journal article·2025-06-01

Effect of steam curing on strength, durability and microstructure of concretes with and without mineral admixtures

Beixing Li, Yucheng Yang, An Huang, Liang Huang, Yuxin Guo

Advances in Cement Research· Volume 37· Issue 6
Publisher page

Abstract

This research explores the effect of steam curing on the strength, durability and microstructure of concretes with and without mineral admixtures of fly ash (FA) and ground granulated blast-furnace slag powder (SL). Two types of C55 strength grade concretes (one was pure cement concrete, the other was a concrete made by replacing part of the cement with 12% FA and 18% SL) were prepared and their compressive strength, chloride diffusion coefficient and carbonation depth under standard and steam-curing conditions were measured and compared. The phase composition and microstructure of the concretes under the two curing conditions were tested by X-ray diffraction, scanning electron microscopy and mercury intrusion porosimetry. The results showed that, on the one hand, compared with standard curing, steam curing is beneficial to the early strength, but not conducive to the later strength development and chloride permeability resistance of both types of concretes. Furthermore, for the steam-cured concrete, the 28 days carbonation depth of the forming surface is higher than that of the bottom surface. In addition, steam curing can reduce the carbonisation resistance of pure cement concrete and improve the carbonisation resistance of concrete mixed with FA and SL. On the other hand, composite mineral admixtures of FA and SL reduce the early strength and the carbonisation resistance of concrete cured by standard curing, but improve the later strength, the carbonisation resistance and chloride permeability resistance of concrete cured by steam curing. FA and SL are thermally activated under steam curing and can react with the calcium hydroxide formed by cement hydration in the early stage, which produces a larger amount of secondary hydration products to improve the pore structure and interfacial microstructure of the concrete with FA and SL. In this way, the adverse effects of steam curing on later strength and durability of concrete are significantly restrained by composite mineral admixtures of FA and SL.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Professor, State Key Laboratory of Silicate Materials for Architecture, Wuhan University of Technology, Wuhan, PR China (corresponding author: )

Master’s course student, School of Materials Science and Engineering, Wuhan University of Technology, Wuhan, PR China

References (39)

Show source-provided references
1. 10.1016/j.conbuildmat.2010.06.04910.1016/j.conbuildmat.2010.06.049 ↗
2. 10.1016/S0008-8846(01)00471-910.1016/S0008-8846(01)00471-9 ↗
3. Geng J · Journal of Building Materials · 2011 · 14 · 116
4. He ZM (2012) Heat Damage Effects of Steam Curing on Concrete and Corresponding Improvement Measures. PhD thesis, Central South University, Changsha, China.
5. 10.1007/s11771-012-1122-210.1007/s11771-012-1122-2 ↗
6. Huang A · Bulletin of the Chinese Ceramic Society · 2021 · 40 · 1170
7. 10.1016/j.conbuildmat.2023.13247610.1016/j.conbuildmat.2023.132476 ↗
8. Jahami A · Nano World Journal · 2023 · 9 · S87
9. 10.3390/infrastructures811015710.3390/infrastructures8110157 ↗
10. 10.1007/s41062-024-01384-x10.1007/s41062-024-01384-x ↗
11. 10.1016/j.conbuildmat.2017.03.22510.1016/j.conbuildmat.2017.03.225 ↗
12. Jung W · Advances in Materials Science and Engineering · 2017 · 2017 · 1
13. 10.1016/0008-8846(91)90044-I10.1016/0008-8846(91)90044-I ↗
14. 10.1016/S0008-8846(00)00213-110.1016/S0008-8846(00)00213-1 ↗
15. 10.1155/2017/986321910.1155/2017/9863219 ↗
16. Li X · Journal of Central South University (Natural Science Edition) · 2010 · 41 · 2321
17. Liu YB · ACI Materials Journal · 2014 · 111 · 531
18. 10.1016/j.cemconres.2004.05.04410.1016/j.cemconres.2004.05.044 ↗
19. 10.1680/macr.11.0016410.1680/macr.11.00164 ↗
20. Ma KL · Materials Review · 2017 · 31 · 171
21. Meng ZY · Concrete · 2010 · 7 · 28
22. 10.1016/0008-8846(95)00036-C10.1016/0008-8846(95)00036-C ↗
23. 10.1016/j.conbuildmat.2014.09.07210.1016/j.conbuildmat.2014.09.072 ↗
24. 10.1007/s41062-022-00896-810.1007/s41062-022-00896-8 ↗
25. 10.1016/j.conbuildmat.2017.07.00610.1016/j.conbuildmat.2017.07.006 ↗
26. 10.1016/j.conbuildmat.2020.11909510.1016/j.conbuildmat.2020.119095 ↗
27. 10.1016/j.conbuildmat.2020.11940710.1016/j.conbuildmat.2020.119407 ↗
28. 10.1016/j.jobe.2020.10147510.1016/j.jobe.2020.101475 ↗
29. 10.1061/(ASCE)0899-1561(2003)15:2(134)10.1061/(ASCE)0899-1561(2003)15:2(134) ↗
30. Tian YG · Journal of Building Materials · 2010 · 13 · 515
31. Tian YG · Journal of Building Materials · 2009 · 12 · 720
32. 10.1016/j.cemconres.2004.07.03810.1016/j.cemconres.2004.07.038 ↗
33. 10.1007/s10853-011-5689-z10.1007/s10853-011-5689-z ↗
34. Wang X · Bulletin of the Chinese Ceramic Society · 2021 · 40 · 1170
35. Wu ZW · 1999
36. Xiang Y · Structural Concrete · 2021 · 22 · E1074
37. Yan PY · Electron Micrograph · 2019 · 38 · 82
38. Yang JB · Fly Ash Comprehensive Utilization · 2021 · 4 · 104
39. 10.1016/j.conbuildmat.2021.12240910.1016/j.conbuildmat.2021.122409 ↗