journal article·2020

Mechanisms of a Rectifying TiN Gate Contact for AlGaN$/$GaN HEMTs on Silicon Substrate

Hassane Ouazzani Chahdi, Brahim Benbakhti, Maghnia Mattalah, Jean Claude Gerbedoen, Abdelatif Jaouad, Nour Eddine Bourzgui, Ali Soltani

Publisher page

Abstract

Rectifying Titanium Nitride (TiN) gate contact technology is developed for AlGaN/GaN based micro and nanometer HEMTs. A high compressive strain occurring in thinner TiN films (ranging from 5 nm to 60 nm), deposited by sputtering, leads to a reduction in tensile strain at the surface of AlGaN barrier. The diminution in tensile strain forms a pseudo-p-type layer (diodelike). This strain reduction has no effect on the bandgap of the AlGaN barrier layer, allowing the gate to withstand a reverse gate bias larger than 100 V. Characterization using the high-resolution transmission electron microscopy combined with the X-ray photoelectron spectroscopy reveals a good TiN/AlGaN interface quality and no diffusion of TiN into AlGaN. The effective energy barrier of the rectifying nanoscale TiN gate contact has a relatively large height of 1.1 eV associated with an ideality factor of 1.4. A dramatic drop of the reverse-bias leakage current down to 11 pA/mm is measured at -30 V. In addition, electrical measurements show very low gate and drain lag effects of 4.2% and 6.7%, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor materials and devices · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. 10.1002/pssa.20030674810.1002/pssa.200306748 ↗
2. 10.1063/1.233711010.1063/1.2337110 ↗
3. 10.1016/j.jmps.2009.11.01010.1016/j.jmps.2009.11.010 ↗
4. gerbedoen · Proc Eur Microw Integr Circuits Conf · 0 · 136
5. 10.1002/pssc.20110021110.1002/pssc.201100211 ↗
6. Materials and Reliability Handbook for Semiconductor Optical and Electron Devices · 2013
7. 10.1109/TED.2017.271278210.1109/TED.2017.2712782 ↗
8. 10.1109/LED.2013.227442910.1109/LED.2013.2274429 ↗
9. 10.1088/0268-1242/28/7/07400410.1088/0268-1242/28/7/074004 ↗
10. 10.1088/0268-1242/29/9/09500510.1088/0268-1242/29/9/095005 ↗
11. 10.1109/LED.2013.229185410.1109/LED.2013.2291854 ↗
12. 10.1109/LED.2017.273491410.1109/LED.2017.2734914 ↗
13. 10.1109/LED.2012.220485410.1109/LED.2012.2204854 ↗
14. 10.1109/TED.2017.278114110.1109/TED.2017.2781141 ↗
15. 10.1109/ACCESS.2018.286132310.1109/ACCESS.2018.2861323 ↗
16. 10.1016/j.diamond.2006.06.02210.1016/j.diamond.2006.06.022 ↗
17. 10.1016/j.apsusc.2004.05.09110.1016/j.apsusc.2004.05.091 ↗
18. 10.1109/LED.2013.224484110.1109/LED.2013.2244841 ↗
19. 10.1109/LED.2018.284495110.1109/LED.2018.2844951 ↗
20. 10.1109/JEDS.2019.291509710.1109/JEDS.2019.2915097 ↗
21. 10.1109/TED.2014.229955610.1109/TED.2014.2299556 ↗
22. 10.1109/TED.2019.291278310.1109/TED.2019.2912783 ↗
23. 10.1109/JEDS.2017.267268510.1109/JEDS.2017.2672685 ↗
24. li · Phys Status Solidi · 0 · 214
25. 10.1109/LED.2015.239545410.1109/LED.2015.2395454 ↗
26. 10.1109/TED.2018.285677310.1109/TED.2018.2856773 ↗
27. 10.1007/s11664-007-0189-210.1007/s11664-007-0189-2 ↗
28. 10.1109/ESSDERC.2013.681883010.1109/ESSDERC.2013.6818830 ↗
29. GaN MIS-HEMTs with nitrogen passivation for power device applications10.1109/LED.2014.2345130 ↗
30. 10.1109/TED.2013.227379610.1109/TED.2013.2273796 ↗
31. 10.1109/ICSICT.2014.702166910.1109/ICSICT.2014.7021669 ↗
32. 10.1109/LPT.2013.229013010.1109/LPT.2013.2290130 ↗
33. 10.1109/TED.2009.202840010.1109/TED.2009.2028400 ↗
34. 10.1109/LED.2014.235998610.1109/LED.2014.2359986 ↗
35. The influence mechanism of Al$_{\mathrm{2}}$O$_{\mathrm{3}}$ layer and etching depth on 2DEG sheet density in gate-recessed Al$_{\mathrm{2}}$O$_{\mathrm{3}}$$/$AlGaN$/$GaN MOS-HEMTs