journal article·2025

Improvement of Surface Roughness in SiO 2 Thin Films via Deuterium Annealing at 300 °C

Ju-Won Yeon, Hyo-Jun Park, Eui-Cheol Yun, Moon-Kwon Lee, Tae-Hyun Kil, Yong-Sik Kim, Jun-Young Park

Publisher page

Abstract

Recently, deuterium annealing at a reduced temperature range of 300 °C has been proposed to enhance SiO2 gate dielectrics and the Si/SiO2 interface, thereby improving device reliability. As a further investigation into deuterium annealing, for the first time this study compared deuterium absorption characteristics with various SiO2 dielectrics formed by wet oxidation, dry oxidation, low-pressure chemical vapor deposition (LPCVD), and plasma-enhanced chemical vapor deposition (PECVD). Deuterium annealing can also be used to reduce the roughness and improve the uniformity of SiO2 dielectric films. Surface roughness of various samples was measured and quantitatively compared using atomic force microscopy (AFM) after deuterium annealing.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Semiconductor Engineering, Chungbuk National University, Cheongju, South Korea

Department of Semiconductor Engineering, Daelim University College, Anyang, South Korea

Funding

National Research Foundation of Korea · Start up Pioneering in Research and Innovation · Commercialization Promotion Agency for R&D Outcomes · Korea government · IC Design Education Center

References (36)

Show source-provided references
1. 10.1109/5.22090010.1109/5.220900 ↗
2. 10.1109/jproc.2003.81833610.1109/jproc.2003.818336 ↗
3. 10.1109/jproc.2002.80815610.1109/jproc.2002.808156 ↗
4. 10.1109/iedm.1999.82384810.1109/iedm.1999.823848 ↗
5. 10.1109/LED.2006.87338110.1109/LED.2006.873381 ↗
6. 10.1109/nvmts.2014.706084010.1109/nvmts.2014.7060840 ↗
7. 10.1109/LED.2004.82519910.1109/LED.2004.825199 ↗
8. 10.5573/jsts.2021.21.5.33410.5573/jsts.2021.21.5.334 ↗
9. 10.23919/VLSIT.2017.799818310.23919/VLSIT.2017.7998183 ↗
10. 10.1364/OL.46817710.1364/OL.468177 ↗
11. 10.1117/1.175691710.1117/1.1756917 ↗
12. Contrast optimization for 0.33 NA EUV lithography
13. 10.1109/TED.2010.204840510.1109/TED.2010.2048405 ↗
14. 10.1109/IEDM19573.2019.899361510.1109/IEDM19573.2019.8993615 ↗
15. 10.1080/09500340.2014.97584610.1080/09500340.2014.975846 ↗
16. 10.1109/JMEMS.2005.85909210.1109/JMEMS.2005.859092 ↗
17. 10.1109/TNANO.2017.276180310.1109/TNANO.2017.2761803 ↗
18. 10.1063/1.11281810.1063/1.112818 ↗
19. 10.1109/IEDM.2018.861466710.1109/IEDM.2018.8614667 ↗
20. 10.1109/imw.2016.749527710.1109/imw.2016.7495277 ↗
21. 10.1063/1.32258810.1063/1.322588 ↗
22. 10.1016/j.surfcoat.2017.11.01310.1016/j.surfcoat.2017.11.013 ↗
23. 10.1109/iedm.2007.441888610.1109/iedm.2007.4418886 ↗
24. 10.1109/IWAPS54037.2021.967106910.1109/IWAPS54037.2021.9671069 ↗
25. 10.1007/s12633-023-02789-610.1007/s12633-023-02789-6 ↗
26. 10.1016/j.sse.2022.10842110.1016/j.sse.2022.108421 ↗
27. 10.1109/TDMR.2023.327594710.1109/TDMR.2023.3275947 ↗
28. 10.1109/TED.2023.327862610.1109/TED.2023.3278626 ↗
29. 10.1016/j.microrel.2023.11527610.1016/j.microrel.2023.115276 ↗
30. 10.1063/1.504769910.1063/1.5047699 ↗
31. 10.1116/1.176107210.1116/1.1761072 ↗
32. AFM studies on surface morphology, topography and texture of nanostructured zinc aluminum oxide thin films
33. 10.1109/TED.2023.334409010.1109/TED.2023.3344090 ↗
34. 10.1007/s41871-022-00126-w10.1007/s41871-022-00126-w ↗
35. 10.1063/1.476745610.1063/1.4767456 ↗
36. 10.1016/j.tsf.2009.03.18610.1016/j.tsf.2009.03.186 ↗