/JMR.2002.0108 ↗
32. 10.1007/s11664-005-0190-610.1007/s11664-005-0190-6 ↗
33. 10.1007/BF0265136210.1007/BF02651362 ↗
34. Effects of Co addition on the microstructure and tensile behavior of Sn–3.0Ag–0.5Cu solder alloy
35. Aging and creep behavior of Sn3.9Ag0.6Cu solder alloy
36. The measurement of creep rates and stress relaxation for micro-sized lead-free solder joints
37. 10.1109/ECTC.2003.121627710.1109/ECTC.2003.1216277 ↗
38. Alternatives to cross-sectional sample preparation for package and board-level failure analysis
39. 10.1109/ECTC.2005.144137710.1109/ECTC.2005.1441377 ↗
40. 10.1115/1.290931110.1115/1.2909311 ↗
41. 10.1016/0025-5416(81)90179-810.1016/0025-5416(81)90179-8 ↗