journal article·2014-01

Preparation of Silver Nanoparticles by Using Tripropylene Glycol as the Reducing Agents of Polyol Process

Tzu Hsuan Chiang, K.-D. Wu, Tsung-Eong Hsieh

Publisher page

Abstract

Silver (Ag) nanoparticles were prepared by the polyol process using tripropylene glycol, 3-ethyl-3-oxetanemethanol, and polycaprolactone triol as the reducing agents and poly(vinylpyrrolidone) (PVP) with average molecular weights (Mw) of 10 000, 55 000, and 1 300 000 as the protective agent, respectively. It was found that the sizes of Ag particles were affected by the type of reducing agent, Mw of PVP, the concentration of PVP, reaction temperature, and time. The Ag nanoparticles as small as 34.4 nm were achieved when the reaction was conducted at atmospheric ambient and a temperature of 120 °C for 3 h by using tripropylene glycol as the reducing agent and 20 wt.% PVP with an Mw of 55 000. The nanoscale Ag particles with face-centered cubic structure exhibited a strong surface plasmon resonance peak at 350 nm in the UV-visible spectrum.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Gold and Silver Nanoparticles Synthesis and Applications · Nanomaterials and Printing Technologies · Nanoparticles: synthesis and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. 10.1016/j.saa.2006.01.01010.1016/j.saa.2006.01.010 ↗
2. 10.1016/j.saa.2007.12.00210.1016/j.saa.2007.12.002 ↗
3. 10.1016/j.matchemphys.2007.12.00910.1016/j.matchemphys.2007.12.009 ↗
4. 10.14429/dsj.59.154510.14429/dsj.59.1545 ↗
5. 10.1016/j.colsurfa.2005.09.00410.1016/j.colsurfa.2005.09.004 ↗
6. 10.1103/PhysRevB.64.23540210.1103/PhysRevB.64.235402 ↗
7. 10.1002/chem.20040092710.1002/chem.200400927 ↗
8. SPR of Ag nanoparticles in a photothermochromic glasses
9. 10.1039/jm996060057310.1039/jm9960600573 ↗
10. 10.1557/S088376940006093010.1557/S0883769400060930 ↗
11. 10.1016/j.physe.2004.07.01010.1016/j.physe.2004.07.010 ↗
12. 10.1002/app.2702410.1002/app.27024 ↗
13. 10.1088/0022-3727/38/7/01510.1088/0022-3727/38/7/015 ↗
14. 10.1007/s10853-005-0669-910.1007/s10853-005-0669-9 ↗
15. 10.1016/j.apcata.2008.02.01610.1016/j.apcata.2008.02.016 ↗
16. 10.1039/a605347e10.1039/a605347e ↗
17. 10.1088/0957-4484/22/4/04560210.1088/0957-4484/22/4/045602 ↗
18. 10.1016/j.molcata.2004.06.02510.1016/j.molcata.2004.06.025 ↗
19. 10.1016/j.ijadhadh.2005.07.00410.1016/j.ijadhadh.2005.07.004 ↗
20. Preparation of ultrafine silver powder using glycerol as reducing agent
21. Use of sodium borohydride to control heavy metal discharge in the photographic industry
22. 10.1016/j.tsf.2004.11.07710.1016/j.tsf.2004.11.077 ↗
23. 10.1016/S0254-0584(00)00223-610.1016/S0254-0584(00)00223-6 ↗
24. 10.1016/0022-4596(92)90101-Z10.1016/0022-4596(92)90101-Z ↗
25. 10.1006/jssc.1996.001510.1006/jssc.1996.0015 ↗
26. 10.1063/1.11595510.1063/1.115955 ↗
27. Preparation of nanocrystalline silver powders by ?-ray radiation combined with hydrothermal treatment10.1016/0167-577X(93)90021-O ↗
28. 10.1002/marc.20040044510.1002/marc.200400445 ↗
29. 10.1021/cm950285s10.1021/cm950285s ↗
30. 10.1002/adma.20050242210.1002/adma.200502422 ↗
31. 10.1002/marc.20060089510.1002/marc.200600895 ↗
32. 10.1016/j.jcis.2005.03.00510.1016/j.jcis.2005.03.005 ↗
33. 10.1006/jcis.2002.867410.1006/jcis.2002.8674 ↗
34. 10.1021/nl800910d10.1021/nl800910d ↗
35. 10.1007/BF0271125010.1007/BF02711250 ↗
36. Investigation of silver nanoparticles formation kinetics during reduction of silver nitrate with sodium citrate
37. 10.2147/IJN.S1686710.2147/IJN.S16867 ↗