Abstract

The charge-trapping characteristics of Ga 2 O 3 (Gd 2 O 3 ) (denoted as GGO) with and without nitrogen incorporation were investigated based on Al/Al 2 O 3 /GGO/SiO 2 /Si (metalalumina-nitride-oxide-silicon) capacitors. Compared with the capacitor without nitrogen incorporation, the one with nitrided GGO showed a larger memory window (10 V at ±16 V, 1 s), a higher program speed with a low gate voltage (2.2V at +8 V, 100 μs), and a better retention property (charge loss of 9.7% after 104 s at 125°C) mainly due to higher charge-trapping efficiency of the nitrided GGO film and the nitrogen-induced suppressed formation of the undesirable silicate interlayer at the GGO/SiO 2 interface, as confirmed by the transmission electron microscopy and the X-ray photoelectron spectroscopy.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Ga2O3 and related materials · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Energy-band parameters at the GaAs– and GaN–Ga$2$O $3$(Gd$2$O $3$) interfaces10.1016/S0038-1101(01)00175-7 ↗
2. Molecular beam epitaxy grown Ga$2$O$3$ (Gd$2$O$3$ ) high κ dielectrics for germanium passivation-x-ray photoelectron spectroscopy and electrical characteristics10.1116/1.2884752 ↗
3. Gd$2$O$3$ , Ga$2$O$3$ (Gd$2$O$3$ ), Y$2$O$3$ , and Ga$2$O $3$, as high-k gate dielectrics on SiGe: A comparative study
4. Effect of temperature on Ga$2$O $3$(Gd$2$O $3$)/GaN metal–oxide–semiconductor field-effect transistors10.1063/1.122927 ↗
5. 10.1103/PhysRevB.69.04511510.1103/PhysRevB.69.045115 ↗
6. 10.1063/1.160963610.1063/1.1609636 ↗
7. 10.1063/1.137501810.1063/1.1375018 ↗
8. Enhanced thermal stability of high-dielectric Gd$2$ O$_3$ films using ZrO $2$ incorporation10.1063/1.1644047 ↗
9. 10.1063/1.360647710.1063/1.3606477 ↗
10. 10.1016/j.sse.2012.09.00510.1016/j.sse.2012.09.005 ↗
11. Comparison of MONOS memory device integrity when using Hf $1-x-y$N$x$ O$y$ trapping layers with different N compositions10.1109/TED.2008.920973 ↗
12. Nitrided tetragonal ZrO$_2$as the charge-trapping layer for nonvolatile memory application10.1109/LED.2009.2034115 ↗
13. 10.1063/1.352289010.1063/1.3522890 ↗
14. 10.1109/LED.2010.205209010.1109/LED.2010.2052090 ↗
15. CF$4$ plasma treatment on nanostructure band engineered Gd $2$O$3$ -nanocrystal nonvolatile memory
16. High-performance high-k Y$2$O $_3$SONOS-type flash memory10.1109/TED.2008.927401 ↗
17. Good 150°C retention and fast erase charge-crapping-engineered memory with scaled Si$3$N $4$
18. 10.1063/1.136106510.1063/1.1361065 ↗
19. 10.1063/1.353155910.1063/1.3531559 ↗
20. 10.1149/1.349415010.1149/1.3494150 ↗
21. 10.1063/1.220274910.1063/1.2202749 ↗
22. 10.1063/1.360147310.1063/1.3601473 ↗
23. Tunnel oxide thickness dependence of activation energy for retention time in SiGe quantum dot flash memory
24. 10.1016/j.sse.2004.06.00910.1016/j.sse.2004.06.009 ↗